journal article·2001-07

Study of the mechanical properties of TiCN–WC–CO hardmetals by the interpretation of internal friction spectra

D. Mari, S. Bolognini, T. Viatte, W. Benoit

Publisher page

Abstract

Abstract TiCN–WC–Mo–Co mixed carbide hardmetals have an interesting application potential for cutting tool fabrication combining the high toughness of WC–Co with the resistance to plastic deformation of TiCN–Co cermets. Mechanical spectroscopy (MS) is used in order to separate the effects of the constituents on the mechanical properties. Internal friction (IF) spectra are measured in a torsion pendulum on WC–TiCN–Mo–Co samples where TiCN/WC ratio is varied as well as the Co content. Six components of the characteristic IF spectrum of WC–TiCN–Mo–Co have been identified and interpreted. Two peaks are located in the cobalt, two peaks in the TiCN phase and two peaks in the ceramic grain boundaries. Four temperature domains are defined depending on the mechanical behaviour: brittle (I), anelastic (IIa), limited plasticity (IIb) and extended plasticity (III). The anelastic domain is characterized by the bulk deformation of cobalt. In the limited plasticity domain, both cobalt and TiCN are deformed by dislocation movement. The high temperature extended plasticity should be attributed to grain boundary sliding in the ceramic phase (mainly WC) enhanced by cobalt diffusion in the grain boundaries.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (27)

Show source-provided references
1. Microstructure and high temperature mechanical properties of TiC0.7N0.3–Mo2C–Ni cermets10.1016/0921-5093(95)10100-4 ↗
2. Grain growth in TiC–Ni–Mo and TiC–Ni–W cemented carbides10.1179/pom.1976.19.4.210 ↗
3. Microstructural evolution during the sintering of TiC–Mo–Ni cermets10.1111/j.1151-2916.1993.tb08331.x ↗
4. Effect of carbon on the microstructure and mechanical properties of (Ti,W,Ta,Mo) (C,N)–(Co,Ni) cermets10.1016/S0263-4368(98)00074-2 ↗
5. A new look at carbide tool life10.1016/0043-1648(93)90366-T ↗
6. Experimental study of the mechanics of fracture in WC–Co alloys10.1007/BF02647199 ↗
7. On the fracture toughness of cemented carbides10.1016/0001-6160(88)90143-5 ↗
8. Comportement mécanique á haute température du métal dur et de différents cermets de coupe10.1051/mattech/199785090013 ↗
9. High temperature mechanical behaviour of Ti (C,N)–Mo–Co cermets10.1016/S0263-4368(98)00033-X ↗
10. The development of cubic-carbide-free surface layers in cemented carbides without nitrogen10.1016/0263-4368(93)90063-L ↗
11. Investigation into the potential of a composite combining toughness and plastic deformation resistance10.1016/S0263-4368(98)00044-4 ↗
12. Bolognini S, Mari D, Viatte T, Benoit W. Fracture toughness of coated WC–TiCN–Co cermets with graded composition. Int J Refract Metals Hard Mater, this conference
13. Experimental strategy to study the mechanical behaviour of hardmetals for cutting tools10.1016/S0263-4368(98)00078-X ↗
14. Nowick · 1972
15. Electrical properties of solids. VIII. Dipole moments in polyvinyl chloride–diphenyl systems10.1021/ja01847a013 ↗
16. Influence of a changing microstructure on high temperature relaxation peaks, an example: WC-11 wt% Co10.1016/0925-8388(94)90530-4 ↗
17. Bolognini S. Propriétés mécaniques á haute température de cermets Ti (C,N)–WC–Mo–Co à gradient de composition pour outils de coupe. Ph.D. Thesis EPFL No 2161, Lausanne, Switzerland, 2000
18. High temperature mechanical properties of TiC0.7N0.3–Mo2C–Ni cermets studied by internal friction measurements
19. Diffusion de quelques éléments de substitution dans le fer, le nickel et le cobalt
20. Microstructure and hardness of cobalt rich Co–W–C alloys after ageing in the range 400–1000°C
21. Feusier G. Etude des propriétés mécaniques à haute température des cermets Ti (C,N)–Mo–Co par mesures de flexion trois points. Ph.D. Thesis EPFL No 1659, Lausanne, Switzerland, 1997
22. Internal friction and microdeformation due to the intrinsic properties of dislocations: the bordoni relaxation10.1016/0079-6425(82)90003-2 ↗
23. Residual stress and stress distribution in a WC–Ni Composite10.1016/0921-5093(89)90531-5 ↗
24. Residual stress in WC–Co measured by neutron diffraction10.1016/0921-5093(95)10147-0 ↗
25. Hirth · 1982
26. The kink picture of dislocation mobility and dislocation-point-defect interactions
27. Gadaud P. Etude par Frottement Intérieur Haute Température des Défauts Structuraux dans le Silicium Monocristallin. Ph.D. Thesis, ENSMA, Poitiers, France, 1987