journal article·2011-01

A feasibility study of W-Cu composites production by high pressure compression of tungsten powder

A. Ghaderi Hamidi, H. Arabi, S. Rastegari

Publisher page

Abstract

Abstract For manufacturing a heavy duty W-Cu composite, a porous tungsten skeleton is required; which later can be filled by molten copper via infiltration technique. The compression force usually up to 200 MPa can be provided by cold isostatic press (CIP) and the temperatures used for sintering the green compacts are more 2000 °C. However, in this research, high pressure within the range of 200 to 663 MPa was used to produce high density green specimens (60-80%) by CIP while sintering was carried out at a moderate temperature of 1550 °C. The tungsten skeletons were infiltrated with molten copper at 1300 °C. The reduction of sintering temperature from over 2000 °C to 1550 °C for a highly densified W-skeleton not only resulted into a successful production of W-Cu composites but also the obtained physical and mechanical properties of these composites are comparable to those obtained for lower compaction pressures and sintering temperature higher than 2000 °C.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (15)

Show source-provided references
1. Evaluation of conductivity in W–Cu composites through the estimation of topological microstructures10.1016/j.matlet.2005.12.113 ↗
2. Arc erosion behavior of a nanocomposite W-Cu electrical contact material10.1016/S1001-0521(06)60011-9 ↗
3. Effect of TiC in copper-tungsten electrodes on EDM performance10.1016/S0924-0136(01)00622-7 ↗
4. Effect of carbide particles on the ablation properties of tungsten composites10.1016/S1044-5803(03)00123-2 ↗
5. Elevated temperature ablation resistance and thermophysical properties of tungsten matrix composites reinforced with ZrC10.1023/A:1017989913219 ↗
6. Lassner · 1999
7. Yih · 1979
8. Mechanical and Thermal Properties of Cu-Infiltrated P/M Tungsten Nozzles10.2514/3.57184 ↗
9. Fabrication of copper infiltrated tungsten jet vanes
10. Barth · 1965
11. Diffusion Mechanism for Tungsten Sintering Kinetics10.1063/1.1713072 ↗
12. Reduction of Sintering Temperature of Porous Tungsten Skeleton Used for Production of W-Cu Composites by Ultra High Compaction Pressure of Tungsten Powder
13. A Normalized Density-Pressure Curve for Powder Compaction
14. Some characteristics of powder consolidation at various pressing stages
15. German · 1996