Tungsten/copper (W/Cu) laminated composites possess high application potential in electronic, aerospace, and nuclear industries by combining the advantages of W and Cu. Among various fabrication methods , the explosive welding method is regarded as one rapid and cost-effective approach to producing W/Cu laminated composites considering the huge differences in physical properties between W and Cu. However, the lack of investigation on the bonding interface evolution between thick W plate and Cu plate inhibits the potential application of explosive welding on the large-scale production of the W/Cu laminated composites. In this study, the crack-free thick W/Cu laminated composites have been obtained successfully through the hot explosive welding approach, and the evolution mechanism of wavy interface formation is studied through numerical simulation and experimental investigation. The microstructure of welded W/Cu interface zone is further characterized to analyze the evolution mechanism of the wavy interface and corresponding bonding features. Moreover, the results of the mechanical property tests, such as compression shear, direct tensile, and micro-hardness tests, demonstrate that the welded W/Cu laminated composite features outstanding mechanical properties. Our study reveals the formation mechanism of the W/Cu interface during the hot explosive welding process and provides a rapid and efficient strategy to produce large-size W/Cu laminated composite with a thick W layer.
Source: expertdata · Quality: candidate unverified · Source record ↗
Research context
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (50)
Show source-provided references
1. Status of international collaborative efforts on selected ITER materials10.1016/S0022-3115(00)00233-6 ↗
2. Effect of interface modification by Cu-coated W powders on the microstructure evolution and properties improvement for Cu–W composites10.1016/j.surfcoat.2016.01.014 ↗
3. Effect of cyclic heat loading on pure tungsten for the ITER divertor10.1016/j.jnucmat.2020.152509 ↗
4. A novel approach for fabrication of functionally graded W/Cu composites via microwave processing10.1016/j.jallcom.2018.01.372 ↗
5. Overview on fabrication and joining of plasma facing and high heat flux materials for ITER10.1016/S0022-3115(02)01070-X ↗
6. Explosive cladding for ITER components
7. High heat flux testing for W/Cu monoblock PFUs with varying defects10.1016/j.fusengdes.2022.113137 ↗
8. Fabrication of W–Cu composite by resistance sintering under ultra-high pressure10.1016/j.jmatprotec.2004.11.008 ↗
9. W–Cu/Cu composite electrodes fabricated via laser surface alloying10.1016/j.matchar.2021.111715 ↗
10. W–Cu composites with submicron- and nanostructures: progress and challenges10.1038/s41427-019-0179-x ↗
11. Outgassing of implanted He via short circuit transport along phase and grain boundaries in vapor co-deposited Cu-W nanocomposites10.1016/j.actamat.2022.118306 ↗
12. Investigation on the interfacial microstructure and mechanical properties of the W-Cu joints fabricated by hot explosive welding10.1016/j.jmatprotec.2021.117400 ↗
13. Tensile and compressive stresses in Cu/W multilayers: correlation with microstructure, thermal stability, and thermal conductivity10.1016/j.actamat.2022.118315 ↗
14. High-strength diffusion bonding of oxide-dispersion-strengthened tungsten and CuCrZr alloy through surface nano-activation and Cu plating10.1016/j.jmst.2021.03.040 ↗
15. Vacuum diffusion bonding W to W-Cu composite: interfacial microstructure and mechanical properties10.1016/j.vacuum.2019.03.060 ↗
16. Direct diffusion bonding of immiscible tungsten and copper at temperature close to Copper's melting point10.1016/j.matdes.2017.10.052 ↗
17. Fabrication and characterization of vacuum plasma sprayed W/Cu-composites for extreme thermal conditions10.1007/s10853-006-1039-y ↗
18. Microstructural and mechanical characterizations of W/CuCrZr and W/steel joints brazed with Cu-22TiH2 filler10.1016/j.jmatprotec.2017.11.056 ↗
