journal article·2018-09

Effects of ZrO2 and Y2O3 on physical and mechanical properties of ceramic bond and ceramic CBN composites

Xuezhi Wang, Zhelun Ma, Xue Sun, Tianbiao Yu, Wanshan Wang

Publisher page

Abstract

Abstract In order to optimize the structure performances of ceramic cubic boron nitride (CBN) grinding wheels, the effects of ZrO2 and Y2O3 addition on the physical and mechanical properties of ceramic bond and ceramic CBN composites were systematically investigated. The basic ceramic bond was composed of B2O3, Al2O3, SiO2, Li2O and Na2O. The additions of ZrO2 and Y2O3 had a certain effect on refractoriness, liquidity, flexural strength of ceramic bonds. The experimental results demonstrated that in the ceramic bonds, both ZrO2 and Y2O3 could promote the formation of glass grid, while the ceramic bond strength would further increase. In addition, the new phase of YBO3 appeared in the ceramic bond, due to the filling of Y2O3. When the contents of ZrO2 and Y2O3 were 4 wt% respectively, the strength of the ceramic bond was highest, increasing by 23% (16.1 Mpa) compared to the basic ceramic bond. The last point required to be pointed out was that the phase transformation toughening of ZrO2 cannot be achieved and it was limited by low temperature sintering.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (21)

Show source-provided references
1. Effects of Y2O3 addition on structure and properties of LZAS vitrified bond for CBN grinding tools application10.1016/j.ceramint.2015.04.069 ↗
2. Comparison of tool life between ceramic and cubic boron nitride (CBN) cutting tools when machining hardened steels10.1016/j.jmatprotec.2008.08.016 ↗
3. Study for groove grinding a nickel-based superalloy using electroplated cubic boron nitride (cbn) grinding wheels10.1115/1.1763181 ↗
4. Effect of iron on the wetting, sintering ability, and the physical and mechanical properties of boron carbide composites: a review10.1016/j.ijrmhm.2016.02.007 ↗
5. The influence of sintering parameters on the mechanical properties of vitrified bond diamond tools10.1016/j.matdes.2015.05.011 ↗
6. Effects of Cu on properties of vitrified bond and vitrified CBN composites10.1016/j.ijrmhm.2015.01.002 ↗
7. Effect of CaO on the surface morphology and strength of water soaked Na2O–B2O3–Al2O3–SiO2 vitrified bond10.1016/j.jnoncrysol.2007.12.010 ↗
8. Effect of ZnO on the interfacial bonding between Na2O–B2O3–SiO2 vitrified bond and diamond10.1016/j.solidstatesciences.2009.04.026 ↗
9. Influence of TiO2 on the physical properties of low-temperature ceramic vitrified bond and mechanical properties of CBN composites10.1016/j.ceramint.2012.02.035 ↗
10. Effect of polycrystalline mullite fibers on the properties of vitrified bond and vitrified CBN composites10.1016/j.ceramint.2012.09.059 ↗
11. Effect of Al2O3 additions on the thermal expansion behavior of a Li2O-ZnO-SiO2 glass-ceramic10.1111/j.1151-2916.1999.tb02289.x ↗
12. Transformation toughening mechanisms and application of ZrO2 ceramics
13. The research progress of zirconia ceramics toughening method
14. Effect of nano-ZrO2 on properties and structure of vitrified bond for diamond grinding tools
15. Effect of ZrO2 content on the properties of diamond grinding wheel vitrified bond10.1007/s11595-014-0860-4 ↗
16. Structure and dissolution of CaO–ZrO2–TiO2–Al2O3–B2O3–SiO2 glass (II)
17. Influences of ZrO2 on microstructures and properties of Li2O–Al2O3–SiO2 glass–ceramics for LTCC applications10.1007/s10854-015-3728-2 ↗
18. Transformation toughening in zirconia-containing ceramics10.1111/j.1151-2916.2000.tb01221.x ↗
19. Spark plasma sintering of transparent Y 2 O 3 ceramic using hydrothermal synthesized nanopowders10.1016/j.ceramint.2016.06.022 ↗
20. Properties of Ni/Y2O3 and its catalytic performance in methane conversion to syngas10.1016/j.ijhydene.2011.08.025 ↗
21. Synthesis of mono-dispersed spherical Nd:Y2O3 powder for transparent ceramics10.1016/j.ceramint.2011.06.008 ↗