Preparation of dense TiN1−X (X=0–0.4) by pulsed electric current sintering: Densification and mechanical behavior
Source abstract
Abstract
Abstract Bulks of TiN 1 − X in the range of X = 0–0.4 with high density were prepared by a new method which comprises the reaction between TiN with TiH 2 through pulsed electric current sintering. X-ray diffractograms revealed that single fcc phase with nitrogen vacancies was achieved after sintering; further observation by scanning electron microscopy showed homogeneous structure in all samples and larger grain size by increasing the amount of TiH 2 . The maximum Vickers hardness measured on the samples was approximately 31 GPa at X = 0.3. An increase in hardness was observed in non-stoichiometric samples even its larger grain size. The grain size-indent diagonal ratio was calculated from 1.2 at X = 0 to 5.6 at X = 0.4. The addition of TiH 2 showed an improvement in both densification and hardness without significant degradation of fracture toughness. Based on these results, the mechanical properties of TiN 1 − X bulks can be controlled as a function of TiH 2 /TiN ratios in order to be used for different applications.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (17)
Show source-provided references
1. The N–Ti (nitrogen–titanium) system10.1007/BF02869274 ↗
2. Lattice parameter of the non-stoichiometric compound TiNx10.1107/S0021889875009545 ↗
3. Hot isostatic pressing and thermoelectrical properties of non-stoichiometric titanium nitride10.2109/jcersj.97.63 ↗
4. Properties of bulks δ-TiN1−x prepared by nitrogen diffusion into titanium metal10.1016/0925-8388(92)90016-3 ↗
5. Preparation and some properties of titanium nitride in the homogeneity region
6. Densification and characteristics of TiN ceramics10.1007/BF00258170 ↗
7. Mechanical properties of bulk sintered titanium nitride ceramics10.1016/S0921-5093(01)00936-4 ↗
8. Field-assisted sintering of nanocrystallin titanium nitride10.1111/j.1151-2916.2000.tb01369.x ↗
9. Spark plasma sintering of nano-sized TiN prepared from TiO2 by controlled hydrolysis of TiCl4 and Ti(O-i-C3H7)4 solution10.1111/j.1151-2916.2003.tb03524.x ↗
10. Consolidation of nano-sized TiN powders by spark plasma sintering10.1111/j.1551-2916.2006.01066.x ↗
11. Evaluation of elastic/plastic indentation stress to determine fracture toughness10.2320/jinstmet1952.48.12_1157 ↗
12. Dehydrogenation of TiH210.1016/S0921-5093(03)00117-5 ↗
13. An investigation of the Ti–C–N system
14. Hardness-grain size relations in ceramics10.1111/j.1151-2916.1994.tb04641.x ↗
15. Mechanical properties of ceramics and composites
16. Spark plasma sintering and mechanical behaviour of ZrC-based composites10.1016/j.scriptamat.2008.05.026 ↗
17. Hot pressed titanium nitride obtained from SHS starting powders: influence of a pre-sintering heat-treatment of the starting powders on the densification process10.1016/j.jeurceramsoc.2006.02.032 ↗