journal article·2012-07

Machinability investigations on hardened AISI 4340 steel using coated carbide insert

R. Suresh, S. Basavarajappa, V.N. Gaitonde, G.L. Samuel

Publisher page

Abstract

Abstract The hard turning process with advanced cutting tool materials has several advantages over grinding such as short cycle time, process flexibility, compatible surface roughness, higher material removal rate and less environment problems without the use of cutting fluid. However, the main concerns of hard turning are the cost of expensive tool materials and the effect of the process on machinability characteristics. The poor selection of the process parameters may cause excessive tool wear and increased work surface roughness. Hence, there is a need to study the machinability aspects in high-hardened components. In this work, an attempt has been made to analyze the influence of cutting speed, feed rate, depth of cut and machining time on machinability characteristics such as machining force, surface roughness and tool wear using response surface methodology (RSM) based second order mathematical models during turning of AISI 4340 high strength low alloy steel using coated carbide inserts. The experiments were planned as per full factorial design (FFD). From the parametric analysis, it is revealed that, the combination of low feed rate, low depth of cut and low machining time with high cutting speed is beneficial for minimizing the machining force and surface roughness. On the other hand, the interaction plots suggest that employing lower cutting speed with lower feed rate can reduce tool wear. Chip morphology study indicates the formation of various types of chips operating under several cutting conditions.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (56)

