Relationship between hardness and fracture toughness in WC–FeAl composites fabricated by pulse current sintering technique
Source abstract
Abstract
Abstract WC–FeAl composites having notable mechanical properties as hard metal materials are successfully fabricated by using pulse current sintering technique. The relationship between hardness H V and fracture toughness K IC of the composites is compared with those of WC–Co materials reported. The comparison suggests successful development of WC–FeAl composites with the characteristics almost equal to WC–Co materials currently used for the hard metal tools. Microstructure of the sintered WC–FeAl is uniform without any grain growth. In the K IC – H V plot, WC–FeAl composites locate at the same position as that of WC–Co materials. The total mechanical property of WC–FeAl is comparable to WC–Co. The developed WC–FeAl is a very promising candidate to replace WC–Co materials. Fully controlled microstructure is crucial.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (23)
Show source-provided references
1. Synthesis of full-density nanocrystalline tungsten carbide by reduction of tungstic oxide at room temperature10.1007/BF02595669 ↗
2. Densification of ultrafine WC–12Co cermets by pressure assisted fast electric sintering10.1016/j.ijrmhm.2009.10.007 ↗
3. Sintering of nanophase WC–15vol.%Co hard metals by rapid sintering process10.1016/j.ijrmhm.2004.06.006 ↗
4. Properties of ultra-fine grain binderless cemented carbide ‘RCCFN’10.1016/0263-4368(95)92676-B ↗
5. Based WC composites prepared by combustion synthesis
6. Liquid-phase sintered iron aluminide–ceramic composites10.1016/S0966-9795(96)00066-0 ↗
7. Preparation and mechanical property for WC–25vol%FeAl using wet milling process10.2497/jjspm.57.764 ↗
8. The fracture toughness of WC/Co alloys measured on single-edge notched beam specimens precracked by electron discharge machining10.1016/0025-5416(78)90164-7 ↗
9. Validation of the Palmqvist indentation approach to toughness determination in WC/Co composites10.1016/0272-8842(89)90024-2 ↗
10. New results on the relationship between hardness and fracture toughness of WC/Co hardmetal10.1016/0921-5093(95)10112-8 ↗
11. Hardness to toughness relationship of fine-grained WC/Co hardmetals10.1016/S0263-4368(98)00028-6 ↗
12. Correlation of transverse rupture strength of WC/Co with hardness10.1016/j.ijrmhm.2004.11.005 ↗
13. Microstructure and mechanical properties of nanocrystalline WC–12Co consolidated by spark plasma sintering10.1016/j.ijrmhm.2006.03.008 ↗
14. VC, Cr3C2 and NbC doped WC/Co cemented carbides prepared by pulsed electric current sintering10.1016/j.ijrmhm.2006.11.003 ↗
15. Mechanical test discriminability for WC hardmetals10.1016/0263-4368(92)90055-7 ↗
16. Microstructure and mechanical properties of WC–TiN–Co and WC–TiN–Mo2C–Co(Ni) cemented carbides10.1016/0272-8842(92)90082-O ↗
17. Microstructure, hardness and toughness of nanostructured and conventional WC/Co composites10.1016/S0965-9773(98)00123-8 ↗
18. Evaluation of KIC of brittle solids by the indentation method with low crack-to-indent ratios10.1007/BF00724706 ↗
19. The deformation and ageing of mild steel: III Discussion of results10.1088/0370-1301/64/9/303 ↗
20. The cleavage of polycrystals
21. Tabor · 1951
22. Charpy impact energy of nanocrystalline and polycrystalline cobalt10.1016/j.scriptamat.2006.10.018 ↗
23. Nickel and iron aluminides: an overview on properties, processing, and applications10.1016/0966-9795(95)00056-9 ↗