Characterization of quasi-plastic deformation of WC–Co composite using Hertzian indentation technique
Source abstract
Abstract
Abstract Using the Hertzian indentation technique, the evolution of the WC–Co composite from plastic deformation to final fracture was studied. Loaded with a spherical indenter, the material underwent initial elastic, elastic–plastic, and fully plastic deformations, finally ended with macrocracks, namely cone cracks and radial cracks. The behaviors of both WC grains and cobalt binder phase during each step of the deformation process was studied including the slip of WC grains, the formation of microcracks, the apparent strain hardening of the WC–Co composite, and the evolution from quasi-plastic deformation to the formation of macro-rings cracks and radial cracks. The correlation between microcracks and the quasi-plastic deformation, apparent strain hardening, and macrocracks are examined.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (37)
Show source-provided references
1. Mechanism of plastic deformation and dislocation damping of cemented carbides
2. Determination of the slip systems in single crystals of tungsten monocarbide10.1080/14786436508224941 ↗
3. Room temperature deformation mechanisms and the defect structure of tungsten carbide10.1016/0001-6160(81)90047-X ↗
4. Compression deformation and fracture in WC materials10.1016/0025-5416(88)90710-0 ↗
5. On the deformation of WC–Co cemented carbides10.1179/030634575790444531 ↗
6. The defect structure of tungsten carbide in deformed tungsten carbide-cobalt composites10.1016/0001-6160(82)90013-X ↗
7. Metallographic aspects of deformation and fracture of hard alloys under compression10.1007/s11106-006-0014-0 ↗
8. Elastic and plastic behavior of WC–Co composites10.1016/0272-8842(83)90017-2 ↗
9. Determination of ductility and stress strain curve of WC based hard metals by indentation method
10. Tumanov VI, et al. Deformation and elastic properties of WC–Co system sintered carbides of micro- and macroindentation. All-Union Scientific Research Institute of Hard Alloys and High Melting Metals, Moscow. Translated from Problemy Prochnosti 1985;3:99–103.
11. Chernayavskii KS, Travushkin GG, Sapronova ZN, Aleksandrovich AA. Micromechanisms of deformation and failure at successive stages of compressive loading of hard alloys WC–Co. All-Union Scientific Research Institute of Hard Alloys and High Melting Metals, Moscow, Translated from Problemy Prochnosti 1993;10:53–62.10.1007/BF00777122 ↗
12. On the fracture toughness of cemented carbides10.1016/0001-6160(88)90143-5 ↗
13. Prediction of crack paths in WC–Co alloys10.1016/0956-7151(92)90108-Q ↗
14. A microstructure model relating fracture toughness and hardness in WC–Co composites
15. The fracture toughness of WC–Co alloys measured on single-edge notched beam specimens precracked by electron discharge machining10.1016/0025-5416(78)90164-7 ↗
16. The fracture toughness of WC–Co two-phase alloys-a preliminary model10.1007/BF02700449 ↗
17. Microscopic aspects of fracture in WC–Co alloys10.1016/0001-6160(68)90128-4 ↗
18. Experimental study of the mechanics of fracture in WC–Co alloys10.1007/BF02647199 ↗
19. Defect interactions in deformed WC10.1016/0001-6160(84)90031-2 ↗
20. Deformation and fracture processes and the physical metallurgy of WC–Co hardmetals10.1179/imr.1988.33.1.90 ↗
21. Correlation of transverse rupture strength of WC–Co with hardness10.1016/j.ijrmhm.2004.11.005 ↗
22. Zhang H, Fang ZZ, Belnap J. Quasi-plastic deformation of WC–Co composites loaded with a spherical indenter. Metall Trans A, in press, doi:10.1007/s11661-006-9036-y.10.1007/s11661-006-9036-y ↗
23. Lawn · 1993
24. Nondestructive evaluation of WC–Co composites using magnetic properties
25. Data from RTW (Rogers Tool Works) Inc. and Mega Diamond, Smith Tool Inc.
26. Johnson · 1985
27. Indentation stress–strain curves for “quasi-ductile” ceramics10.1016/1359-6454(95)00204-9 ↗
28. Indentation on ceramics with spheres: a century after Hertz10.1111/j.1151-2916.1998.tb02580.x ↗
29. Deformation and fracture of mica-containing glass–ceramics in Hertzian contacts10.1557/JMR.1994.0762 ↗
30. Dehoff · 1968
31. Indentation fracture: principles and applications10.1007/BF00823224 ↗
32. Wear induced material modifications of cemented carbide rock drill buttons10.1016/j.ijrmhm.2005.05.003 ↗
33. Nonlinear stress–strain curves for solids containing closed cracks with friction10.1016/S0022-5096(97)00036-7 ↗
34. On the theory of Hertzian fracture10.1098/rspa.1967.0137 ↗
35. Role of microstructure in Hertzian contact damage in silicon nitride: I, mechanical characterization10.1111/j.1151-2916.1997.tb03129.x ↗
36. Contact fatigue of a silicon carbide with a heterogeneous grain structure10.1111/j.1151-2916.1995.tb08834.x ↗
37. Elastic/plastic indentation damage in ceramics: the median/radial crack system10.1111/j.1151-2916.1980.tb10768.x ↗