journal article·2017-04

Effects of wire-electro discharge machining process on surface integrity of WC-10Co alloy

Erdem Sireli, Nilufer Orhon, Guldem Kartal Sireli

Publisher page

Abstract

Abstract In this study, the effects of heat affected zone generated by wire electro discharge machining (w-EDM) process on the surface integrity of a K15 grade hard metal before and after TiN coating application via chemical vapour deposition (CVD) was investigated. It was observed that applying dry blasting (DB) on w-EDM'ed surfaces is a very efficient way to remove heat affected zone, namely recast layer. TiN layers deposited on w-EDM'ed surfaces showed a great diversity in their morphologies depending on the w-EDM process parameters and exhibited irregularities whereas the ones coated on dry blasted (DB'ed) surfaces constituted much finer mixture of nodular, star shaped and lenticular crystals. Adhesion of TiN layers on the DB'ed hard metal samples was better compared to the ones deposited directly on w-EDM'ed samples with a thick heat affected zone on their surfaces. Friction and wear properties of the TiN layer formed on DB'ed surface against alumina ball were also superior which were also in good agreement with its higher adhesion strength and distinctive morphology.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (34)

Show source-provided references
1. Microstructure and mechanical properties of WC–10Co cemented carbide containing VC or (Ta, Nb)C and fracture toughness evaluation using different models10.1016/j.ijrmhm.2011.10.004 ↗
2. Effect of microstructure on edge wear mechanisms in WC–Co10.1016/j.ijrmhm.2006.04.004 ↗
3. Friction and wear characteristics of WC–Co cemented carbides in dry reciprocating sliding contact10.1016/j.wear.2010.02.029 ↗
4. Advances in alloy design aspects of cemented carbides10.1016/S0261-3069(01)00003-6 ↗
5. Impact of Cr3C2/VC addition on the dry sliding friction and wear response of WC–Co cemented carbides10.1016/j.wear.2009.06.013 ↗
6. Effect of WC particle size on the microstructure, mechanical properties and fracture behavior of WC–(W, Ti, Ta) C–6 wt%Co cemented carbides10.1016/j.ijrmhm.2006.11.005 ↗
7. Alloyed W–(Co,Ni,Fe)–C phases for reaction sintering of hardmetals10.1016/j.ijrmhm.2010.06.003 ↗
8. Binder phase structure in fine and coarse WC–Co hard metals with Cr and V carbide additions10.1016/j.ijrmhm.2013.04.001 ↗
9. Effect of Cu, Ni on the property and microstructure of ultrafine WC-10Co alloys by sinter–hipping10.1016/j.ijrmhm.2011.02.012 ↗
10. On the solubility of chromium in the cubic carbide and M7C3 carbide in the WC–Co–Cr–Me systems (Me=Ti, Nb, Ta and Zr)10.1016/j.ijrmhm.2013.04.005 ↗
11. Microwave sintering of nanocrystalline WC–12Co: challenges and perspectives10.1016/j.ijrmhm.2009.08.005 ↗
12. Fabrication of WC–8 wt%Co hard materials by two rapid sintering processes10.1016/j.ijrmhm.2006.09.001 ↗
13. Reactive spark plasma sintering of binderless WC ceramics at 1500°C10.1016/j.ijrmhm.2013.10.013 ↗
14. Suppression of abnormal grain growth in WC–Co via pre-sintering treatment10.1016/j.ijrmhm.2008.04.001 ↗
15. Fatigue performance improvement of electrical discharge machined hardmetals by means of combined thermal annealing and surface modification routes10.1016/j.ijrmhm.2011.12.008 ↗
16. A review on the conventional and micro-electrodischarge machining of tungsten carbide10.1016/j.ijmachtools.2011.08.016 ↗
17. Influence of electrical discharge machining on the reciprocating sliding wear response of WC-Co cemented carbides10.1016/j.wear.2008.05.009 ↗
18. Fracture and fatigue behavior of electrical-discharge machined cemented carbides10.1016/j.ijrmhm.2005.04.007 ↗
19. Influence of electrical discharge machining on the sliding contact response of cemented carbides10.1016/S0263-4368(00)00045-7 ↗
20. Study of the effect of machining parameters on the machining characteristics in electrical discharge machining of tungsten carbide10.1016/S0924-0136(01)00992-X ↗
21. Analysis of the influence of EDM parameters on surface quality, MRR and EW of WC–Co10.1016/j.jmatprotec.2004.04.346 ↗
22. Surface finishing: impact on tribological characteristics of WC–Co hardmetals10.1016/j.triboint.2009.04.029 ↗
23. Reciprocating friction and wear behavior of WC-Co based cemented carbides manufactured by electro-discharge machining
24. Residual stresses in hardmetals caused by grinding and EDM machining and their influence on the flexural strength
25. Abrasive micro-blasting to improve surface integrity of electrical discharge machined WC–Co composite10.1016/j.jmatprotec.2004.09.075 ↗
26. Mechanical strength improvement of electrical discharge machined cemented carbides through PVD (TiN, TiAlN) coatings10.1016/S0040-6090(03)01062-9 ↗
27. The effect of deposition temperature on microstructure and properties of thermal CVD TiN coatings10.1016/j.ijrmhm.2007.01.010 ↗
28. Kinetics and microstructure of TiN coatings by CVD10.1016/S0257-8972(00)00986-5 ↗
29. Microstructural and physical properties of titanium nitride coatings produced by CVD process10.1016/S0921-5093(00)00744-9 ↗
30. Surface modification by electrical discharge machining: a review10.1016/j.jmatprotec.2008.09.032 ↗
31. The VDI 3198 indentation test evaluation of a reliable qualitative control for layered compounds10.1016/S0924-0136(03)00300-5 ↗
32. Adhesion and abrasive wear resistance of TiN deposited on electrical discharge machined WC–Co cemented carbides10.1016/j.wear.2007.11.016 ↗
33. Correlation between process parameters, microstructure and hardness of titanium nitride films by chemical vapor deposition10.1016/S0257-8972(03)00789-8 ↗
34. Production and characterization of wear resistant Ti(C,N) coatings manufactured by modified chemical vapor deposition process10.1016/j.surfcoat.2010.09.013 ↗