Vacuum sintering of novel cemented carbide hard alloy (W0.4Al0.6)C0.5–Co

Jianwei Liu, Xianfeng Ma, Huaguo Tang, Wei Zhao

Publisher page

Abstract

Cemented carbide hard metals (W0.4Al0.6)C-0.5-13.3vol.%Co were successfully prepared by mechanical alloying and vacuum sintering. The impacts of the sintering temperature and time on the microstructure and mechanical properties of the samples have been studied. Both sintering time and temperature have great influence on the mechanical properties, density and microstructure of the specimens. The optimal vacuum sintering condition for this work is 1350 degrees C for 90 min. Another phenomenon is that the -type phases were not discernable in the bulk specimens, although it was prepared by vacuum sintering and the carbon vacancy reached to the astonished 50% value. (C) 2011 Elsevier Ltd. All rights reserved.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (14)

Show source-provided references
1. Synthesis, crystal structure, and density of (W1−xAlx)C10.1016/j.jssc.2004.03.009 ↗
2. Synthesis, reactive mechanism and thermal stability of W1−xAlxC (x=0.33, 0.5, 0.75, 0.86) nanocrystalline10.1016/j.materresbull.2003.11.006 ↗
3. High-pressure sintering study of a novel hard material (W0.5Al0.5)C-0.5 without binder metal10.1016/j.ijrmhm.2005.12.001 ↗
4. Nanostructured novel cemented hard alloy obtained by mechanical alloying and hot-pressing sintering and its applications10.1016/j.jallcom.2007.08.062 ↗
5. The deformation of low-carbon steel in the blue-brittle range
6. The cleavage strength of polycrystals
7. Rearrangement and pore size evolution during WC–Co sintering below the eutectic temperature10.1016/j.actamat.2004.12.017 ↗
8. Grain growth during the early stage of sintering of nanosized WC–Co powder10.1016/j.ijrmhm.2007.04.006 ↗
9. Synthesis, sintering, and mechanical properties of nanocrystalline cemented tungsten carbide — a review10.1016/j.ijrmhm.2008.07.011 ↗
10. Effect of WC particle size on the microstructure, mechanical properties and fracture behavior of WC-(W, Ti, Ta) C-6wt.% Co cemented carbides10.1016/j.ijrmhm.2006.11.005 ↗
11. Crystal structure and carbon vacancy hardening of (W0.5Al0.5)C1−x prepared by a solid-state reaction10.1002/cphc.200500143 ↗
12. A study of the effect of carbon content on the structure and properties of sintered Wc–Co alloys
13. Role of the binder phase in cemented tungsten carbide–cobalt alloys
14. The Co–Fe–Ni–W–C phase-diagram — a thermodynamic description and calculated sections for (Co–Fe–Ni) bonded cemented Wc tools