journal article·2025-08

Alloy design for powder bed fusion - laser beam: Grain boundary and segregation engineering in a novel molybdenum-boron-lanthanum alloy

L. Kaserer, D. Brennsteiner, J. Braun, V. Goettgens, I. Letofsky-Papst, B. Mayr-Schmoelzer, B. Distl, G. Leichtfried

Publisher page

Abstract

No abstract is available for this record. The assistant can identify its topic from the title, but cannot infer the study’s results.

Source: Not provided · Quality: missing

Research context

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (35)

Show source-provided references
1. Molybdenum and molybdenum alloys10.1002/0471238961.1315122504150114.a01.pub3 ↗
2. Molybdenum and tungsten manufactured by selective laser melting: analysis of defect structure and solidification mechanisms
3. Fully dense and crack free molybdenum manufactured by selective laser melting through alloying with carbon
4. Selective laser melting of pure molybdenum: evolution of defect and crystallographic texture with process parameters10.1016/j.matdes.2020.108588 ↗
5. Densification and crack suppression in selective laser melting of pure molybdenum10.1016/j.matdes.2017.04.094 ↗
6. Towards understanding grain nucleation under additive manufacturing solidification conditions10.1016/j.actamat.2020.05.012 ↗
7. Revealing the mechanisms of grain nucleation and formation during additive manufacturing10.1007/s11837-020-04019-5 ↗
8. On grain boundary segregation in molybdenum materials10.1016/j.matdes.2017.09.019 ↗
9. Grain boundary segregation in recrystallized molybdenum alloys and its effect on brittle intergranular fracture10.1016/0263-4368(92)90060-F ↗
10. Atom probe study of grain boundary segregation in technically pure molybdenum10.1016/j.matchar.2013.11.001 ↗
11. Grain boundary segregation and intergranular fracture in molybdenum
12. Chemical states of oxygen segregated intergranular fracture surfaces of molybdenum10.1016/0169-4332(86)90051-6 ↗
13. Grain boundary segregation engineering in metallic alloys: a pathway to the design of interfaces10.1016/j.cossms.2014.06.002 ↗
14. Effect of hot rolling and annealing on the mechanical properties and thermal conductivity of W-0.5wt.% TaC alloys10.1016/j.ijrmhm.2015.12.004 ↗
15. Methods for improving ductility of tungsten - a review10.1016/j.ijrmhm.2018.04.012 ↗
16. Excellent high-temperature strength and ductility of the ZrC nanoparticles dispersed molybdenum10.1016/j.actamat.2022.117725 ↗
17. Solute-induced grain refinement and defect suppression in boron-modified molybdenum manufactured via laser powder-bed fusion10.1016/j.ijrmhm.2023.106384 ↗
18. Microstructure and mechanical properties of molybdenum-titanium-zirconium-carbon alloy TZM processed via laser powder-bed fusion10.1016/j.ijrmhm.2020.105369 ↗
19. Molybdenum alloy Mo-Ti-Zr-C adapted for laser powder bed fusion with refined isotropic microstructure and excellent high temperature strength10.1016/j.ijrmhm.2023.106174 ↗
20. On the influence of AlSi10Mg powder recycling behavior in the LPBF process and consequences for mechanical properties10.1007/s11837-021-05080-4 ↗
21. Metal vaporization and its influence during laser powder bed fusion process10.1016/j.matdes.2022.110505 ↗
22. Vaporization of alloying elements and explosion behavior during laser powder bed fusion of Cu–10Zn alloy10.1016/j.ijmachtools.2020.103686 ↗
23. Element vaporization of Ti-6Al-4V alloy during selective laser melting10.3390/met10040435 ↗
24. Selective laser melting of Al-Zn-Mg-Cu: heat treatment, microstructure and mechanical properties10.1016/j.jallcom.2016.11.210 ↗
25. Influence of keyhole and conduction mode melting for top-hat shaped beam profiles in laser powder bed fusion10.1016/j.jmatprotec.2019.116514 ↗
26. Corrected values for boiling points and enthalpies of vaporization of elements in handbooks10.1021/je1011086 ↗
27. Clift · 2013
28. Formation and reduction of hydrogen porosity during selective laser melting of AlSi10Mg10.1016/j.jmatprotec.2015.02.013 ↗
29. In situ X-ray imaging of defect and molten pool dynamics in laser additive manufacturing10.1038/s41467-018-03734-7 ↗
30. Pore elimination mechanisms during 3D printing of metals10.1038/s41467-019-10973-9 ↗
31. Supplemental literature review of binary phase diagrams: Ag-Te, B-Mo, C-Nd, Cd-Te, Ce-S, Co-Er, Fe-La, Fe-V, Ho-Mo, Ho-V, Ni-Th, and Ni-U10.1007/s11669-018-0669-5 ↗
32. Alloy Phase Diagrams · Bull. Alloy Phase Diagr. · 1988 · 9 · 51010.1007/BF02881876 ↗
33. Chapter 3.3 - Ellingham diagram
34. High-temperature Na 2SO4 deposit-assisted corrosion of silicon carbide– II effects of B, C, and Si10.1111/jace.14596 ↗
35. Influence of nano-sized SiC on the laser powder bed fusion of molybdenum10.3390/cryst12091276 ↗