journal article·2024-02

Grain boundary strengthening in nanocrystalline Mo0.2CoNi medium-entropy alloys produced via high-pressure torsion

Juyeon Han, Seungjin Nam, Yeon Taek Choi, Tae Jin Jang, Chahee Jung, Seok Su Sohn, Hyoung Seop Kim, Hyunjoo Choi

Publisher page

Abstract

In this study, we produced nanocrystalline (NC) MoCoNi-based medium-entropy alloys (MEAs) with a single face-centered cubic (FCC) phase, which exhibit exceptional hardness through combining compositional and microstructural features of alloys. The alloys were prepared via powder metallurgy and high-pressure torsion, and the processing condition was optimized to achieve full densification and prevent grain growth in order to maximize the effect of grain boundary strengthening. Consequently, NC Mo 0.2CoNi MEAs revealed the refined microstructures with a grain size of approximately 50 nm and outstanding hardness of 857 HV (corresponding to approximately 2.86 GPa in yield strength). This remarkable property, even compared to the single FCC phase alloys with similar grain size, is attributed to the existence of alloying elemental atoms of Mo with large atomic radius, which leads to severe lattice distortion allows to improve friction stress as well as the Hall-Petch coefficient. This study aims to discuss the potential of developing hard metallic materials by using grain boundary strengthening from alloys with large atomic size difference.
Source: expertdata · Quality: candidate unverified · Source record ↗

Research context

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (50)

