journal article·2025-11

Effect of cooling rate on the microstructure stability and creep properties of Ni–Cr–Mo–Co alloy for 700 °C A-USC large-scale rotors

Yaguan Bai, Yihong Nie, Wei Guo, Jinfeng Kou, Dapeng Wang, Xinghong Bai, Deli Zhao, Wantang Fu

Publisher page

Abstract

No abstract is available for this record. The assistant can identify its topic from the title, but cannot infer the study’s results.

Source: Not provided · Quality: missing

Research context

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (36)

Show source-provided references
1. Research and development of heat-resistant materials for advanced USC power plants with steam temperatures of 700 °C and above10.15302/J-ENG-2015031 ↗
2. Wrought Ni-Base superalloys for steam turbine applications beyond 700 °C10.1002/adem.200310083 ↗
3. Nickel base superalloys for next generation coal fired AUSC power plants10.1016/j.proeng.2013.03.250 ↗
4. Superalloys and the development of advanced ultra-supercritical power plants10.4028/www.scientific.net/MSF.747-748.594 ↗
5. Large-Scale manufacture of nickel alloy turbine rotor forgings for A-USC power plants10.1007/s41403-020-00091-0 ↗
6. Materials development for boilers and steam turbines operating at 700 °C
7. Imano · 2005 · 77
8. Superalloy forgings for advanced high temperature power plants
9. Materials for advanced ultra-supercritical fossil-fuel power plants: materials properties, microstructure, and component behavior10.1002/ente.201500311 ↗
10. Research and development on the heat resistant alloy used for 700 °C advanced fossil fired ultra Super-Critical(A-USC) power plant in China
11. Systematical innovation of heat resistant materials used for 630 ∼ 700 °C advanced ultra-supercritical (A-USC) fossil fired boilers
12. The Chinese 700 °C A-USC development program
13. D progress of 700 °C power generation technology and alloy 617 in Europe
14. Development of nickel alloys based on alloy 617 for components in 700 °C power plants10.1016/j.proeng.2013.03.247 ↗
15. Two stress rupture modes observed in alloy 617-9%Cr dissimilar welded joint
16. Microstructure evolution in alloy 617 B after a long-term creep and thermal aging at 700 °C10.1016/j.msea.2017.11.004 ↗
17. Microstructural insights into creep of Ni-based alloy 617 at 700 °C provided by electron microscopy and modelling10.1016/j.matchar.2023.112720 ↗
18. Effect of ageing on creep behaviour of IN 617 nickel base super alloy for advanced USC power plant applications10.1007/s12666-015-0772-9 ↗
19. Creep behavior of INCOLOY alloy 61710.1007/s10853-007-1803-7 ↗
20. Microstructure of long-term aged IN617 Ni-base superalloy10.1007/s11661-008-9618-y ↗
21. The effect of Mo and Ti elements on long-term microstructure stability of 617B nickel-base superalloy10.1016/j.jallcom.2019.153217 ↗
22. Solidification and segregation characteristics of Ni-based superalloy C700R-1 for ultra-supercritical steam turbine rotor10.1016/j.jallcom.2022.165107 ↗
23. Effect of compositional modifications on microstructure and properties of IN 617 alloy
24. Microstructure evolution during aging of alloy 617B for 700 °C ultra-supercritical boiler pipe
25. Effect of aging temperature on microstructure and mechanical properties of modified inconel 617 alloy
26. Microstructure and phase stability of INCONEL alloy 61710.1007/BF02643879 ↗
27. Microstructure and mechanical properties of alloy 617B10.1016/S1003-6326(15)63704-9 ↗
28. Effects of different elevated temperature and long-term exposure on microstructural evolution and mechanical characteristics of IN617 Ni-based superalloy10.1016/j.msea.2022.143025 ↗
29. Effect of increasing Al content on creep rupture performance and microstructure stability of IN 617 alloy
30. Investigation on precipitation phenomena of Ni-22Cr-12Co-9Mo alloy aged and crept at high temperature10.1016/j.ijpvp.2007.06.014 ↗
31. The effect of grain boundary serration on creep resistance in a wrought nickel-based superalloy10.1016/j.msea.2009.03.071 ↗
32. On the mechanism of serrated grain boundary formation in Ni-based superalloys10.1016/0001-6160(83)90202-X ↗
33. The impact of grain boundary serration treatments on the creep deformation of Udimet-720Li superalloy10.1016/j.msea.2024.147729 ↗
34. Phase transformation of alloy 617B during 10000 h aging: an element Redistribution-related process10.1016/j.jallcom.2018.06.229 ↗
35. The characteristics of μ phase precipitated during 720 °C long-term aging in alloy 617B10.1016/j.jmrt.2018.11.006 ↗
36. Formation of μ phase during thermal exposure and its effect on the properties of K465 superalloy10.1016/j.scriptamat.2006.04.032 ↗