journal article·2023-02

Additive manufacturing of titanium alloys via selective laser melting: Fabrication, microstructure, post-processing, performance and prospect

Jinwen Lu, Longchao Zhuo

Publisher page

Abstract

Growing maturity of SLM has enabled the use of rapid manufacturing technology on hard-to-machine Ti alloys . In this review, selective laser melted titanium alloys are reviewed based on the ever-growing database recently. This study aims to systematically collect relevant and up-to-date information from an exhaustive literature on selective laser melted Ti alloys including the detailed elaboration of recent advances on fabrication, post-processing, microstructure characteristics, mechanical and biocompatibility performances, simulation as well as their correlation of Ti alloys for engineering applications manufactured by SLM. By summarizing the state-of-the-art progress of SLM Ti alloys, five future perspectives on challenges and prospects perspectives for SLM Ti alloys are proposed accordingly. This review advances the associated limitations and overcoming attempts, providing a better understanding and future perceptions on the interdependency between different aspects in this field.
Source: expertdata · Quality: candidate unverified · Source record ↗

Research context

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (100+)

Show source-provided references
1. Deoxygenation of Ti metal: a review of processes in literature10.1016/j.ijrmhm.2020.105270 ↗
2. New opportunities in refractory alloys10.1007/s11661-020-05803-3 ↗
3. In-situ tensile deformation behavior of powder metallurgy Ti6Al4V alloys10.1016/j.ijrmhm.2020.105266 ↗
4. A review of microstructure and texture evolution during plastic deformation and heat treatment of β-Ti alloys10.1016/j.jallcom.2021.163242 ↗
5. Selective laser manufacturing of Ti-based alloys and composites: impact of process parameters, application trends, and future prospects
6. Additive manufacturing of structural materials10.1016/j.mser.2020.100596 ↗
7. Additive manufacturing of titanium-based alloys-a review of methods, properties, challenges, and prospects10.1016/j.heliyon.2022.e09041 ↗
8. A review on metallurgical aspects of laser additive manufacturing (LAM): stainless steels, nickel superalloys, and titanium alloys10.1016/j.jmrt.2021.12.039 ↗
9. Biomedical applications of the powder-based 3D printed titanium alloys: a review10.1016/j.jmst.2021.11.084 ↗
10. Titanium based bone implants production using laser powder bed fusion technology10.1016/j.jmrt.2022.01.087 ↗
11. A critical review on additive manufacturing of Ti-6Al-4V alloy: microstructure and mechanical properties10.1016/j.jmrt.2022.04.055 ↗
12. Additive manufacturing of Ti6Al4V alloy via electron beam melting for the development of implants for the biomedical industry10.1016/j.heliyon.2021.e06892 ↗
13. A state-of-the-art direct metal laser sintering of Ti6Al4V and AlSi10Mg alloys: surface roughness, tensile strength, fatigue strength and microstructure10.1016/j.optlastec.2021.107366 ↗
14. Solidification microstructure simulation of Ti-6Al-4V in metal additive manufacturing: a review
15. Additive manufacturing of Ti6Al4V alloy: a review10.1016/j.matdes.2018.107552 ↗
16. Research trends in laser powder bed fusion of Al alloys within the last decade
17. Main defects observed in aluminum alloy parts produced by SLM: from causes to consequences
18. Review on thermal analysis in laser-based additive manufacturing10.1016/j.optlastec.2018.04.034 ↗
19. Numerical and experimental analysis of the effect of volumetric energy absorption in powder layer on thermal-fluidic transport in selective laser melting of Ti6Al4V10.1016/j.optlastec.2018.09.054 ↗
20. Review on residual stress in selective laser melting additive manufacturing of alloy parts10.1016/j.optlastec.2020.106283 ↗
21. State-of-the-art of selective laser melting process: a comprehensive review10.1016/j.jmsy.2022.04.002 ↗