Show source-provided references
1. Fabrication methods of particulate reinforced aluminium metal matrix composite-a review10.1016/j.matpr.2017.12.194 ↗
2. Hall–Petch relation and boundary strengthening10.1016/j.scriptamat.2004.06.002 ↗
3. Grain-boundary strengthening in nanocrystalline chromium and the Hall–Petch coefficient of body-centered cubic metals10.1016/j.scriptamat.2012.09.025 ↗
4. A continuum theory of stress gradient plasticity based on the dislocation pile-up model10.1016/j.actamat.2014.07.043 ↗
5. Estimation of micro-Hall-Petch coefficients for prismatic slip system in Mg-4Al as a function of grain boundary parameters10.1016/j.actamat.2021.117613 ↗
6. Six decades of the Hall–Petch effect – a survey of grain-size strengthening studies on pure metals10.1080/09506608.2016.1191808 ↗
7. A critical review of high entropy alloys and related concepts10.1016/j.actamat.2016.08.081 ↗
8. Phase selection, lattice distortions, and mechanical properties in high-entropy alloys10.1002/adem.202000466 ↗
9. Deformation behavior of nanocrystalline and ultrafine-grained CoCrCuFeNi high-entropy alloys10.1557/jmr.2018.477 ↗
10. Optimizing the coupled effects of hall-Petch and precipitation strengthening in a Al0.3CoCrFeNi high entropy alloy10.1016/j.matdes.2017.02.072 ↗
11. Effects of cryogenic temperature on tensile and impact properties in a medium-entropy VCoNi alloy10.1016/j.jmst.2021.02.034 ↗
12. Ultra-strong and strain-hardenable ultrafine-grained medium-entropy alloy via enhanced grain-boundary strengthening10.1080/21663831.2021.1913768 ↗
13. Ultrastrong medium-entropy single-phase alloys designed via severe lattice distortion10.1002/adma.201807142 ↗
14. Mechanical properties, microstructure and thermal stability of a nanocrystalline CoCrFeMnNi high-entropy alloy after severe plastic deformation10.1016/j.actamat.2015.06.025 ↗
15. Severe plastic deformation on powder metallurgy Cu–Al–Ni shape memory alloys10.1016/j.matpr.2015.07.390 ↗
16. Effect of grain refinement on mechanical properties of ball-milled bulk aluminum10.1016/j.msea.2008.01.045 ↗
17. Microstructure and strengthening mechanisms in an FCC structured single-phase nanocrystalline Co25Ni25Fe25Al7.5Cu17.5 high-entropy alloy10.1016/j.actamat.2016.01.050 ↗
18. Densification and grain growth during sintering of nanosized particles10.1179/174328008X353538 ↗
19. Study of friction stir processing (FSP) and high pressure torsion (HPT) and their effect on mechanical properties10.1016/j.proeng.2011.04.482 ↗
20. Superior cryogenic tensile properties of ultrafine-grained CoCrNi medium-entropy alloy produced by high-pressure torsion and annealing10.1016/j.scriptamat.2019.01.016 ↗
21. On the enhanced hardening ability and plasticity mechanisms in a novel Mn-added CoCrNi medium entropy alloy during high-pressure torsion10.1016/j.jallcom.2022.163941 ↗
22. Effect of high energy ball milling on the morphology, microstructure and properties of nano-sized TiC particle-reinforced 6005A aluminium alloy matrix composite10.1016/j.powtec.2017.07.089 ↗
23. Lightweight AlCuFeMnMgTi high entropy alloy with high strength-to-density ratio processed by powder metallurgy10.1007/s12540-020-00823-5 ↗
24. A new class of high strength high temperature Cobalt based γ–γ′ Co–Mo–Al alloys stabilized with Ta addition10.1016/j.actamat.2015.06.034 ↗
25. Self-assembled network structures in Al/C60 composites10.1016/j.carbon.2010.06.013 ↗
26. Nanostructure formation mechanism during in-situ consolidation of copper by room-temperature ball milling
27. On the homogeneity of deformation by high pressure torsion10.1016/j.scriptamat.2004.04.025 ↗
28. Deformation twinning10.1016/0079-6425(94)00007-7 ↗
29. Deformation twinning and the Hall–Petch relation in commercial purity Ti10.1007/s11661-007-9442-9 ↗
30. Influence of grain size and stacking-fault energy on deformation twinning in fcc metals10.1007/s11661-999-0272-9 ↗
31. Grain size effect on deformation twinning and detwinning10.1007/s10853-013-7140-0 ↗
32. Role of supersaturated Al-C phases in mechanical properties of Al/fullerene composites10.1038/s41598-021-92551-y ↗
33. Combination of enhanced strength and sufficient tensile ductility in a sintered ultrafine-grained CoFeMnNi medium-entropy alloy10.1016/j.msea.2021.142175 ↗
34. Deformation behavior of nanocrystalline and ultrafine-grained CoCrCuFeNi high-entropy alloys10.1557/jmr.2018.477 ↗
35. Effect of Ti on phase stability and strengthening mechanisms of a nanocrystalline CoCrFeMnNi high-entropy alloy10.1016/j.msea.2018.04.014 ↗
36. A nanocrystalline AlCoCuNi medium-entropy alloy with high thermal stability via entropy and boundary engineering10.1016/j.msea.2020.138925 ↗
37. Ultrafine-grained AlCoCrFeNi2.1 eutectic high-entropy alloy10.1080/21663831.2016.1160451 ↗
38. High-strength ultrafine-grained CoCrFeNiNb high-entropy alloy prepared by mechanical alloying: properties and strengthening mechanism10.1016/j.jallcom.2020.155308 ↗
39. Strengthening of Al0.15CoCrCuFeNiTix–C (x = 0, 1, 2) high-entropy alloys by grain refinement and using nanoscale carbides via powder metallurgical route10.1016/j.jallcom.2018.05.180 ↗
40. Thermal stability and grain boundary strengthening in ultrafine-grained CoCrFeNi high entropy alloy composite10.1016/j.matdes.2017.08.053 ↗
41. Superior high tensile elongation of a single-crystal CoCrFeNiAl0.3 high-entropy alloy by Bridgman solidification10.1016/j.intermet.2014.05.018 ↗
42. Solid solution softening in a Al0.1CoCrFeMnNi high-entropy alloy10.1016/j.scriptamat.2020.04.034 ↗
43. Effect of a minor titanium addition on the superplastic properties of a CoCrFeNiMn high-entropy alloy processed by high-pressure torsion10.1016/j.msea.2018.02.002 ↗
44. Positive deviation from a Hall-Petch relation in nanocrystalline aluminum10.2320/matertrans.MRA2008343 ↗
45. Microstructure, wear, and oxidation resistance of nanostructured carbide-strengthened cobalt-based composite coatings on Invar alloys by laser cladding10.1016/j.surfcoat.2019.125188 ↗
46. Effect of vanadium addition on the microstructure and properties of AlCoCrFeNi high entropy alloy10.1016/j.matdes.2013.12.048 ↗
47. Effects of lattice distortion and chemical short-range order on creep behavior of medium-entropy alloy CoCrNi10.1016/j.mechmat.2022.104549 ↗
48. A simplified model connecting lattice distortion with friction stress of Nb-based equiatomic high-entropy alloys10.1080/21663831.2019.1610105 ↗
49. Determination of grain size and lattice distortions in ground YBa2Cu3O710.1007/BF01117612 ↗
50. Ab initio investigation of the role of atomic radius in the structural formation of PtnTM55–n (TM = Y, Zr, Nb, Mo, and Tc) nanoclusters10.1021/acs.jpcc.7b05714 ↗