journal article·2023-01

Porosity reduction in WC-12Co laser cladding by aluminum addition

Takuto Yamaguchi, Keigo Tanaka, Hideki Hagino

Publisher page

Abstract

Laser cladding of WC-Co cermet materials has been limited by defects such as pores and cracks. Especially, numerous pores with a large size in clad beads are typical defects in laser cladding of WC-Co, in comparison with other cladding materials. Previous studies show that pores in WC-Co laser clad beads are generated from CO gas reaction between oxygen and carbon dissociated from WC. CO gas formation also leads to decarburization of WC-Co, resulting in a brittle phase such as W 2C or M 6 C. In this study, we attempted to add an element with a strong affinity for oxygen to reduce porosity by preventing CO gas formation. We prepared an aluminum-added stainless steel substrate by laser alloying, followed by laser cladding of WC-Co on the laser-alloyed substrate. The addition of aluminum drastically reduced pores in the clad bead. The clad bead on the laser-alloyed substrate contained Al-oxide particles with a sub-micron size. Oxygen elements can be trapped as solid state Al-oxide before CO gas formation, contributing to lower porosity. Preventing CO gas formation also resulted in the microstructure without any W 2C.
Source: expertdata · Quality: candidate unverified · Source record ↗

Research context

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (29)

Show source-provided references
1. Additive manufacturing of functionally graded metallic materials using laser metal deposition
2. Arias-González · 2021
3. A review of additive manufacturing of cermets
4. Effects of laser-beam defocus on microstructural features of compositionally graded WC/Co-alloy composites additively manufactured by multi-beam laser directed energy deposition10.1038/s41598-020-65429-8 ↗
5. The influence of working distance on laser deposited WC-Co10.1016/j.jmatprotec.2009.01.016 ↗
6. Impact of localized surface preheating on the microstructure and crack formation in laser direct deposition of Stellite 1 on AISI 4340 steel10.1016/j.apsusc.2010.09.003 ↗
7. Calculating the stress of multi-track formations in induction-assisted laser cladding, ICALEO 2012 - 31st
8. Microstructure evolution of laser clad layers of W-C-Co alloy powders10.1016/S0257-8972(00)00909-9 ↗
9. Structure of laser cladded tungsten carbide composite coatings10.1016/S0924-0136(00)00790-1 ↗
10. Cladding of WC-12 co on low carbon steel using a pulsed Nd:YAG laser10.1016/j.msea.2007.01.132 ↗
11. An empirical-statistical model for laser cladding of WC-12Co powder on AISI 321 stainless steel10.1016/j.optlastec.2017.06.026 ↗
12. Influence of using electroless Ni-P coated WC-Co powder on laser cladding of stainless steel10.1016/j.surfcoat.2018.05.016 ↗
13. Microstructure and wear resistance of WC-Co by three consolidation processing techniques10.1016/j.ijrmhm.2008.07.002 ↗
14. Microstructure and wear properties of laser deposited WC-12%Co composites10.1016/j.msea.2010.07.006 ↗
15. Effects of the ambient oxygen concentration on WC-12Co cermet coatings fabricated by laser cladding10.1016/j.optlastec.2021.106922 ↗
16. Holappa · 2014
17. Metallurgical effects of the weld thermal cycle10.1533/9781845694869.169 ↗
18. Laser surface alloying: a bibliography10.1007/BF00980743 ↗
19. Wear and oxidation properties of titanium aluminides formed on titanium surface by laser alloying10.1016/0921-5093(93)90507-B ↗
20. Hardening of 316L stainless steel by laser surface alloying10.1007/BF00351880 ↗
21. Formation of titanium carbide layer by laser alloying with a light-transmitting resin10.1016/j.optlaseng.2016.07.007 ↗
22. Microstructure and corrosion studies on different zones of super duplex stainless steel UNS S32750 weldment10.3389/fmats.2020.00251 ↗
23. Ferrite/austenite stabilizing parameter of alloying elements in steel at 200 ∼ 500°C10.2320/matertrans1960.15.217 ↗
24. Hardness and Young’s modulus distributions in atmospheric plasma sprayed WC-Co coatings using nanoindentation10.1016/j.surfcoat.2011.03.012 ↗
25. Development of WC-Co coatings deposited by warm spray process10.1007/s11666-008-9271-4 ↗
26. Study of carbide dissolution into the matrix during laser cladding of carbon steel plate with tungsten carbides-stellite powders10.2351/1.4906480 ↗
27. Effect of powder structure on the structure of thermally sprayed WC-Co coatings10.1007/BF00367900 ↗
28. Microstructural evolution in thermally sprayed WC-Co coatings: comparison between nanocomposite and conventional starting powders10.1016/S1359-6454(99)00440-1 ↗
29. Kubaschewski · 1993