22. Modeling of the thermal physical process and study on the reliability of linear energy density for selective laser melting10.1016/j.rinp.2018.03.047 ↗
23. Effect of laser power and scan speed on melt pool characteristics of commercially pure titanium (CP-Ti)10.1007/s11665-017-2768-6 ↗
24. Trabecular-like Ti-6Al-4V scaffolds for orthopedic: fabrication by selective laser melting and in vitro biocompatibility10.1016/j.jmst.2019.01.012 ↗
25. Achieving high ductility in a selectively laser melted commercial pure-titanium via in-situ grain refinement10.1016/j.scriptamat.2020.09.023 ↗
26. Additive manufacturing of pure Ti with superior mechanical performance, low cost, and biocompatibility for potential replacement of Ti-6Al-4V10.1016/j.matdes.2020.109142 ↗
27. Densification behavior, microstructure evolution, and mechanical performances of selective laser melted Ti-5Al-2.5Sn alpha titanium alloy: effect of laser energy input10.1016/j.jallcom.2018.09.153 ↗
28. Selective laser melting of near-alpha titanium alloy Ti-6Al-2Zr-1Mo-1V: parameter optimization, heat treatment and mechanical performance10.1016/j.jmst.2020.05.004 ↗
29. Enhanced mechanical properties of Ti-6Al-2Zr-1Mo-1V with ultrafine crystallites and nano-scale twins fabricated by selective laser melting10.1016/j.msea.2018.09.087 ↗
30. Microstructural examination and corrosion behavior of selective laser melted and conventionally manufactured Ti6Al4V for dental applications10.1016/j.msec.2020.110980 ↗
31. Influence of defects on mechanical properties of Ti-6Al-4 V components produced by selective laser melting and electron beam melting10.1016/j.matdes.2015.07.147 ↗
32. Microstructural tailoring of as-selective laser melted Ti6Al4V alloy for high mechanical properties10.1016/j.jallcom.2019.152536 ↗
33. Numerical simulation in the absorption behavior of Ti6Al4V powder materials to laser energy during SLM10.1016/j.jmatprotec.2019.01.002 ↗
34. Selective laser melting of typical metallic materials: an effective process prediction model developed by energy absorption and consumption analysis
35. Synthesis of Ti-5Al, Ti-6Al-7Nb, and Ti-22Al-25Nb alloys from elemental powders using powder-bed fusion additive manufacturing10.1016/j.jallcom.2018.05.325 ↗
36. Influence of processing parameters on density, surface morphologies and hardness of as-built Ti-5Al-5Mo-5V-3Cr alloy manufactured by selective laser melting10.1016/j.jallcom.2022.164760 ↗
37. The aging response of direct laser deposited metastable β-Ti alloy, Ti-5Al-5Mo-5V-3Cr
38. Microstructure and mechanical property of Ti-5Al-5Mo-5V-3Cr-1Zr alloy fabricated by selective laser melting with a preheated substrate10.1002/adem.202100265 ↗
39. Densification, microstructure evolution and fatigue behavior of Ti-13Nb-13Zr alloy processed by selective laser melting10.1016/j.powtec.2018.09.073 ↗
40. Microstructure and mechanical properties of selective laser melted biomaterial Ti-13Nb-13Zr compared to hot-forging10.1016/j.msea.2018.04.001 ↗
41. Microstructural homogeneity and mechanical behavior of a selective laser melted Ti-35Nb alloy produced from an elemental powder mixture10.1016/j.jmst.2020.05.052 ↗
42. Microstructure and corrosion resistance of novel b-type titanium alloys manufactured by selective laser melting10.1016/j.jmrt.2022.07.021 ↗
43. Additive manufacturing of a novel Ti-Al-V-Fe alloy using selective laser melting
44. Metallurgy principles applied to powder bed fusion 3D printing/additive manufacturing of personalized and optimized metal and alloy biomedical implants: an overview10.1016/j.jmrt.2019.12.015 ↗
45. Defect formation mechanisms in selective laser melting: a review, Chin
46. X-ray CT analysis of the influence of process on defect in Ti-6Al-4V parts produced with selective laser melting technology, the10.1007/s00170-019-04347-0 ↗
