The oxidation behavior of high Cr and Al containing Nb-Si-Ti-Hf-Al-Cr alloys at 1200 and 1250 °C
Source abstract
Abstract
Abstract The oxidation behavior of two alloys containing different content of Al and Cr from the Nb-Si-Ti-Hf-Al-Cr system has been evaluated at 1200 and 1250 °C. The alloy compositions in atomic percent are Nb-24Ti-16Si-2Hf-2Al-10Cr (B1), and Nb-24Ti-16Si-2Hf-6Al-17Cr (B2). The oxidation kinetic of B1 alloy at 1200 and 1250 °C followed a mixed parabolic-linear law, while the oxidation kinetic of B2 alloy at 1200 and 1250 °C followed a parabolic law. The weight gain of B2 alloy was 18.9 mg/cm 2 after oxidation at 1200 °C for 100 h, which was a seventh of the value of that of B1 alloy. Besides, oxidation became more severe as temperature increased to 1250 °C. The oxide scales of B2 alloy consisted of CrNbO 4 , TiNb 2 O 7 and SiO 2 , which were relatively compact and protective. In addition, the oxidation mechanism of Nb-Si based alloys were also discussed.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (31)
Show source-provided references
1. The hotter the engine, the better10.1126/science.1179327 ↗
2. A review of very-high temperature Nb-silicide-based composites10.1007/s11661-003-0269-8 ↗
3. The balance of mechanical and environmental properties of a multi-element niobium-niobium silicide-based in-situ composite10.1007/BF02595629 ↗
4. Oxidation of Nb-Si-Cr-Al in situ composites with Mo, Ti and Hf additions10.1016/j.msea.2006.08.093 ↗
5. Experimental study and modeling of high temperature oxidation of Nb-base in situ composites10.1016/j.corsci.2008.11.004 ↗
6. The effects of uncommon silicides on the oxidation behavior of alloys from the Nb-Cr-Si system10.1016/j.corsci.2012.04.029 ↗
7. Ultrahigh temperature materials for jet engines10.1557/mrs2003.189 ↗
8. Microstructure and room-temperature fracture toughness of directionally solidified Nb-Si-Ti-Cr-Al-Hf alloy10.1016/j.msea.2012.10.011 ↗
9. Effect of Al, Cr and Ta additions on the oxidation behaviour of Nb-Ti-Si in situ composites at 800°C10.1016/j.msea.2005.10.017 ↗
10. Room temperature mechanical properties and high temperature oxidation resistance of a high Cr containing Nb-Si based alloy10.1016/j.msea.2014.11.001 ↗
11. Rapid fabrication of Nb-Si based alloy by selective laser melting: microstructure, hardness and initial oxidation behavior10.1016/j.matdes.2016.07.048 ↗
12. Oxidation of refractory metals in air and low pressure oxygen gas10.1016/S0263-4368(00)00026-3 ↗
13. Effect of boronizing on the oxidation of niobium10.1016/j.ijrmhm.2013.04.014 ↗
14. Protection of Nb- and Ta-based alloys against high temperature oxidation10.1016/0263-4368(93)90036-F ↗
15. Oxidation behavior of Nb-Si-B alloys with the NbSi2 coating layer formed by a pack cementation technique10.1016/j.ijrmhm.2013.02.010 ↗
16. Characterization of microstructures and oxidation behaviour of Nb-20Si-20Cr-5Al alloy10.1016/j.corsci.2011.02.038 ↗
17. A comparison of the effect of Cr and Al additions on the oxidation behaviour of alloys from the Nb-Cr-Si system10.1179/1878641315Y.0000000012 ↗
18. Oxidation response of three Nb-Cr-Mo-Si-B alloys in air10.1016/j.corsci.2015.06.026 ↗
19. Phase equilibria in the Nb-Ti side of the Nb-Si-Ti system at 1200°C and its oxidation behavior10.1016/j.jallcom.2017.02.007 ↗
20. Isothermal oxidation mechanism of a newly developed Nb-Ti-V-Cr-Al-W-Mo-Hf alloy at 800-1200 °C10.1016/j.ijrmhm.2015.08.012 ↗
21. Improvement in the oxidation resistance of Nb-Ti-Si-Cr-Al-Hf alloys containing alloyed Ge and B10.1016/j.corsci.2014.08.006 ↗
22. Oxidation of Nb-Si-Cr-Al in situ composites with Mo, Ti and Hf additions10.1016/j.msea.2006.08.093 ↗
23. Cyclic oxidation response of multiphase niobium-based alloys10.1007/s11661-004-0370-7 ↗
24. Effects of Cr and Al on high temperature oxidation resistance of Nb-Si system intermetallics10.4028/www.scientific.net/MSF.546-549.1485 ↗
25. Effect of Al additions on the oxidation behavior of Laves phase NbCr2 alloys at 1373 K and 1473 K10.1016/j.ijrmhm.2008.09.007 ↗
26. Oxidation resistance of powder compacts of the Nb-Si-Cr system and Nb3Si5Al2 matrix compacts prepared by spark plasma sintering10.1016/S0966-9795(01)00043-7 ↗
27. Oxidation behavior and kinetics of Al2O3-TiC-Co composites10.1016/j.ijrmhm.2012.08.005 ↗
28. Alloying effects on the microstructure and properties of Nb-Si based ultrahigh temperature alloys10.1016/j.intermet.2015.12.002 ↗
29. Li · 2003
30. Isothermal oxidation mechanism of Nb-Ti-V-Al-Zr alloy at 700-1200 °C: diffusion and interface reaction10.1016/j.corsci.2015.04.002 ↗
31. Hot corrosion behaviour of Nbss/Nb5Si3 in situ composites in the mixture of Na2SO4 and NaCl melts10.1016/j.corsci.2013.04.057 ↗