Effect of Mo2C on the microstructure and properties of (W, Mo)C-10Co cemented carbides
Source abstract
Abstract
Mo 2C doped WC-10Co alloys were prepared via an in- situ synthesis method composed of steps of spray drying, roasting, carbothermal pre-reduction and carbonization-vacuum sintering. The effects of Mo 2 C content on the microstructure and mechanical properties of cemented carbides were studied in detail. The results showed that WC and Mo 2 C formed a complete solid solution by the current method. With the increase of Mo 2C content from 0 wt% to 0.5 wt%, the effects of solution strengthening and fine grain strengthening were obvious, and the grain size was decreased from 0.72 ± 0.32 μm to 0.62 ± 0.27 μm, while the hardness was improved from 1316 ± 20 HV 30 to 1549 ± 14 HV 30 . However, the (W, Mo)C solid solution would deteriorate the fracture toughness of the alloys. With the further increase of Mo 2 C content to 9 wt%, the lattice distortion in the solid solution became more serious. Meanwhile, the dissolution of more Mo 2C in the liquid Co further weakened the dissolution-precipitation process of the solid solution, thus inhibiting the growth of grains and increasing the hardness of the alloys. In addition, with the increase of Mo 2 C content, the dominant fracture mode of the alloy changed from transgranular fracture to intergranular fracture.
Source: expertdata · Quality: candidate unverified · Source record ↗
Research context
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (41)
Show source-provided references
1. Grain size effect on wear resistance of WC-Co cemented carbides under different tribological conditions10.1016/j.jmst.2019.07.016 ↗
2. Effect of carbon addition on microstructure and properties of WC-Co cemented carbides10.1016/S1005-0302(12)60140-6 ↗
3. The influence of powder preparation condition on densification and microstructural properties of WC-Co-Al2O3 cermets10.1016/j.ijrmhm.2020.105275 ↗
4. Effect of Co on morphology and preparation of in situ synthesis of WC-Co composite powders10.1088/2053-1591/ab1c38 ↗
5. Investigation on reduction and carbonization process of WC-Co composite powder obtained by in situ synthesis10.1016/j.jallcom.2018.10.211 ↗
6. Effects of NbC additions on the microstructure and properties of non-uniform structure WC-Co cemented carbides10.1016/j.msea.2017.01.077 ↗
7. Preparation and performance of ultrafine grained WC-10Co alloys with added La2O310.1016/j.ceramint.2018.11.071 ↗
8. General aspects and limits of conventional ultrafine WC powder manufacture and hard metal production10.1016/0263-4368(95)92674-9 ↗
9. Grain growth during the early stage of sintering of nanosized WC-Co powder10.1016/j.ijrmhm.2007.04.006 ↗
10. Effects of initial particle size distribution and sintering parameters on microstructure and mechanical properties of functionally graded WC-TiC-VC-Cr3C2 -Co hard alloys10.1016/j.ceramint.2016.11.086 ↗
11. Microstructural study on the grain growth inhibition of VC-doped WC-Co cemented carbides10.1016/j.ijrmhm.2016.06.009 ↗
12. Effects of Cr3C2 additions on the densification, grain growth and properties of ultrafine WC-11Co composites by spark plasma sintering10.1016/j.ijrmhm.2007.08.009 ↗
13. Study on the properties of WC-10Co alloys adding Cr3C2 powder via various vacuum sintering temperatures10.1016/j.jallcom.2016.06.221 ↗
14. Sintering of binderless WC-Mo2C hard materials by rapid sintering process10.1016/j.ceramint.2007.03.029 ↗
