journal article·2022-01

Comparative study of WC-based hard alloys fabrication via spark plasma sintering using Co, Fe, Ni, Cr, and Ti binders

O.O. Shichalin, I.Yu. Buravlev, E.K. Papynov, A.V. Golub, A.A. Belov, A.A. Buravleva, V.N. Sakhnevich, M.I. Dvornik, N.M. Vlasova, A.V. Gerasimenko, V.P. Reva, A.A. Yudakov

Publisher page

Abstract

Abstract The paper presents a method of fabrication and a comparison of the characteristics of obtained cemented carbide samples based on tungsten carbide with 10% metal binder. They were synthesized by spark plasma sintering (SPS) at different sintering temperatures: Co (1200 °C), Fe and Ni (1150 °C), Cr (1500 °C), and Ti (1400 °C). During the SPS-consolidation process, investigations of the dilatometric characteristics of samples of starting powders of identical granulometric composition obtained by mixing/grinding resulting in the fractional composition in the particle size range up to 10 μm are presented. The mechanism of phase formation and microstructure of the obtained materials is investigated by XRD, SEM, and EDS. The possibility of synthesizing hard alloys WC – 10%Ti and WC – 10% Cr by the mechanism of reaction SPS synthesis with a reduction in the synthesis time in comparison with traditional sintering methods has been demonstrated. Analyses have shown that during sintering of alloys containing Ti and Cr the volume content of WC decreases to 47% because of dissolution and interaction, while in alloys containing Co, Ni, and Fe, the volume content of WC remains unchanged (85–86%). This led to a dramatic change in hardness, fracture toughness, and strength when replacing Co, Ni, or Fe with Ti or Cr.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (88)

