The enhancement of the microstructure and mechanical performances of ultrafine WC-Co cemented carbides by optimizing Cr2(C,N) addition and WC particle sizes
Source abstract
Abstract
Abstract Ultrafine WC-10Co cemented carbides with different Cr2(C,N) inhibitor contents and different-scaled WC powders were prepared by low-pressure sintering. Their influence on the microstructure and mechanical performances were investigated and expounded in this work. The result shows that the Cr2(C,N) addition homogenized the microstructure of the cemented carbides and refined WC grains. With the Cr2(C,N) addition increasing, hardness increased to 1870 kg/mm2, transverse rupture strength (TRS) first increased to 4435 MPa and then sharply decreased to 3230 MPa due to the existence of more pores with excessive Cr2(C,N). With the reduction of WC particle size, the mean WC grain size and mean free path of Co phase decreased, while the contiguity of the WC grains increased. The hardness and TRS of the specimens reduced, while fracture toughness increased. The comprehensive mechanical properties namely the TRS, hardness, and fracture toughness in the cemented carbides with 0.5 wt% Cr2(C,N) and 0.4 μm WC powder, were 4748 MPa, 1786 kg/mm2, 10.1 MPa· m1/2, respectively. A good combination of high TRS and hardness could be obtained in the cemented carbides by adopting appropriate amount of Cr2(C,N) and reducing the WC particle size.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (44)
Show source-provided references
1. Effects of Mo and Vc on the microstructure and properties of nano-cemented carbides10.2298/SOS1601041C ↗
2. Nanocrystalline WC-co composite with ultrahigh hardness and toughness10.1016/j.compositesb.2020.108161 ↗
3. Interface character distributions in WC–co composites10.1111/j.1551-2916.2007.02226.x ↗
4. Effect of WC/co coherency phase boundaries on fracture toughness of the nanocrystalline cemented carbides10.1038/srep31047 ↗
5. A new insight into the ∑=2 grain boundary characteristics in WC powder and in WC-Co sintered materials10.1016/j.actamat.2018.06.022 ↗
6. Sintering of nanophase WC–15vol.%Co hard metals by rapid sintering process10.1016/j.ijrmhm.2004.06.006 ↗
7. Annealing effect on the mechanical properties of ultrafine WC–Co materials10.1016/j.jart.2017.03.005 ↗
8. Reinforcement of tungsten carbide grains by nanoprecipitates in cemented carbides10.1088/0957-4484/27/41/415710 ↗
9. Effect of (Cr0.8V0.2)2(C,N) addition on microstructure and mechanical properties of WC–8Co cemented carbides10.1016/j.ijrmhm.2014.07.012 ↗
10. Effects of NbC additions on the microstructure and properties of non-uniform structure WC-Co cemented carbides10.1016/j.msea.2017.01.077 ↗
11. Preparation and properties of the VC/Cr3C2/TaC doped ultrafine WC-Co tool material by spark plasma sintering10.1016/j.jallcom.2019.152598 ↗
12. Complexions in WC-Co cemented carbides10.1016/j.actamat.2018.02.018 ↗
13. Grain and phase boundary segregation in WC–Co with small V, Cr or Mn additions10.1016/j.actamat.2010.03.038 ↗
14. Microstructure and composition of segregation layers at WC/Co interfaces in ultrafine-grained cemented carbides co-doped with Cr and V10.1016/j.ijrmhm.2016.04.003 ↗
15. Segregation of dopants at WC/Co and WC/WC interfaces in solid-state-sintered WC-VC- Cr3C2-co cemented carbides10.2320/matertrans.M2015198 ↗
16. Effects of Cr3C2 additions on the densification, grain growth and properties of ultrafine WC–11Co composites by spark plasma sintering10.1016/j.ijrmhm.2007.08.009 ↗
17. Influence and effectivity of VC and Cr3C2 grain growth inhibitors on sintering of binderless tungsten carbide10.1016/j.ijrmhm.2011.11.006 ↗
