journal article·2017-11

Electrochemical machining of a solid-state sintered ceramic – A parameter study

M. Schneider, E. Safonow, N. Junker, N. Schubert, A. Michaelis

Publisher page

Abstract

Abstract The present work deals with the electrochemical machining (ECM) of a commercially produced solid-state sintered silicon carbide ceramic (EKasic®D). Current controlled pulse experiments under near-ECM conditions are carried out using a micro-electrochemical flow cell. The influence of different pulse-on time and pulse amplitude, respectively, on the efficiency, the removal rate and the surface morphology was studied. The results clearly show that the higher the applied current density and the longer the pulse-on time the higher the removed material volume. Again, the current efficiency is limited at approximately 25%. Supplementary, electrolyte variations regarding concentration and temperature show a small influence on the efficiency.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (19)

Show source-provided references
1. Silicon carbide and boron carbide based hard materials
2. Sintered silicon carbide for slide bearings and seal rings10.1016/S1350-4789(00)80015-X ↗
3. Electrochemical corrosion of solid and liquid phase sintered silicon carbide in acidic and alkaline environments10.1016/j.jeurceramsoc.2006.07.011 ↗
4. Electrical resistivity of silicon carbide ceramics sintered with 1wt% aluminum nitride and rare earth oxide10.1016/j.jeurceramsoc.2012.07.021 ↗
5. An overview of electric discharge machining of ceramics and ceramic based composites10.1016/j.jmapro.2016.12.010 ↗
6. Laser machining of structural ceramics—a review10.1016/j.jeurceramsoc.2008.11.010 ↗
7. Anodic dissolution of metals at high rates10.1147/rd.372.0207 ↗
8. Electrochemical machining
9. Influence of kinematic operating parameters on kerf geometry in abrasive waterjet machining of silicon carbide ceramics10.1016/j.ijmachtools.2009.07.007 ↗
10. Machining performance of silicon carbide ceramic in end electric discharge milling10.1016/j.ijrmhm.2010.09.001 ↗
11. Electrochemical corrosion of silicon carbide ceramics in H2SO410.1016/j.jeurceramsoc.2013.08.024 ↗
12. Electrochemical corrosion of silicon carbide ceramics. Part 1: electrochemical investigation of sintered silicon carbide (SSiC)10.1002/maco.200905448 ↗
13. Electrochemical corrosion of liquid phase sintered silicon carbide ceramics10.1002/maco.201106283 ↗
14. Anodic dissolution of solid-state sintered silicon carbide at high current densities
15. Moehring · 2004
16. A new microcell or microreactor for material surface investigations at large current densities10.1016/j.electacta.2004.01.068 ↗
17. Electrochemical machining of cemented carbides10.1016/j.ijrmhm.2014.06.010 ↗
18. Sheasby · 2001 · vol. 1 · 326
19. Electrochemical properties of sintered polycrystalline α-SiC10.1007/s11106-005-0011-8 ↗