15. Effect of Mo2C addition on the microstructure and fracture behavior of (W, Ti)C-based cemented carbides10.1016/j.ceramint.2014.07.150 ↗
16. Microhomogeneous WC-TiC-Co composite powders with enhanced sinterability via a two-step carburization method10.1016/j.ijrmhm.2020.105413 ↗
17. WC-5TiC-10Co hard metal alloy fabrication via mechanochemical and SPS techniques10.1016/j.ijrmhm.2020.105385 ↗
18. NbC as grain growth inhibitor and carbide in WC-Co hardmetals10.1016/j.ijrmhm.2007.09.003 ↗
19. The effect of NbC on mechanical properties and fracture behavior of WC-10Co cemented carbides10.1016/j.ijrmhm.2014.11.006 ↗
20. VC, Cr3C2 doped ultrafine WC-Co cemented carbides prepared by spark plasma sintering10.1016/j.ijrmhm.2010.09.004 ↗
21. Enhancement of the mechanical properties of ultrafine-grained WC-Co cemented carbides via the in-situ generation of VC10.1016/j.jallcom.2022.163961 ↗
22. The optimization of mechanical property and corrosion resistance of WC-6Co cemented carbide by Mo2C content10.1016/j.ceramint.2020.04.011 ↗
23. Effect of Mo and Co additions on the microstructure and properties of WC-TiC-Ni cemented carbides10.1016/j.ijrmhm.2011.07.011 ↗
24. Microstructure and mechanical properties of 90WC-8Ni-2Mo2C cemented carbide developed by conventional powder metallurgy10.1016/j.ijrmhm.2017.06.009 ↗
25. Effect of CeO2 and VC co-doping on the microstructure and properties of WC-10Co cemented carbide10.1016/j.ijrmhm.2022.105938 ↗
26. Effects of oxide addition on structure and properties of WC-10Co cemented carbide obtained by in situ synthesized powder10.1111/ijac.14058 ↗
27. The effects of metallic additives on the microstructure and mechanical properties of WC-Co cermets prepared by microwave sintering10.1016/j.ceramint.2020.08.093 ↗
28. Effects of micro/nano CeO2 on the microstructure and properties of WC-10Co cemented carbides10.1016/j.ijrmhm.2020.105432 ↗
29. Preparation of fine-grained Mo-W solid solution alloys with excellent performances10.1016/j.matchar.2022.112140 ↗
30. Inhibition of grain coarsening up to 1000 °C in (AlCrNbSiTiV)N superhard coatings10.1016/j.scriptamat.2009.09.015 ↗
31. Effect of Mo2C on the microstructure and properties of WC-TiC-Ni cemented carbide10.1016/j.ijrmhm.2008.01.007 ↗
32. Effect of coalescence on the grain coarsening during liquid-phase sintering10.1016/S1359-6454(00)00117-8 ↗
33. Microstructure and properties of ultrafine WC-Co-VC cemented carbides with different Co contents10.1007/s12598-014-0424-y ↗
34. Analytical modeling to calculate the hardness of ultra-fine WC-Co cemented carbides10.1016/j.msea.2007.12.036 ↗
35. Hardness and deformation of cemented tungsten carbide10.1016/0025-5416(78)90163-5 ↗
36. Effect of CeO2 on impact toughness and corrosion resistance of WC reinforced Al-based coating by laser cladding10.3390/ma12182901 ↗
37. Three dimensional topographic studies on worn surfaces of coated cemented carbide tools with different workpiece materials10.1016/j.cirpj.2016.05.003 ↗
38. On the fatigue crack growth behavior of WC-Co cemented carbides: kinetics description, microstructural effects and fatigue sensitivity10.1016/S1359-6454(02)00071-X ↗
39. Microstructural characterization and corrosion resistance of WC-Ni-Cr-Mo composite -The effect of Mo10.1016/j.ijrmhm.2019.105090 ↗
40. Effect of Mo2C additions on the properties of SPS manufactured WC-TiC-Ni cemented carbides10.1016/j.ijrmhm.2013.01.008 ↗
41. Effects of nano-alumina on mechanical properties and wear resistance of WC-8Co cemented carbide by spark plasma sintering10.1016/j.ijrmhm.2020.105337 ↗