Show source-provided references
1. Identification of cutting errors in precision hard turning process10.1016/j.jmatprotec.2004.04.331 ↗
2. Surface integrity in finish hard turning of case hardened steels10.1016/S0890-6955(02)00141-4 ↗
3. Technology key to mold making success
4. High-speed milling of dies and molds in their hardened state10.1016/S0007-8506(07)60775-6 ↗
5. Hard turning — influence on the workpiece properties
6. Hard turning of hot work steel AISI H11: evaluation of cutting pressures, resulting force and temperature
7. Surface roughness model in turning hardened hot work steel using mixed ceramic tool
8. Statistical analysis of surface roughness and cutting forces using response surface methodology in hard turning of AISI 52100 bearing steel with CBN tool10.1016/j.ijrmhm.2009.11.011 ↗
9. Advancing cutting technology10.1016/S0007-8506(07)60200-5 ↗
10. Capability profile of hard cutting and grinding processes10.1016/S0007-8506(07)60018-3 ↗
11. Sahni JA comparative study of hard turned and cylindrically ground white layers10.1016/j.ijmachtools.2003.10.009 ↗
12. Cutting forces modeling considering the effect of tool thermal property — application to CBN hard turning10.1016/S0890-6955(02)00185-2 ↗
13. Effect of cutting edge geometry and workpiece hardness on surface residual stresses in finish hard turning of AISI 52100 steel10.1115/1.1286369 ↗
14. Surface roughness model for machining mild steel with coated carbide tool10.1016/j.matdes.2004.06.015 ↗
15. Hard turning AISI 4340 high strength low alloy steel and AISI D2 cold work steel10.1016/j.jmatprotec.2005.04.082 ↗
16. Wear characteristics in turning high hardness alloy steel by ceramic and CBN tools10.1016/S0924-0136(98)00376-8 ↗
17. Hard machining of hardened bearing steel using cubic boron nitride tool10.1016/j.jmatprotec.2008.03.014 ↗
18. Machinability evaluation in hard turning of cold work tool steel (D2) with ceramic tools using statistical techniques10.1016/j.matdes.2006.01.011 ↗
19. Predictive modeling of surface roughness and tool wear in hard turning using regression and neural networks10.1016/j.ijmachtools.2004.09.007 ↗
20. Comparing statistical models and artificial networks on predicting the tool wear in hard machining D2 AISI steel10.1007/s00170-007-0999-7 ↗
21. Analysis of tool wear and surface finish in hard turning10.1007/s00170-004-2411-1 ↗
22. Hard turning in continuous and interrupted cut with PCBN and whisker reinforced cutting tools10.1016/j.jmatprotec.2009.03.012 ↗
23. A CBN–TiN composite coating for carbide inserts: coating characterization and its application for finish hard turning10.1016/j.surfcoat.2006.04.026 ↗
24. Experimental investigation of cutting tool performance in high speed cutting of hardened X210Cr12 cold-work tool steel (62 HRC)10.1016/j.matdes.2004.04.004 ↗
25. Tool life performance of multilayer hard coatings produced by HTCVD for machining of nodular cast iron10.1016/j.ijrmhm.2007.12.003 ↗
26. Turning hardened steel using coated carbide at high cutting speeds10.1590/S1678-58782008000200002 ↗
27. Machining performance and decomposition of TiAlN/TiN multilayer coated metal cutting inserts10.1016/j.surfcoat.2011.02.031 ↗
28. Performance of multilayer coated carbide tools when turning cast iron
29. Machining of austenitic stainless steels using CVD multi-layer coated cemented carbide tools10.1016/j.triboint.2005.05.005 ↗
30. The Influence of the coating thickness on its strength properties and on the milling performance of PVD coated inserts10.1016/S0257-8972(03)00678-9 ↗
31. Influence of tool wear on surface roughness in hard turning using differently shaped ceramic tools10.1016/j.wear.2007.11.001 ↗
32. Machinability investigations in hard turning of AISI D2 cold work tool steel with conventional and wiper ceramic inserts10.1016/j.ijrmhm.2008.12.007 ↗
33. Analysis of machinability during hard turning of cold work tool steel (Type: AISI D2)10.1080/10426910902997415 ↗
34. Performance comparison of conventional and wiper ceramic inserts in hard turning through artificial neural network modeling10.1007/s00170-010-2714-3 ↗
35. On machining of hardened AISI D2 steel with PCBN tools10.1016/j.jmatprotec.2005.06.079 ↗
36. The effect of tool wear on tool life of alumina-based ceramic cutting tools while machining hardened martensitic steels10.1016/j.jmatprotec.2005.11.012 ↗
37. Tool wear and machining performance of CBN–TiN coated carbide inserts and PCBN compact inserts in turning AISI 4340 hardened steel10.1016/j.jmatprotec.2006.06.013 ↗
38. Tool wear mechanism in continuous cutting of hardened tool steels10.1016/S0043-1648(97)00139-7 ↗
39. Experimental investigation on CBN turning of hardened AISI 52100 steel10.1016/S0924-0136(02)00180-2 ↗
40. Effect of cutting edge geometry and workpiece hardness on surface generation in the finish hard turning of AISI 52100 steel10.1016/S0924-0136(99)00111-9 ↗
41. Effects of cutting edge geometry, workpiece hardness, feed rate and cutting speed on surface roughness and forces in finish turning of hardened AISI H13 steel
42. The influence of the microstructure of hardened tool steel workpiece on the wear of PCBN cutting tools10.1016/S0890-6955(02)00170-0 ↗
43. Surface integrity of die material in high-speed hard machining, Part 1, micro graphical analysis10.1115/1.1286367 ↗
44. Surface integrity of die material in high-speed hard machining, Part 2, micro hardness variations and residual stresses10.1115/1.1286557 ↗
45. Tool wear and surface integrity during high-speed turning hardened steel with polycrystalline cubic boron nitride tools10.1243/0954405011518700 ↗
46. Tool nose radius effects on finish turning10.1016/j.jmatprotec.2003.10.029 ↗
47. Turning of hardened 100Cr6 bearing steel with ceramic and PCBN cutting tools10.1016/S0924-0136(03)00346-7 ↗
48. Machinability of hardened steel using alumina based ceramic cutting tools10.1016/S0263-4368(03)00004-0 ↗
49. Comparative assessment of surface roughness produced by hard machining with mixed ceramic tools including 2D and 3D analysis10.1016/j.jmatprotec.2005.04.080 ↗
50. Hard turning of quenched alloy steel parts using conventional and wiper ceramic inserts10.1016/j.ijmachtools.2006.01.009 ↗
51. Advanced tool edge geometry for high precision hard turning10.1016/S0007-8506(07)60046-8 ↗
52. Feasibility of producing optimal surface integrity by process design in hard turning10.1016/j.msea.2004.12.012 ↗
53. Effect of tool wear on surface finish for a case of continuous and interrupted hard turning10.1016/j.jmatprotec.2005.04.119 ↗
54. Hard turning of interrupted surfaces using CBN tools10.1016/j.jmatprotec.2007.05.022 ↗
55. Evaluation of the performance of CBN when turning Ti-6Al-4V alloy with high pressure coolant supplies10.1016/j.ijmachtools.2004.11.027 ↗
56. Montgomery · 2004