19. Thermal stability of Cu/W nano-multilayers10.1016/j.actamat.2016.02.003 ↗
20. Effect of composite interlayer on bonding quality of W and steel HIP joint10.1016/j.fusengdes.2019.111337 ↗
21. Interface diffusion and mechanical properties of ODS-W/Cu prepared by spark plasma sintering10.1016/j.vacuum.2021.110278 ↗
22. Friction stir forming to fabricate copper–tungsten composite10.1016/j.jmatprotec.2014.11.024 ↗
23. Explosive compact-coating of tungsten–copper alloy to a copper surface10.1088/2053-1591/aa664c ↗
24. Multi-material additive-manufacturing of tungsten - copper alloy bimetallic structure with a stainless-steel interlayer and associated bonding mechanisms
25. Energy balance during explosive welding10.1016/j.jmatprotec.2015.03.024 ↗
26. Lower boundary in metal explosive welding. Evolution of ideas10.1016/j.jmatprotec.2011.08.017 ↗
27. Microstructure development during explosive welding of metal foil:morphologies, mechanical behaviors and mechanisms10.1016/j.compositesb.2021.108685 ↗
28. Investigation on explosive welding of Zr53Cu35Al12 bulk metallic glass with crystalline copper10.1007/s11665-018-3396-5 ↗
29. Some trials on underwater explosive welding of thin W plate onto copper substrate10.4028/www.scientific.net/MSF.638-642.1041 ↗
30. Numerical and experimental studies on the explosive welding of tungsten foil to copper10.3390/ma10090984 ↗
31. Cladding of a crack-free W plate on Cu plates using explosive welding at higher collision velocity with lower collision angle
32. Performance of fine-grained W/Cu plate prepared by explosive welding with high wave impedance confinement at room temperature10.1016/j.fusengdes.2021.112855 ↗
33. Underwater explosive welding of thin tungsten foils and copper10.1016/j.jnucmat.2011.07.013 ↗
34. Bonding Interface of W–CuCrZr Explosively Welded Composite Plates for Plasma Facing Components10.1016/j.jmst.2014.11.014 ↗
35. Fabrication and characterization of the Mo/cu bimetal with thick Mo layer and high interfacial strength10.1016/j.ijrmhm.2020.105383 ↗
36. Experiment and simulation investigations on W/Cu components prepared by strong confinement thermal explosive welding
37. Study on weldability window and interface morphology of steel tube and tungsten alloy rod welded by explosive welding10.1016/j.ijrmhm.2019.105005 ↗
38. Hokamoto, underwater shock wave weldability window for Sn-Cu plates10.1016/j.jmatprotec.2018.11.044 ↗
39. Hielscher · 2022
40. Understanding interface evolution during explosive welding of silver foil and Q235 substrate through experimental observation coupled with simulation10.1016/j.apsusc.2021.150703 ↗
41. Numerical and experimental studies of the mechanism of the wavy interface formations in explosive/impact welding10.1016/j.jmps.2005.06.001 ↗
42. Interfacial reactions and microstructure related properties of explosively welded tantalum and steel sheets with copper interlayer10.1016/j.matdes.2021.109873 ↗
43. High cooling rates and metastable phases at the interfaces of explosively welded materials10.1016/j.actamat.2017.06.038 ↗
44. Numerical study on the interfacial behavior of Mg/Al plate in explosive/impact welding10.1515/secm-2015-0316 ↗
45. Atomistic simulation on the formation mechanism of bonding interface in explosive welding10.1063/5.0069720 ↗
46. Enhancing explosive weldability of thick precipitate-hardened alloys10.1016/j.jmapro.2022.03.041 ↗
47. Uncover the mystery of interfacial interactions in immiscible composites by spectroscopic microscopy: a case study with W-Cu10.1016/j.jmst.2022.03.014 ↗
48. The mechanics of wave formation in explosive welding
49. Effect of impact loading and heat treatment on microstructure and properties of multi-layered AZ31/AA1050 plates fabricated by single-shot explosive welding10.1016/j.matdes.2022.110411 ↗
50. Microstructure evolution and mechanical properties of an AA6061/AZ31B alloy plate fabricated by explosive welding10.1016/j.jallcom.2017.11.285 ↗