Influence of electrical discharge machining on the reciprocating sliding friction and wear response of WC–Co cemented carbides

K. Bonny, P. De Baets, W. Ost, S. Huang, J. Vleugels, W. Liu, B. Lauwers

Publisher page

Abstract

Abstract The dry friction and wear behavior of a number of WC–Co cemented carbides, exhibiting 6 up to 12 wt.% cobalt as binder phase and average carbide grain sizes ranging from 0.3 up to 2.2 μm, combined with various surface finishing variants of wire electrical discharge machining (EDM), was evaluated by performing linearly reciprocating pin-on-flat sliding experiments against WC–Co cemented carbide using normal contact loads of 15 N up to 35 N and a sliding velocity of 0.3 m/s. Post-mortem obtained wear volumes and volumetric wear rates were correlated to real-time recorded penetration depth curves versus sliding distance. Consecutive execution of gradually finer EDM regimes onto the WC–Co alloys was found to considerably enhance the wear performance. Scanning electron microscopy on the worn surfaces revealed the occurrence of several wear mechanisms, i.e., grain polishing, abrasion, grain cracking and surface binder removal, mainly depending on the original surface finish EDM regime.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (33)

Show source-provided references
1. Machining of low electrical conductive materials by wire electrical discharge machining (WEDM)10.1016/j.jmatprotec.2003.11.055 ↗
2. Machining of WC–Co composites10.1080/10426918908956301 ↗
3. Electrical discharge machining of tungsten carbide–cobalt composites10.1111/j.1151-2916.1989.tb07660.x ↗
4. Influence of the composition of WC-based cermets on the manufacturability by Wire-EDM
5. ED machining of WC–Co10.1016/j.jmatprotec.2005.02.211 ↗
6. Investigation of material removal mechanisms in EDM of composite ceramic materials10.1016/j.jmatprotec.2004.02.013 ↗
7. Analysis of the influence of EDM parameters on surface quality, MRR and EW of WC–Co10.1016/j.jmatprotec.2004.04.346 ↗
8. Relationship of surface roughness with current and voltage during wire EDM10.3923/jas.2006.2317.2320 ↗
9. Abdullah A, Shabgard MR, Ivanov A, Shervanyi-Tabar MT. Effect of ultrasonic-assisted EDM on the surface integrity of cemented tungsten carbide (WC–Co). Int J Adv Manuf Tech. doi: 10.1007/s00170-008-1476-7.10.1007/s00170-008-1476-7 ↗
10. Fundamental study on corrosion of cemented carbide during wire EDM10.1016/j.jmatprotec.2003.10.045 ↗
11. Jiang D, Anné G, Vleugels J, Vanmeensel K, Eeraerts W, Lauwers B, et al. Residual stress in hardmetals caused by grinding and EDM machining and its influence on flexural strength. In: Proc 16th Int Plansee Seminar. Powder Metallurgical High Performance Material, vol. 2, 2005. p. 1075–85.
12. Effects of electrical discharge energy on machining performance and bending strength of cemented tungsten carbides10.1016/j.jmatprotec.2007.12.056 ↗
13. Fracture and fatigue behavior of electrical-discharge machined cemented carbides10.1016/j.ijrmhm.2005.04.007 ↗
14. Surface integrity effects on the fracture resistance of electrical-discharge-machined WC–Co cemented carbides10.1111/j.1551-2916.2004.01687.x ↗
15. Effect of the electro-discharge machined surface on the mechanical properties – On the fatigue strength of cemented carbide
16. Nanoindentation characterization of surface layers of electrical discharge machined WC–Co10.1016/S0921-5093(02)00395-7 ↗
17. Influence of EDM on the wear characteristics of WC–Co cemented carbide
18. Influence of electrical discharge machining on the sliding contact response of cemented carbides10.1016/S0263-4368(00)00045-7 ↗
19. Bonny K, De Baets P, Lauwers B, Vleugels J, Van Der Biest O. Influence of Electro-discharge machining, microstructural and mechanical properties on wear behavior of hardmetals. In: Proc 16th Int Plansee Seminar, Powder Metallurgical High Performance Materials, vol. 2, 2005. p. 863–77.
20. Influence of surface finishing and binder phase on friction and wear of WC based hardmetals10.4028/www.scientific.net/MSF.561-565.2403 ↗
21. Reciprocating friction and wear behavior of WC–Co based cemented carbides manufactured by electro-discharge machining10.4028/www.scientific.net/MSF.561-565.2025 ↗
22. Relations between condition and electrically discharge machining and depth of surface crack in cemented carbides10.1299/kikaic.61.1192 ↗
23. XPS and AES surface characterization of WC–Co after electro-discharge machining10.1002/sia.1762 ↗
24. Indentation fracture of WC–Co cermets10.1007/BF00555296 ↗
25. ASTM G 133-05, Standard Test Method for Linearly Reciprocating Ball-on-Flat SlidingWear. Annual Book of ASTM Standards, vol. 03.02, 2005.
26. Influence of secondary electro-conductive phases on the electrical discharge machinability and frictional behavior of ZrO2-based ceramic composites10.1016/j.jmatprotec.2008.01.020 ↗
27. Sliding wear of electrically conductive ZrO2-WC composites against WC–Co cemented carbide10.1007/s11249-008-9326-1 ↗
28. Wear mechanisms in abrasion and erosion of WC/Co and related hardmetals10.1016/j.wear.2006.12.046 ↗
29. Gee MG, Gant A, Byrne LP, Roebuck B. Abrasion and reciprocating wear of hardmetals and ceramics. NPL Report CMMT(A) 1999. p. 166.
30. Friction and wear behaviour of cemented carbides10.1016/j.wear.2003.12.014 ↗
31. Basic principles of rough surface contact analysis using numerical methods10.1016/0301-679X(96)00016-3 ↗
32. A fast solution of the dry contact problem and associated surface stress field using multilevel techniques10.1115/1.2920577 ↗
33. Effect of roughness and sliding friction on contact stress10.1115/1.2920686 ↗