journal article·2025-12

The effect of TaC on the friction and Wear performance and oxidation resistance of WC–co cemented carbides

Zeyi Hu, Yinchun Xiao, Caihe Fan, Rui Zuo, Jiangxiong Gao, Xiaoliang Lin, Yiling Lu

Publisher page

Abstract

No abstract is available for this record. The assistant can identify its topic from the title, but cannot infer the study’s results.

Source: Not provided · Quality: missing

References (44)

Show source-provided references
1. Additive manufacturing of WC-co cemented carbides: process, microstructure, and mechanical properties
2. Ultrafine/nano WC-co cemented carbide: overview of preparation and key technologies10.1016/j.jmrt.2023.10.315 ↗
3. Approaching the 100th anniversary of the Hardmetal invention: from first WC-co samples towards modern advanced Hardmetal grades10.1016/j.ijrmhm.2023.106113 ↗
4. Preparation, properties and microstructure of high hardness WC-co cemented carbide tool materials for ultra-precision machining10.1016/j.ijrmhm.2023.106356 ↗
5. WC-co-re cemented carbides: structure, properties and potential applications10.1016/j.ijrmhm.2018.10.001 ↗
6. Fabrication and performances of WC-co cemented carbide with a low cobalt content10.1111/ijac.13966 ↗
7. Outstanding high-temperature oxidation-and wear-resistance of WC based cermets10.1016/j.jmst.2022.12.071 ↗
8. Mechanism of the early stages of oxidation of WC–co cemented carbides10.1016/j.corsci.2015.11.007 ↗
9. The selective oxidation behaviour of WC–co cemented carbides during the early oxidation stage10.1016/j.corsci.2015.02.033 ↗
10. Grain growth behaviour and mechanical properties of coarse-grained cemented carbides with bimodal grain size distributions10.1016/j.msea.2020.140586 ↗
11. The WC-co/Fe–Ni interface: effect of holding time on the microstructure, grain size and grain growth mechanism10.1016/j.ceramint.2019.08.031 ↗
12. Sliding wear behavior of nanostructured WC–co–Cr coatings10.1016/j.apsusc.2015.07.144 ↗
13. Sliding wear of conventional and suspension sprayed nanocomposite WC-co coatings: an invited review10.1007/s11666-021-01185-z ↗
14. Influences of the compositions and mechanical properties of HVOF sprayed bimodal WC-co coating on its high temperature wear performance10.1016/j.ijrmhm.2017.08.012 ↗
15. Friction and wear behavior of laser cladded WC-co and Ni/WC-co deposits at high temperature10.1016/j.ijrmhm.2019.02.025 ↗
16. Sliding wear behavior of nanostructured WC–co–Cr coatings10.1016/j.apsusc.2015.07.144 ↗
17. Sintering of the WC-6% co cemented carbides for improved mechanical and cutting performance using Micro-FAST10.1016/j.ijrmhm.2021.105545 ↗
18. Microstructure and properties of ultrafine WC–co–VC cemented carbides with different co contents10.1007/s12598-014-0424-y ↗
19. Effect of grain size on oxidation resistance of WC-6wt% co cemented carbide sintered by spark plasma sintering10.1016/j.ijrmhm.2023.106108 ↗
20. WC-co-TiNbZr composite with simultaneously high hardness and fracture toughness10.1016/j.ijrmhm.2023.106332 ↗
21. Microstructure, mechanical, electrochemical and tribological performances of WC-based cemented carbides with different NbC amounts10.1016/j.ijrmhm.2025.107099 ↗
22. Microstructural characteristics and wear-resistant mechanisms of WC-TiC-co coatings with varying TiC contents10.1016/j.ijrmhm.2024.106730 ↗
23. Tribological behavior of WC-co HVAF-sprayed composite coatings modified by nano-sized TiC addition10.1016/j.surfcoat.2018.09.017 ↗
24. Tensile creep of WC-10% co and WC-10% TaC-10% co alloys at elevated temperatures10.2320/matertrans1960.16.591 ↗
25. Effects of TaC on microstructure and mechanical properties of coarse grained WC–9Co cemented carbides10.1016/S1003-6326(15)63715-3 ↗
26. Mechanism of the effects of TaC and Cr3C2 on property of WC-co cemented carbides
27. The effect of NbC on mechanical properties and fracture behavior of WC–10Co cemented carbides10.1016/j.ijrmhm.2014.11.006 ↗
28. Effect of TaC and TiC on the friction and dry sliding wear of WC–6 wt.% co cemented carbides against steel counterfaces10.1016/j.ijrmhm.2013.02.009 ↗
29. High-temperature mechanical behavior of ultra-coarse cemented carbide with grain strengthening10.1016/j.jmst.2021.06.067 ↗
30. Strengthening cemented carbides by activated nano TaC10.1016/j.ijrmhm.2020.105449 ↗
31. General aspects and limits of conventional ultrafine WC powder manufacture and hard metal production10.1016/0263-4368(95)92674-9 ↗
32. Advanced and new grades of WC and binder powder–their properties and application10.1016/S0263-4368(00)00002-0 ↗
33. The influence of different content of (W, ta)C composite carbide on microstructure and properties of WC-10Co cemented carbide
34. Dry sliding wear behaviour of additive manufactured CrC-rich WC-co cemented carbides
35. Effects of grain refinement on internal oxidation of alloy 61710.1016/j.jnucmat.2010.05.013 ↗
36. High temperature fracture mechanism of ultrafine WC-co cemented carbides containing (Ti, W) C10.1016/j.ijrmhm.2020.105428 ↗
37. Thermal fatigue behaviour of WC-20Co and WC-30 (CoNiCrFe) cemented carbide10.1016/j.ijrmhm.2016.06.014 ↗
38. Compressive creep of coarse-grain WC–co and WC–TaC–co hardmetals with uniform microstructure comprising rounded WC grains10.1016/j.msea.2020.139998 ↗
39. Effects of VC/Cr3C2 on WC grain morphologies and mechanical properties of WC-6wt.% co cemented carbides10.1016/j.jallcom.2017.04.187 ↗
40. A new viewpoint on the influence mechanism of TaC additions on performance of WC-co cemented carbides
41. Seeding ductile nanophase in ceramic grains10.1039/D3MH02233A ↗
42. Study on the oxidation of WC-co cemented carbide under different conditions10.1016/j.ijrmhm.2020.105381 ↗
43. Effect of particle size on the oxidation of WC powders during heating10.1134/S0020168511020099 ↗
44. Oxidation of tungsten carbide powders in air10.1016/j.ijrmhm.2013.05.001 ↗