Show source-provided references
1. History of hardmetals
2. Wear mechanisms in abrasion and erosion of WC/co and related hardmetals10.1016/j.wear.2006.12.046 ↗
3. The critical raw materials in cutting tools for machining applications: a review10.3390/ma13061377 ↗
4. Ablation resistance of tungsten carbide cermets under extreme conditions10.1016/j.ijrmhm.2020.105356 ↗
5. A candidate fusion engineering material, WC-FeCr10.1016/j.scriptamat.2018.06.027 ↗
6. Sintering of tungsten carbide cermets with an iron-based ternary alloy binder: processing and thermodynamic considerations10.1016/j.ijrmhm.2018.05.008 ↗
7. Modelling the power deposition into a spherical tokamak fusion power plant10.1088/1741-4326/57/3/036001 ↗
8. Design of cemented tungsten carbide and boride-containing shields for a fusion power plant10.1088/1741-4326/aabdb0 ↗
9. Cemented carbide phase diagrams: a review10.1016/j.ijrmhm.2011.02.004 ↗
10. Rapid sintering of ultrafine WC-Ni cermets10.1016/j.ijrmhm.2005.07.002 ↗
11. Formation of hard alloy VK8 using tungsten carbide powder synthesized by mechanochemical technology10.1007/s11148-013-9596-5 ↗
12. Shielding materials in the compact spherical tokamak10.1098/rsta.2017.0443 ↗
13. Rapid sintering of ultrafine WC–Ni cermets10.1016/j.ijrmhm.2005.07.002 ↗
14. Effects of metal binder content and carbide grain size on the microstructure and properties of SPS manufactured WC–Fe composites10.1016/j.jallcom.2019.01.057 ↗
15. Ultrafine WC-Ni cemented carbides fabricated by spark plasma sintering10.1016/j.msea.2011.10.119 ↗
16. Mechanical properties and microstructure of WC-Fe-Ni-co cemented carbides prepared by vacuum sintering10.1016/j.vacuum.2017.06.028 ↗
17. Study on the mechanical properties, microstructure and corrosion behaviors of nano-WC-co-Ni-Fe hard materials through HIP and hot-press sintering processes10.1016/j.msea.2014.08.081 ↗
18. Study on the sintered characteristics and properties of nanostructured WC-15 wt% (Fe-Ni-Co) and WC-15 wt% Co hard metal alloys10.1016/j.jallcom.2015.07.119 ↗
19. Characterization and properties of sintered WC–Co and WC–Ni–Fe hard metal alloys10.1016/j.jallcom.2013.09.188 ↗
20. A comparative study of the dry sliding wear of WC-10wt.%(Co+Fe+Ni) cemented carbides pressureless sintered with different Fe/Co ratios
21. Liu · 2014 · 113
22. Mechanical and microstructural properties of WC-based cermets: a comparative study on the effect of Ni and Mo binder phases10.1016/j.ceramint.2017.10.189 ↗
23. Study of characteristics and properties of spark plasma sintered WC with the use of alternative Fe-Ni-Nb binder as Co replacement10.1016/j.ijrmhm.2020.105316 ↗
24. Versatility of the sputtering technique in the processing of WC-Fe-Ni-Cr composites10.1016/j.surfcoat.2012.05.093 ↗
25. High-frequency induction-heated consolidation of nanostructured WC and WC-Al hard materials and their mechanical properties10.1016/j.ijrmhm.2016.07.024 ↗
26. Effect of Al on sintering and mechanical properties of WC-Al composites10.1016/j.ceramint.2016.07.050 ↗
27. Effect of chromium and carbon contents on the sintering of WC-Fe-Ni-Co-Cr multicomponent alloys10.1016/j.ijrmhm.2020.105317 ↗
28. Microstructure and mechanical properties of WC Ni-Si based cemented carbides developed by powder metallurgy10.1016/j.ijrmhm.2010.04.003 ↗
29. Comparison between ultrafine-grained WC–co and WC–HEA-cemented carbides10.1080/00325899.2016.1260903 ↗
30. Fabrication and characterization of WC-HEA cemented carbide based on the CoCrFeNiMn high entropy alloy10.1016/j.jallcom.2018.02.292 ↗
31. SPS hard metal alloy WC-8Ni-8Fe fabrication based on mechanochemical synthetic tungsten carbide powder10.1016/j.jallcom.2019.152547 ↗
32. Microstructure and mechanical properties and of pulse plasma compacted WC - Co10.1016/j.ijrmhm.2016.07.002 ↗
33. Microstructure and mechanical properties of WC–co, WC–co–Cr3C2 and WC–co–TaC cermets fabricated by spark plasma sintering10.1016/S1003-6326(16)64390-X ↗
34. Effect of Co content on microstructure and mechanical properties of ultrafine grained WC-Co cemented carbide sintered by spark plasma sintering10.1016/j.ceramint.2018.07.100 ↗
35. Perspectives on the spark plasma sintering process
36. Spark plasma sintering of special-purpose functional ceramics based on UO2, ZrO2, Fe3O4/α-Fe2O310.1134/S1087659618060159 ↗
37. What’s new in ceramics sintering? A short report on the latest trends and future prospects10.1016/j.cossms.2020.100868 ↗
38. Fabrication of magnesium-boron carbide metal matrix composite by powder metallurgy route: comparison between microwave and spark plasma sintering10.1016/j.jallcom.2016.12.146 ↗
39. The effect of electric field and pressure on the synthesis and consolidation of materials: a review of the spark plasma sintering method10.1007/s10853-006-6555-2 ↗
40. Spark plasma sintering as a high-tech approach in a new generation of synthesis of nanostructured functional ceramics10.1134/S1995078017010086 ↗
41. Spark plasma sintering of nanopowders in the CeO2-Y2O3 system as a promising approach to the creation of nanocrystalline intermediate-temperature solid electrolytes10.1016/j.ceramint.2018.07.249 ↗
42. Preparation and investigation of ultrafine-grained tungsten carbide with high hardness and fracture toughness10.1134/S1028335815070095 ↗
43. High-strength ultrafine-grained tungsten-carbide-based materials obtained by spark plasma sintering10.1134/S1063785015040203 ↗
44. Field-assisted sintering technology/spark plasma sintering: mechanisms, materials, and technology developments
45. Combustion synthesis and the electric field: a review10.3103/S1061386217030037 ↗
