journal article·2014-03

Spark plasma sintering of (Ti0.9W0.1) C powders prepared by mechanical alloying

C. Slama, M.D. Boulaares, A. Teber, F. Schoenstein, M. Abdellaoui, N. Jouini

Publisher page

Abstract

Abstract Nanocrystalline (Ti0.9W0.1)C powder with a diffraction crystallite size of about 10 nm was synthesized by mechanical alloying. The formation of (Ti0.9W0.1)C carbide was detected by XRD measurements and microscopic observation. The sintering of these powders by a spark plasma sintering (SPS) at different temperatures were also studied. The results show that the maximum hardness was obtained for more relative density materials, meanwhile, the grain size is large. The micro-hardness and the relative density of the powder milled for 10 h and sintered at 1200 °C for 5 min under 100 MPa reach, respectively, 2978 HV and 98.35%.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (37)

Show source-provided references
1. McColm · 1986
2. Cermets
3. Sintering properties of submicron TiC powders from carbon coated titania precursor10.1023/A:1004876121000 ↗
4. Study on phase evolution during reaction synthesis of ultrafine (Ti, W, Mo, V) (CN)-Ni composite powders10.1016/j.matchemphys.2009.07.021 ↗
5. Microstructure evolution and mechanical properties of (Ti0.93W0.7) C-xWC-20Ni cermets10.1016/j.msea.2010.12.038 ↗
6. Sintered (Ti, W)C carbides10.1016/j.scriptamat.2006.12.026 ↗
7. Effect of nano-size powders on the microstructure of Ti (C, N)–xWC–Ni cermets10.1111/j.1551-2916.2007.01654.x ↗
8. Dissolution phenomena in the Ti (C0.7N 0.3)–WC–Ni system10.1016/j.ijrmhm.2007.08.007 ↗
9. Structure and properties of nanocrystalline TiC full-density bulk alloy consolidated from mechanical reacted powders10.1016/S0925-8388(00)00692-7 ↗
10. Effect of SPS process sintering on the microstructure and mechanical properties of nanocrystalline TiC for tools application10.1016/j.ijrmhm.2011.06.013 ↗
11. Thorne · J Mater Sci · 1992 · 27 · 440610.1007/BF00541573 ↗
12. Reaction synthesis of Fe–(W, Ti)C composites10.1016/S0924-0136(99)00049-7 ↗
13. Fast low temperature consolidation of bulk nanometric ceramic materials10.1016/j.scriptamat.2005.11.015 ↗
14. Consolidation/synthesis of materials by electric current activated/assisted sintering10.1016/j.mser.2008.09.003 ↗
15. A mathematical and experimental dynamical phase diagram for ball-milled Ni10Zr710.1016/0925-8388(94)91124-X ↗
16. The physics of mechanical alloying in a planetary ball mill: mathematical treatment10.1016/0956-7151(95)92625-7 ↗
17. Recent advances in magnetic structure determination by neutron powder diffraction10.1016/0921-4526(93)90108-I ↗
18. A profile refinement method for nuclear and magnetic structures10.1107/S0021889869006558 ↗
19. Microstructure characterization of nanocrystalline TiC synthesized by mechanical alloying10.1016/j.matchemphys.2009.11.048 ↗
20. Mechanochemical synthesis of nano TiC powder by mechanical milling of titanium and graphite powders10.1016/j.powtec.2011.10.050 ↗
21. Spark plasma sintering consolidation of nanostructured TiC prepared by mechanical alloying10.1016/j.ijrmhm.2010.10.003 ↗
22. Densification of nanocrystalline TiC ceramics by spark plasma sintering10.1016/j.matchemphys.2011.07.072 ↗
23. The effects of ball-milling treatment on the densification behavior of ultra-fine tungsten powder10.1016/j.ijrmhm.2011.06.010 ↗
24. The effect of Ti substitution by Zr on the microstructure and mechanical properties of the cermet Ti1−xZrxC sintered by SPS10.1016/j.ijrmhm.2011.10.002 ↗
25. Fabrication, microstructure and mechanical properties of novel bulk bindrless (Ti0.8Zr0.2)C carbides prepared by mechanical alloying and spark plasma sintering10.1016/j.ceramint.2012.02.085 ↗
26. The shape of WC crystals in cemented carbides10.1016/S0921-5093(97)00509-1 ↗
27. Spark plasma sintering of Mo–W powders prepared by mechanical alloying10.1016/j.jallcom.2013.01.142 ↗
28. Spark plasma sintering of TiC particle-reinforced molybdenum composites10.1016/j.ijrmhm.2011.12.001 ↗
29. Effect of ball milling on simultaneous spark plasma synthesis and densification of TiC–TiB2 composites10.1016/j.msea.2006.06.131 ↗
30. The carbon nonstoichiometry and the lattice parameter of (Ti1−xWx)C1−y10.1016/j.jeurceramsoc.2009.10.022 ↗
31. Properties of complex TiC–WC carbides in their homogeneity region. I. Preparation and phase and structural analyses of TiC–WC alloys10.1007/BF00801945 ↗
32. 1974
33. The XRD study of the nanostructured TiC/C and TiN/C composites
34. Characterization and EPR studies of TiC and TiN ceramics at room temperature
35. Effects of AGG on fracture toughness of tungsten carbide10.1016/j.msea.2006.09.076 ↗
36. Thermomechanical properties of TiC particle-reinforced tungsten composites for high temperature applications10.1016/S0263-4368(02)00105-1 ↗
37. Zhuzhou cemented carbide Industry Company · 1974 · 94