Abstract
Abstract Structural ceramics, including zirconium diborides, are brittle and sensitive to superficial flaws such as cracks and pores. These aspects, which can lead to unexpected catastrophic failure, are still the obstacles preventing the structural ceramics from being widely used. In this paper, a ZrB2 ceramic composite reinforced with SiC particles and ZrO2 fibers was prepared. The oxidation behavior and crack-healing ability of the ZrO2 fiber toughened ZrB2-based ceramics as a function of temperature and time were investigated. The results here indicate that the strength of the ZrO2 fiber toughened ZrB2-based ceramics was recovered to 1130 ± 32 MPa at the temperature of 1200 °C for 30 min, which was ~ 44 MPa higher than that of polished specimens, and the fracture toughness was also recovered to 6.92 ± 0.05 MPa·m1/2. The crack was completely healed with oxidation products consisting ZrO2 and SiO2. The good crack-healing ability of the ZrO2 fiber toughened ZrB2-based ceramics would make this composite highly useful as it could heal defects and flaws autonomously in practical applications.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (30)
Show source-provided references
1. Fabrication, mechanical properties and thermal shock resistance of a ZrB2-graphite ceramic10.1016/j.ijrmhm.2010.12.014 ↗
2. Gelcasting of complex shaped ZrB2–SiC ultra high temperature ceramic components10.1016/j.msea.2012.07.018 ↗
3. The repeated thermal shock behaviors of a ZrB2–SiC composite heated by electric resistance method10.1016/j.ijrmhm.2010.06.012 ↗
4. Crack healing behaviour and high-temperature strength of mullite/SiC composite ceramics10.1016/S0955-2219(01)00431-9 ↗
5. Crack healing, reopening and thermal expansion behavior of Al2TiO5 ceramics at high temperature10.1016/j.jeurceramsoc.2006.04.024 ↗
6. Crack-healing ability of structural ceramics and a new methodology to guarantee the structural integrity using the ability and proof-test10.1016/j.jeurceramsoc.2004.01.027 ↗
7. Preparation of ZrB2 based hybrid composites reinforced with SiC whiskers and SiC particles by hot-pressing10.1016/j.ijrmhm.2009.01.002 ↗
8. Microstructure, mechanical properties and thermal shock resistance of zirconium diboride containing silicon carbide ceramic toughened by carbon black10.1016/j.matchemphys.2010.03.028 ↗
9. Pressureless sintering of ZrO2–ZrB2 composites: microstructure and properties10.1016/j.ijrmhm.2006.04.006 ↗
10. Crack-healing behavior of zirconium diboride composite reinforced with silicon carbide whiskers10.1016/j.scriptamat.2008.08.013 ↗
11. Preoxidation and crack-healing behavior of ZrB2–SiC ceramic composite10.1111/j.1551-2916.2008.02760.x ↗
12. The influence of annealing on the strength of corundum
13. Crack healing and strengthening of thermally shocked alumina10.1111/j.1151-2916.1976.tb10949.x ↗
14. Crack healing in UO210.1111/j.1151-2916.1973.tb12499.x ↗
15. Crack healing by heat treatment10.1111/j.1151-2916.1970.tb12002.x ↗
16. Crack-healing behavior and resultant strength properties of silicon carbide ceramic10.1016/j.jeurceramsoc.2004.01.021 ↗
17. Effects of oxidation under load on strength distribution of Si3N410.1111/j.1151-2916.1982.tb10451.x ↗
18. Oxidation-induced crack healing in Ti3AlC2 ceramics10.1016/j.scriptamat.2007.09.006 ↗
19. The oxidation behaviors of a ZrB2–SiC–ZrC ceramic10.1016/j.solidstatesciences.2010.12.022 ↗
20. Effect of surface oxidation on thermal shock resistance of ZrB2–SiC–G composite10.1016/j.ijrmhm.2009.10.013 ↗
21. A technique for ultrahigh temperature oxidation studies of ZrB2–SiC10.1016/j.matlet.2008.01.124 ↗
22. Influence of milling time on the synthesis, microstructure and mechanical properties of ZrB2–SiC–ZrO2f ceramic composites10.1016/j.ceramint.2012.11.003 ↗
23. Transformation toughness in zirconia-containing ceramics10.1111/j.1151-2916.2000.tb01221.x ↗
24. Garvie · 1975
25. A critical evaluation of indentation techniques for measuring fracture toughness: I, direct crack measurements10.1111/j.1151-2916.1981.tb10320.x ↗
26. R-curve behavior, mechanical properties and microstructure of sintered ZrB2–SiCp–ZrO2f ceramics10.1016/j.jeurceramsoc.2012.01.028 ↗
27. Oxidation of zirconium diboride–silicon carbide at 1500°C at a low partial pressure of oxygen10.1111/j.1551-2916.2006.01229.x ↗
28. Oxidation behavior of a pressureless sintered ZrB2–MoSi2 ceramic composite10.1557/JMR.2005.0111 ↗
29. Pecharsky · 2009
30. A computational analysis of a ZrO2–SiO2 scale for a ZrB2–ZrC–Zr ultrahigh temperature ceramic composite system10.1016/j.jeurceramsoc.2010.02.027 ↗