47. Uncovering the coupled impact of defect morphology and microstructure on the tensile behavior of Ti-6Al-4V fabricated via laser powder bed fusion10.1016/j.jmatprotec.2021.117113 ↗
48. As-fabricated surface morphologies of Ti-6Al-4V samples fabricated by different laser processing parameters in selective laser melting
49. Influence of rescanning parameters on selective laser melting of Ti6Al4V10.1016/j.jmapro.2022.08.034 ↗
50. The influence of process parameters and scanning strategy on lower surface quality of TA15 parts fabricated by selective laser melting10.3390/met10091228 ↗
51. Feedback control of selective laser melting
52. Surface roughness of selective laser melted Ti-6Al-4V alloy components
53. Predicting the porosity defects in selective laser melting (SLM) by molten pool geometry10.1016/j.ijmecsci.2022.107478 ↗
54. Effects of defects and microstructures on tensile properties of selective laser melted Ti6Al4V alloys fabricated in the optimal process zone10.1016/j.msea.2021.142294 ↗
55. Effect of scanning strategy during selective laser melting on surface topography, porosity, and microstructure of additively manufactured Ti-6Al-4V10.3390/app9245554 ↗
56. A study on the surface quality of the 3D printed parts caused by the scanning strategy10.1108/RPJ-06-2017-0125 ↗
57. Optimizing the structure accuracy by changing the scanning strategy using selective laser melting10.1007/s00170-017-1503-7 ↗
58. Texture evolution, phase transformation and mechanical properties of selective laser melted Ti-13Nb-13Zr10.1016/j.matchar.2018.08.053 ↗
59. Simultaneous achievement of equiaxed grain structure and weak texture in Pure Titanium via selective laser melting and subsequent heat treatment10.1016/j.jallcom.2019.06.305 ↗
60. On the texture, phase and tensile properties of commercially pure Ti produced via selective laser melting assisted by static magnetic field10.1016/j.msec.2016.09.011 ↗
61. Microstructure and anisotropic mechanical properties of selective laser melted Ti6Al4V alloy under different scanning strategies10.1016/j.msea.2021.142236 ↗
62. Investigation on the effect of scanning strategy on the corrosion properties of gum metal produced using selective laser melting10.1016/j.matchar.2022.111929 ↗
63. Lattice distortion in selective laser melting (SLM)-manufactured unstable β-type Ti-15Mo-5Zr-3Al alloy analyzed by high-precision X-ray diffractometry10.1016/j.scriptamat.2021.113953 ↗
64. The effect of process parameters on residual stress evolution and distortion in the laser powder bed fusion of Ti-6Al-4V
65. Study of residual stresses in additively manufactured Ti-6Al-4V by neutron diffraction measurements10.1007/s11661-019-05538-w ↗
66. Residual stress evaluation in selective-laser-melting additively manufactured titanium (Ti-6Al-4V) and inconel 718 using the contour method and numerical simulation
67. Effect of solid-state phase transformation on residual stress of selective laser melting Ti6Al4V10.1016/j.msea.2021.141299 ↗
68. An experimental study of residual stress and direction-dependence of fatigue crack growth behaviour in as-built and stress-relieved selective-laser-melted Ti6Al4V10.1016/j.msea.2019.04.023 ↗
69. Reduction of residual stress in porous Ti6Al4V by in situ double scanning during laser additive manufacturing10.1007/s12613-020-2212-z ↗
70. Residual stress, defects and grain morphology of Ti-6Al-4V alloy produced by ultrasonic impact treatment assisted selective laser melting10.3390/app6110304 ↗
71. Role of scanning strategy on residual stress distribution in Ti-6Al-4V alloy prepared by selective laser melting
72. Role of martensite decomposition in tensile properties of selective laser melted Ti-6Al-4V10.1016/j.jallcom.2018.02.111 ↗
73. Prior β grain evolution and phase transformation of selective laser melted Ti6Al4V alloy during heat treatment10.1016/j.jallcom.2022.165235 ↗
74. Mechanism of stress relaxation and phase transformation in additively manufactured Ti-6Al-4V via in situ high temperature XRD and TEM analyses10.1016/j.actamat.2020.02.056 ↗