18. Influence of nitridation on surface microstructure and properties of graded cemented carbides with co and Ni binders10.1016/j.surfcoat.2008.06.179 ↗
19. The influence of sintering in nitrogen gas on the microstructure of a WC–VC–TiC–co cemented carbide10.1016/j.ijrmhm.2007.09.004 ↗
20. Microstructure and mechanical properties improvements in cemented carbides by (Cr,Mo,Ta) 2 (C,N) inhibitors10.1007/s12598-019-01343-x ↗
21. Effects of WC particle size on densification and properties of spark plasma sintered WC–co cermet10.1016/j.ijrmhm.2009.07.017 ↗
22. Effect of powder particle size on gradient formation and grain growth in ultrafine crystalline gradient cemented carbide10.1016/j.ijrmhm.2015.11.013 ↗
23. Preparation and crystal structure of ζ-Cr 2 (C,N) powders10.1007/s10853-019-03873-2 ↗
24. Synthesis, characterization, and consolidation of Cr2(C,N) solid solution powders10.1111/jace.14215 ↗
25. Quantitative characterization of the microstructure and properties of nanocrystalline WC–co bulk10.1016/j.scriptamat.2012.02.029 ↗
26. Quantitative metallography in three dimensions10.1515/pm-2001-380705 ↗
27. Hardness to toughness relationship of fine-grained WC-Co hardmetals10.1016/S0263-4368(98)00028-6 ↗
28. Microstructure and mechanical properties of dual-grain structured WC-Co cemented carbides10.1016/j.ceramint.2019.07.146 ↗
29. Effects of fine WC particle size on the microstructure and mechanical properties of WC-8Co cemented carbides with dual-scale and dual-morphology WC grains10.1016/j.ijrmhm.2019.105166 ↗
30. Correlation of transverse rupture strength of WC–Co with hardness10.1016/j.ijrmhm.2004.11.005 ↗
31. Characterizations of WC–10Co nanocomposite powders and subsequently sinterhip sintered cemented carbide10.1016/j.matchar.2006.02.013 ↗
32. Preparation and mechanisms of cemented carbides with ultrahigh fracture strength10.1107/S1600576715012832 ↗
33. One-step synthesis of ultrafine WC–10Co hardmetals with VC/V2O5 addition by plasma assisted milling10.1016/j.ijrmhm.2014.07.035 ↗
34. Sintering behavior and mechanical properties of Cr3C2 doped ultra-fine WC-Co cemented carbides: Experment guided with thermodynamic calculations10.1016/j.ijrmhm.2018.09.014 ↗
35. Optimization of the mechanical properties of ultra-fine WC-Co-Cr3C2 cemented carbides via an approach based on thermodynamic calculations and characterization of the experimental results by the Weibull distribution10.1016/j.calphad.2020.101778 ↗
36. Research on ultrafine tungsten carbide-cobalt (WC-Co) cemented carbide rods of miniature drills for highly integrated printed circuit board (PCB)
37. The temperature ranges for maximum effectiveness of grain growth inhibitors in WC–Co alloys10.1016/j.ijrmhm.2005.05.011 ↗
38. Carbide grain growth in cemented carbides10.1016/j.actamat.2010.11.056 ↗
39. Fabrication and mechanical properties of ultrafine grained WC–10Co–0.45Cr3C2–0.25VC alloys10.1016/j.ijrmhm.2010.11.004 ↗
40. Grain boundary character distributions of coincidence site lattice boundaries in WC-Co composites with different WC grain sizes10.1016/j.jallcom.2013.07.090 ↗
41. Deformation and fracture of WC grains and grain boundaries in a WC-Co hardmetal during microcantilever bending tests10.1016/j.ijrmhm.2019.105163 ↗
42. Fabrication of WC-Co cemented carbides with gradient distribution of WC grain size and Co composition by lamination pressing and microwave sintering10.1016/j.ceramint.2018.03.162 ↗
43. A new hardness model for materials design in cemented carbides10.1016/j.ijrmhm.2018.04.004 ↗
44. Edge toughness of tungsten carbide based hardmetals10.1016/j.ijrmhm.2017.12.020 ↗