Microstructural and mechanical properties at the submicrometric length scale under service-like working conditions on ground WC-Co grades
Source abstract
Abstract
The unique combination of hardness, toughness, and wear resistance exhibited by heterogeneous hard materials, particularly cemented carbides (WC-Co), has made them preeminent material choices for extremely demanding applications, such as metal cutting/forming tools. The grinding post-processing of WC-Co induces changes in their surface integrity by modifying both constitutive phases through cracking the WC ceramic phase, introducing compressive residual stresses and/or inducing phase transformations (from face-centered cubic to hexagonal compact phase) in the metallic Co binder. A systematic micro- and nanomechanical study of different ground WC-Co grades (with distinct metallic Co binder content and WC particle size) is presented. In general, three different aspects are investigated: (1) assessment of the intrinsic hardness of the deformed layer from room temperature up to 600 °C, (2) correlation of the compressive residual stresses with hardness and elastic modulus maps by using high-speed indentation tests, and (3) evaluation of the oxidation process as a function of the testing temperature for the different ground WC-Co grades. It was found that the mechanical properties of the deformed ground layer for the different WC-Co grades slightly decrease at temperatures ranging between 400 and 500 °C, being this temperature non depending on the amount of metallic binder or WC grain size. This is attributed to different effects which take place simultaneously when the testing temperature increases: dislocation motion, reduction of compressive residual stresses and particularly, the generation of a heterogeneous oxide layer formed of CoWO 4, WO 3 and Co 3O 4.
Source: expertdata · Quality: candidate unverified · Source record ↗
Research context
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (34)
Show source-provided references
1. Effect of ultrafine WC contents on the microstructures, mechanical properties and wear resistance of regenerated coarse grained WC-10Co cemented carbides
2. Grinding of WC-Co hardmetals10.1016/S0043-1648(00)00561-5 ↗
3. 3D FIB/FESEM tomography of grinding-induced damage in WC-Co cemented carbides10.1016/j.procir.2020.02.070 ↗
4. Grinding effects on surface integrity and mechanical strenght of WC-Co cemented carbides10.1016/j.procir.2014.04.044 ↗
5. Grinding-induced metallurgical alterations on the binder phase of WC-Co cemented carbides10.1016/j.matchar.2017.11.004 ↗
6. Mechanical behavior of hardmetals at high temperature
7. High-temperature fatigue of cemented carbides under cyclic loads10.1016/S0263-4368(99)00014-1 ↗
8. Mapping of mechanical properties at microstructural lenght scale in WC-Co cemented carbides: Assessment of hardness and elastic modulus by means ofhigh speed massive nanoindentation and statistical analysis10.1016/j.ijrmhm.2018.04.019 ↗
9. Nanomechanical behaviour of individual phases in WC-Co cemented carbides, from ambient to high temperature10.1016/j.mtla.2020.100713 ↗
10. Nanoindentation of WC-Co hardmetals10.1016/j.jeurceramsoc.2012.12.018 ↗
11. Nanoindentation study of WC-12Co hardmetals obtained from nanocrystalline powders: evaluation of hardness and modulus on individual phases10.1016/j.msea.2010.01.026 ↗
12. Intrinsic hardness of constitutive phase in WC-Co composites: nanoindentation testing, statistical analysis, WC crystal orientation effects and flow stress for the constrained metallic binder10.1016/j.jeurceramsoc.2015.04.021 ↗
13. Hall-Petch strenghtening of the constrained metallic binder in WC-Co cemented carbides: experimental assessment by means of massive nanoindentation and statistical analysis10.1016/j.msea.2016.09.020 ↗
14. High temperature hardness of tungsten carbide10.1007/BF02654390 ↗
15. Nanomechanical response of tungsten carbide single crystals in extreme conditions: Temperature and strain rate dependence10.1016/j.mtla.2023.101706 ↗
16. Micropillars compression of single crystal tungsten carbide, Part 1: temperature and orientation dependence of deformation behaviour10.1016/j.ijrmhm.2021.105729 ↗
17. High temperature nanoindentation: the state of the art and futur challenges10.1016/j.cossms.2015.02.002 ↗
18. Implementation of an effective time-saving two-stage methodology for microstructural characterization of cemented carbides10.1016/j.ijrmhm.2015.10.006 ↗
19. Deformation and fracture processes and the physical metallurgy of WC–Co hardmetals10.1179/imr.1988.33.1.90 ↗
20. Hardness and deformation of cemented tungsten carbide10.1016/0025-5416(78)90163-5 ↗
21. WSXM: a software for scanning probe microscopy and a tool for nanotechnology10.1063/1.2432410 ↗
22. X-Ray diffraction determination of residual stresses in functionally graded WC-Co composites10.1016/j.ijrmhm.2004.06.002 ↗
23. An improved technique for determining hardness and elastic modulus load and displacement sensing indentation experiments10.1557/JMR.1992.1564 ↗
24. On the determination of spherical nanoindentation stress-strain curves10.1557/jmr.2006.0324 ↗
25. Implementation of massive nanoindentation coupled with statistical analysis to evaluate complex heterogeneous microstructures in materials manufactured following powder metallurgy processing routes
26. Measurement of hardness and elastic modulus by instrumented indentation: Advances in understanding and refinements to methodology10.1557/jmr.2004.19.1.3 ↗
27. Residual stresses in hardmetals caused by grinding and EDM machining and their influence on the flexural strength
28. Inducement of residual stresses in WC-5%Co cutting inserts by plunge-face grinding10.1007/s00170-020-06583-1 ↗
29. Effect of the grinding process on the wear of cemented tungsten carbide cutting insert during turning10.1016/j.procir.2021.02.020 ↗
30. Oxidation behavior of WC-Co10.1016/0921-5093(95)10145-4 ↗
31. Oxidation of ultrafine-cemented carbide prepared from nanocrystalline WC-10Co composite powder10.1016/j.ceramint.2007.07.029 ↗
32. Remarkable improvement in high temperature oxidation resistance of WC-12Co by the addition of CrSi210.1016/j.ijrmhm.2021.105497 ↗
33. Oxidation-induced strenght degradation of WC-Co hardmetals10.1016/S0263-4368(01)00033-6 ↗
34. Kinetics of WC-Co oxidation accompanied by swelling10.1007/BF00351615 ↗