46. Spark plasma sintering as advanced PM sintering method10.1179/003258902225007041 ↗
47. Variation in strength, hardness, and fracture toughness in transition from medium-grained to ultrafine hard alloy
48. Sparking plasma sintering of tungsten carbide nanopowders10.1134/S1995078015030040 ↗
49. High-speed electropulse plasma sintering of nanostructured tungsten carbide: Part 1. Experiment10.3103/S1067821214060066 ↗
50. Spark plasma sintering of tungsten carbide nanopowders obtained through DC arc plasma synthesis10.1016/j.jallcom.2017.03.035 ↗
51. Spark Plasma Sintering of fine-grain ceramic-metal composites based on garnet-structure oxide Y2.5Nd0.5Al5O12 for inert matrix fuel10.1016/j.matchemphys.2018.03.091 ↗
52. Characterization of Nax(ca/Sr)1-2xNdxWO4 complex tungstates fine-grained ceramics obtained by spark plasma sintering10.1016/j.ceramint.2017.11.199 ↗
53. Sol-gel synthesis and characterization of ZnAl2O4 powders for transparent ceramics10.1016/j.ceramint.2018.11.179 ↗
54. Synthesis of BaCe0.9-xZrxY0.1O3-Δ nanopowders and the study of proton conductors fabricated on their basis by low-temperature spark plasma sintering10.1016/j.ijhydene.2019.05.231 ↗
55. Nanostructured sintered WC–Co hard metals (review)10.1007/s11106-015-9670-2 ↗
56. Synthesis of high-density pellets of uranium dioxide by spark plasma sintering in dies of different types10.1134/S1066362218040045 ↗
57. Reactive spark plasma synthesis of porous bioceramic Wollastonite10.1134/S0036023620020138 ↗
58. Y. Jiang, J.F. Yang, Z.M. Xie, R. Gao, Q.F. Fang, Corrosion resistance of W-Cr-C coatings fabricated by spark plasma sintering method, Surf. Coat. Technol. 254 (2014) 202–206. doi:https://doi.org/10.1016/j.surfcoat.2014.06.012.10.1016/j.surfcoat.2014.06.012 ↗
59. Thermodynamic calculation designed compositions, microstructure and mechanical property of ultra-fine WC-10Co-Cr3C2-TaC cemented carbides10.1016/j.ijrmhm.2017.07.012 ↗
60. Development of advanced high heat flux and plasma-facing materials10.1088/1741-4326/aa6f71 ↗
61. Microstructure and cyclic oxidation behavior of W–Cr alloys prepared by sintering of mechanically alloyed nanocrystalline powders10.1016/j.ijrmhm.2012.08.015 ↗
62. Oxidation behaviour of bulk W-Cr-Ti alloys prepared by mechanical alloying and HIPing10.1016/j.fusengdes.2014.04.057 ↗
63. Revisiting the possibility of formation of hard alloys from powder mixtures of carbides with metals by explosive compacting without sintering10.3103/S1067821218050073 ↗
64. Spark plasma sintering (SPS) method, systems, and applications
65. Consolidation enhancement in spark-plasma sintering: impact of high heating rates10.1063/1.2822189 ↗
66. The synthesis of nanostructured WC-based hardmetals using mechanical alloying and their direct consolidation10.1155/2014/640750 ↗
67. Research of surfaces and interfaces increasing during planetary ball milling of nanostructured tungsten carbide/cobalt powder10.1016/j.ijrmhm.2012.10.004 ↗
68. The influence of the rotation frequency of a planetary ball mill on the limiting value of the specific surface area of the WC and co nanopowders10.1016/j.apt.2020.07.033 ↗
69. Simultaneous spark plasma sintering of multiple complex shapes10.3390/ma12040557 ↗
70. All-Materials-inclusive flash spark plasma sintering10.1038/s41598-017-15365-x ↗
71. Densification mechanism and mechanical properties of tungsten powder consolidated by spark plasma sintering10.1016/j.ijrmhm.2016.07.023 ↗
72. The spatial distribution of temperature and oxygen deficiency in spark-plasma sintered superconducting Bi-based materials10.1016/j.physb.2014.07.040 ↗
73. Numerical simulation of heat transfer during spark plasma sintering of zirconium diboride10.1016/j.ceramint.2019.10.240 ↗
74. Neck formation and self-adjusting mechanism of neck growth of conducting powders in spark plasma sintering10.1111/j.1551-2916.2005.00777.x ↗
75. Effect of electric current on densification behavior of conductive ceramic powders consolidated by spark plasma sintering10.1016/j.actamat.2017.11.010 ↗
76. Spark plasma sintering of zirconium carbide and oxycarbide: finite element modeling of current density, temperature, and stress distributions10.1557/JMR.2009.0039 ↗
77. A review of multi-physical fields induced phenomena and effects in spark plasma sintering: fundamentals and applications10.1016/j.matdes.2020.108662 ↗
78. Current-activated, pressure-assisted densification of materials10.1146/annurev-matsci-070909-104433 ↗
79. Temperature distribution and neck formation of WC–Co combined particles during spark plasma sintering10.1016/j.msea.2008.01.048 ↗
80. Spark plasma sintering densification mechanism for cemented carbides with different WC particle sizes10.1111/j.1551-2916.2010.03862.x ↗
81. Rapid sintering process and mechanical properties of binderless ultra fine tungsten carbide10.1016/j.msea.2006.07.127 ↗
82. Sintering behavior and mechanical properties of WC-10Co, WC-10Ni and WC-10Fe hard materials produced by high-frequency induction heated sintering10.1016/j.ceramint.2007.11.003 ↗
83. Reactive spark plasma sintering of binderless WC ceramics at 1500°C
84. Mechanical properties, phases and microstructure of ultrafine hardmetals prepared by WC–6.29Co nanocrystalline composite powder10.1016/j.msea.2004.09.043 ↗
85. Kurlov · 2013
86. WC-5TiC-10Co hard metal alloy fabrication via mechanochemical and SPS techniques10.1016/j.ijrmhm.2020.105385 ↗
87. Development of a method for producing submicron cemented carbide from a powder obtained by electrical discharge erosion of scrap in oil10.1016/j.powtec.2021.01.048 ↗
88. Correlation of transverse rupture strength of WC–Co with hardness10.1016/j.ijrmhm.2004.11.005 ↗