Effects of Mo target power on the structure and tribological properties of AlB2 Ta1-xMoxB films by magnetron sputtering
Bibliographic record
Abstract
No abstract is available for this record. The assistant can identify its topic from the title, but cannot infer the study’s results.
Source: Not provided · Quality: missing
References (49)
Show source-provided references
1. Advancements in the search for superhard ultra-incompressible metal borides10.1002/adfm.200901257 ↗
2. Architecture of PVD coatings for metalcutting applications: a review10.1016/j.surfcoat.2014.08.068 ↗
3. Plastic deformation of single crystals of CrB2, TiB2 and ZrB2 with the hexagonal AlB2 structure10.1016/j.actamat.2021.116857 ↗
4. Macroscale ultradurable superlubricity on passivated transition-metal diborides10.1016/j.actamat.2023.119439 ↗
5. Where is the unpaired transition metal in substoichiometric diboride line compounds?10.1016/j.actamat.2020.116510 ↗
6. Bamboo-like dual-phase nanostructured copper composite strengthened by amorphous boron framework10.1038/s41467-023-40580-8 ↗
7. Superhard metallic compound TaB2 via crystal orientation resolved strain stiffening
8. Characteristics of sputtered TaBx thin films as diffusion barriers between copper and silicon10.1016/S0169-4332(03)00871-7 ↗
9. Insight into the structure dependence on physical properties of the high temperature ceramics TaB2 boride10.1016/j.vacuum.2020.109427 ↗
10. TaB2-based ceramics: microstructure, mechanical properties and oxidation resistance10.1016/j.jeurceramsoc.2011.07.032 ↗
11. Tribological and biological assessments of TaAgB solid solution coatings for orthodontic treatment10.1016/j.apsusc.2022.153704 ↗
12. Dual-phase nanostructure of amorphous carbon and TaCB solid solution: robust high-performance protective coating for marine equipment10.1016/j.ceramint.2023.04.143 ↗
13. Solid solution hardening of vacancy stabilized TixW1−xB210.1016/j.actamat.2015.08.048 ↗
14. Thermally stable superhard diborides: an ab initio guided case study for V-W-diboride thin films10.1016/j.actamat.2020.01.014 ↗
15. Age hardening in superhard ZrB2-rich Zr1-xTaxBy thin films10.1016/j.scriptamat.2020.09.026 ↗
16. Solving strength–toughness dilemma in superhard transition-metal diborides via a distinct chemically tuned solid solution approach10.34133/research.0035 ↗
17. Ab initio inspired design of ternary boride thin films
18. Alling, B. et al, A theoretical investigation of mixing thermodynamics, age hardening potential, and electronic structure of ternary M11-xM2-xB2 alloys with AlB2 type structure. Sci. Rep. 5, 9888.10.1038/srep09888 ↗
19. Impact of vacancies on structure, stability and properties of hexagonal transition metal diborides, MB2 (M=Sc, Y, Ti, Zr, Hf, V, Nb, ta, Cr, Mo, W, Mn, and Fe)
20. Self-organized columnar Zr0.7Ta0.3B1.5 core/shell-nanostructure thin films10.1016/j.surfcoat.2020.126237 ↗
21. Substoichiometry and tantalum dependent thermal stability of α-structured W-ta-B thin films10.1016/j.scriptamat.2018.06.005 ↗
22. Effect of Cu addition on the microstructure and properties of TiB2 films deposited by a hybrid system combining high power impulse magnetron sputtering and pulsed dc magnetron sputtering10.1016/j.surfcoat.2018.03.026 ↗
23. Electron-configuration stabilized (W,Al)B2 solid solutions10.1016/j.actamat.2019.05.056 ↗
24. Sorting transition-metal diborides: new descriptor for mechanical properties
25. Synthesis and characterization of (Ti1-xAlx)B2+Δ thin films from combinatorial magnetron sputtering10.1016/j.tsf.2018.10.042 ↗
26. Thin WBx and WyTi1−yBx films deposited by combined magnetron sputtering and pulsed laser deposition technique10.1016/j.apsusc.2019.02.006 ↗
27. Stoichiometry, structure and mechanical properties of co-sputtered Ti1-xTaxB2±Δ coatings10.1016/j.surfcoat.2019.04.017 ↗
28. The ideal strength of transition metal diborides TMB2 (TM = Ti, Zr, Hf): plastic anisotropy and the role of prismatic slip10.1016/j.scriptamat.2010.01.009 ↗
29. Spinodal decomposition in the ta-Mo-Al-N films activated by Mo incorporation: toward enhanced hardness and toughness10.1016/j.ceramint.2018.08.189 ↗
30. Effect of Cr addition on oxidation and tribological properties of MoB2-z films by magnetron sputtering
31. Microstructure and properties of Mo doped DLC nanocomposite films deposited by a hybrid sputtering system10.1016/j.vacuum.2022.111732 ↗
32. Toughness measurement of thin films: a critical review10.1016/j.surfcoat.2004.10.021 ↗
33. Structure and mechanical properties of toughening B1 Ta1-xMoxN films with various Mo contents10.1016/j.ceramint.2023.02.179 ↗
34. Effect of sputtering target power density on topography and residual stress during growth of nanocomposite nc-TiN/a-SiNx thin films10.1016/j.diamond.2004.03.008 ↗
35. The effect of process parameters on rhenium diboride films deposited by PLD10.1016/j.surfcoat.2015.07.024 ↗
36. An XPS study of the adherence of refractory carbide, silicide and boride rf sputtered wear-resistant coatings
37. A XPS study of the Mo effect on passivation behaviors for highly controlled stainless steels in neutral and alkaline conditions10.1016/j.apsusc.2012.12.118 ↗
38. Chemical vapor deposition of tantalum nitride with tert-butylimino tris (diethylamino) tantalum and atomic hydrogen10.1016/j.tsf.2004.10.042 ↗
39. Core electron count as a versatile and accurate new descriptor for sorting mechanical properties of diverse transition metal compounds10.1002/adma.202304729 ↗
40. Alling, B. et al, A theoretical investigation of mixing thermodynamics, age hardening potential, and electronic structure of ternary M11-xM2-xB2 alloys with AlB2 type structure. Sci. Rep. 5, n.d. 9888.10.1038/srep09888 ↗
41. Effect of ag target power on structure, mechanical properties of TaC-ag films10.1016/j.ceramint.2022.01.030 ↗
42. Reprint of: improving oxidation and wear resistance of TiB2 films by nano-multilayering with Cr
43. Improved mechanical properties of W-Zr-B coatings deposited by hybrid RF magnetron-PLD method10.1016/j.apsusc.2021.151239 ↗
44. Deformation induced twinning and phase transition in an interstitial intermetallic compound niobium boride10.1016/j.actamat.2018.12.011 ↗
45. Supertoughening in B1 transition metal nitride alloys by increased valence electron concentration10.1016/j.actamat.2010.12.013 ↗
46. Ab initio study of the alloying effect of transition metals on structure, stability and ductility of CrN10.1088/0022-3727/46/36/365301 ↗
47. Effects of the ratio of hardness to Young’s modulus on the friction and wear behavior of bilayer coatings10.1063/1.1811377 ↗
48. Load-independent friction: MoO3 nanocrystal lubricants10.1021/jp9920794 ↗
49. Tribological properties of self-lubricating ta-cu films10.1016/j.apsusc.2017.11.220 ↗