Flexural strength behavior of a ZrB2–TaB2 composite consolidated by non-reactive spark plasma sintering at 2300 °C

Dmytro Demirskyi, Oleg Vasylkiv

Publisher page

Abstract

Abstract A bulk zirconium–tantalum diboride ceramic composite was consolidated by non-reactive spark plasma sintering (SPS) at 2300 °C. In order to consolidate the ZrB 2 –44 wt% TaB 2 composite and restrict grain-growth, a special loading procedure was used. Pressure was applied and released at 2150 °C and 1250 °C, respectively. These SPS conditions allowed us to obtain a crack-free bulk composite with a grain size of 4–8 μm. Flexural strength at temperatures up to 1800 °C was measured for the ZrB 2 –TaB 2 composite. Importantly, at 1600 °C, the strength was 336 ± 23 MPa, which is superior to that of monolithic ZrB 2 . Moreover, the ZrB 2 –TaB 2 composite only showed plastic behavior at 1800 °C, a finding that is atypical for ZrB 2 -based ceramics.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (28)

Show source-provided references
1. Refractory diborides of zirconium and hafnium10.1111/j.1551-2916.2007.01583.x ↗
2. Boron, its compounds and alloys
3. Samsonov · 1957
4. Consolidation and grain growth of tantalum diboride during spark plasma sintering10.1016/j.ceramint.2016.07.059 ↗
5. Synthesis, densification, and mechanical properties of TaB210.1016/j.matlet.2008.06.052 ↗
6. Sintering of TaB2
7. Bulk monolithic zirconium and tantalum diborides by reactive and non-reactive spark plasma sintering10.1016/j.jallcom.2015.12.096 ↗
8. Strength, fracture mode, and thermal stress resistance of HfB2 and ZrB210.1111/j.1151-2916.1969.tb12655.x ↗
9. Research and Development of Refractory Oxidation-Resistant Diborides Part II, Volume IV: Mechanical Properties
10. Strength of zirconium diboride to 2300°C10.1111/jace.12114 ↗
11. Microstructure and high-temperature strength of textured and non-textured ZrB2 ceramics10.1088/1468-6996/15/1/014202 ↗
12. High-temperature bending strength, internal friction and stiffness of ZrB2–20vol% SiC ceramics10.1016/j.jeurceramsoc.2012.01.035 ↗
13. Ultra high temperature ceramics for hypersonic vehicle applications
14. Mechanical behavior of zirconium diboride–silicon carbide–boron carbide ceramics up to 2200°C10.1016/j.jeurceramsoc.2014.09.021 ↗
15. Elevated temperature strength enhancement of ZrB2-30vol% SiC ceramics by postsintering thermal annealing10.1111/jace.14029 ↗
16. Measurement of thermal residual stresses in ZrB2–SiC composites10.1016/j.jeurceramsoc.2011.03.024 ↗
17. High-strength TiB2–TaC ceramic composites prepared using reactive spark plasma consolidation10.1016/j.ceramint.2015.09.065 ↗
18. Hardness and toughness control of brittle boron suboxide ceramics by consolidation of star-shaped particles by spark plasma sintering10.1016/j.ceramint.2015.10.157 ↗
19. High-temperature strength of boron suboxide ceramic consolidated by spark plasma sintering10.1111/jace.14308 ↗
20. Demirskyi D., Vasylkiv O. Mechanical properties of SiC–NbB2 eutectic composites by in situ spark plasma sintering. Ceram. Int. (10.1016/j.ceramint.2016.09.110).10.1016/j.ceramint.2016.09.110 ↗
21. Ultra-high elevated temperature strength of TiB2-based ceramics consolidated by spark plasma sintering10.1016/j.jeurceramsoc.2016.08.009 ↗
22. Hot pressing
23. Hot-spots generation, exaggerated grain growth and mechanical performance of silicon carbide bulks consolidated by flash spark plasma sintering10.1016/j.jallcom.2016.08.234 ↗
24. High-temperature reaction consolidation of TaC–TiB2 ceramic composites by spark-plasma sintering10.1016/j.jeurceramsoc.2014.08.007 ↗
25. Sintering and properties of titanium diboride made from powder synthesized in a plasma-arc heater10.1111/j.1151-2916.1984.tb19744.x ↗
26. Touloukian · 1977 · 13
27. High-strength B4C–TaB2 eutectic composites obtained via in situ by spark plasma sintering10.1111/jace.14235 ↗
28. Zubarev · 1985