75. Coupling effects of high magnetic field and annealing on the microstructure evolution and mechanical properties of additive manufactured Ti–6Al–4V10.1016/j.msea.2021.141815 ↗
76. Microstructural and mechanical optimization of selective laser melted Ti6Al4V lattices: effect of hot isostatic pressing10.1016/j.jmapro.2022.02.024 ↗
77. Productivity optimization of laser powder bed fusion by hot isostatic pressing
78. Effects of electropulsing on the microstructure and microhardness of a selective laser melted Ti6Al4V alloy10.1016/j.jallcom.2021.160044 ↗
79. Post-processing of additively manufactured metallic alloys-a review10.1016/j.ijmachtools.2022.103908 ↗
80. The influence of chemical polishing of titanium scaffolds on their mechanical strength and in-vitro cell response10.1016/j.msec.2018.04.019 ↗
81. Laser polishing of additive manufactured Ti6Al4V alloy: a review10.1117/1.OE.60.2.020901 ↗
82. High-performance integrated additive manufacturing with laser shock peening-induced microstructural evolution and improvement in mechanical properties of Ti6Al4V alloy components10.1016/j.ijmachtools.2019.103475 ↗
83. Effect of laser remelting on deposition quality, residual stress, microstructure, and mechanical property of selective laser melting processed Ti-5Al-2.5Sn alloy10.1016/j.matchar.2019.02.010 ↗
84. Influence of strut-size and cell-size variations on porous Ti6Al4V structures for load-bearing implants10.1016/j.jmbbm.2021.105023 ↗
85. Fatigue behavior and osseointegration of porous Ti-6Al-4V scaffolds with dense core for dental application10.1016/j.matdes.2020.108994 ↗
86. Additive manufacturing of metallic lattice structures: unconstrained design, accurate fabrication, fascinated performances, and challenges10.1016/j.mser.2021.100648 ↗
87. Properties and applications of additively manufactured metallic cellular materials: a review10.1016/j.pmatsci.2021.100918 ↗
88. Cell-size graded sandwich enhances additive manufacturing fidelity and energy absorption10.1016/j.ijmecsci.2021.106798 ↗
89. Non-layer-wise fracture and deformation mechanism in beta titanium cubic lattice structure manufactured by selective laser melting10.1016/j.msea.2021.141696 ↗
90. Effect of heating treatment on the microstructural evolution and dynamic tensile properties of Ti-6Al-4V alloy produced by selective laser melting10.1016/j.jmapro.2021.12.035 ↗
91. Evolution of the microstructure and optimization of the tensile properties of the Ti-6Al-4V alloy by selective laser melting and heat treatment10.1016/j.msea.2020.140673 ↗
92. Experimental realisation of build orientation effects on the mechanical properties of truly as-built Ti-6Al-4V SLM parts10.1016/j.jmapro.2021.01.027 ↗
93. Anisotropic mechanical behavior of biomedical Ti-13Nb-13Zr alloy manufactured by selective laser melting10.1016/j.jallcom.2018.05.179 ↗
94. Effects of selective laser melting build orientations on the microstructure and tensile performance of Ti–6Al–4V alloy10.1016/j.msea.2020.139001 ↗
95. Influence of processing parameters of selective laser melting on high-cycle and very-high-cycle fatigue behavior of Ti-6Al-4V10.1111/ffe.13361 ↗
96. High cycle fatigue in selective laser melted Ti-6Al-4V10.1016/j.actamat.2020.05.041 ↗
97. Constitutive and damage modelling of selective laser melted Ti-6Al-4V lattice structure subjected to low cycle fatigue10.1016/j.ijfatigue.2022.106800 ↗
98. Prediction of anisotropic LCF behavior for SLM Ti-6Al-4V considering the spatial orientation of defects10.1016/j.ijfatigue.2022.106734 ↗
99. Fatigue performance differences between rolled and selective laser melted Ti6Al4V alloys10.1016/j.matchar.2022.111963 ↗
100. Microstructural optimization through heat treatment for enhancing the fracture toughness and fatigue crack growth resistance of selective laser melted Ti-6Al-4V alloy10.1016/j.actamat.2019.03.003 ↗