Abstract
In this paper, PcBN composites with high strength and high thermal stability were prepared by high temperature and high pressure sintering at 5.5 GPa and 1450 °C using Al-TiSi 2 as binder. The effects of TiSi 2 content on the phase composition, microstructure, mechanical properties, and thermal stability of PcBN composites were investigated. The results indicate that the density of the composites increases with an increase in the TiSi 2 content. The mechanical properties of the composites were found to be the best at 25 wt% TiSi 2 , where the hardness was 3475 HV, and the bending strength was 782.7 MPa. Furthermore, the PcBN composites exhibited good thermal stability in the temperature range of 400 °C–1200 °C due to the presence of the reaction product Si and partially oxidized SiO 2 , which prevented oxidation.
Source: expertdata · Quality: candidate unverified · Source record ↗
Research context
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (37)
Show source-provided references
1. Superhard pcBN tool materials with Ti3SiC2 MAX-phase binder: structure, properties, application[J]10.3103/S1063457617030029 ↗
2. Sintering of cBN based materials with a TaC binder for cutting tool application[J]10.3103/S1063457620020112 ↗
3. Study of fragmentation in cBN powders under ultra-high pressure[J]10.1016/j.ceramint.2019.09.135 ↗
4. In situ synthesis of polycrystalline cubic boron nitride in cBN-Al-Ti system with different Gd2O3 additions[J]10.1007/s12598-020-01407-3 ↗
5. Self-bonding mechanism of pure polycrystalline cubic boron nitride under high pressure and temperature[J]
6. Effect of the TiC-TiB2-AlN system on properties of PCBN tool material[J]
7. Micromechanical mapping of polycrystalline cubic boron nitride composites by means of high-speed nanoindentation: assessment of microstructural assemblage effects[J]10.1016/j.jeurceramsoc.2022.08.047 ↗
8. Influence of binder systems on sintering characteristics, microstructures, and mechanical properties of PcBN composites fabricated by SPS[J]
9. Reaction behavior during spark plasma sintering of cBN-TiCN-Ni powders[J]10.1016/j.jeurceramsoc.2023.06.074 ↗
10. In situ synthesis of polycrystalline cubic boron nitride with high mechanical properties using rod-shaped TiB2 crystals as the binder[J]10.1080/17436753.2017.1343781 ↗
11. In situ synthesis of polycrystalline cubic boron nitride reinforced by different morphologic TiB2[J]10.1007/s11665-020-04896-6 ↗
12. Effect of sintering temperature on synthesis of PCBN in cBN-Ti-Al-W system[J]
13. Enhanced mechanical properties of cBN-Al-Si3N4 composites by introducing diamond[J]
14. TEM investigation of high-pressure reaction-sintered cBN-Al composites[J]10.1023/B:JMSC.0000034176.85765.40 ↗
15. Study of high-pressure sintering behavior of cBN composites starting with cBN-Al mixtures[J]10.1557/jmr.2008.0316 ↗
16. Fabrication of high thermal conductive Al-cBN ceramic sinters by high temperature high pressure method[J]10.1016/j.solidstatesciences.2011.01.023 ↗
17. Self-propagation high-temperature sintering of the Ti-Al-C-diamond/BN system[J]10.3139/146.111039 ↗
18. Effect of diamond additive on the properties of cBN composites with Al-Si as binder by HTHP sintering[J]10.1016/j.ceramint.2022.03.028 ↗
19. The influence of microstructure on the fracture properties of polycrystalline cubic boron nitride[J]10.1016/j.commatsci.2015.06.036 ↗
20. Effect of Al Ti content on mechanical properties of in-situ synthesized PcBN composites[J]
21. Cubic boron nitride—Ti/TiN composites: hardness and phase equilibrium as function of temperature[J]10.1016/j.jallcom.2004.04.140 ↗
22. Synthesis and characterization of cBN-Al2O3-Al cutting tool material by dual power spark plasma sintering[J]
23. Toughening, reinforcement and repair mechanisms of TiSi2 in Al2O3/TiN/TiSi2 ceramics[J]
24. Evaluation of thermal conductivities and thermal expansion coefficients of TiSi2 and Ti5Si3 ceramics prepared from Ti- and Si-rich wastes[J]
25. Preparing B4C-SiC-TiB2 composites via reactive pressureless sintering with B4C and TiSi2 as raw materials[J]10.1016/j.jmrt.2020.05.124 ↗
26. Densification, sintering reactions, and properties of titanium diboride with titanium disilicide as a sintering aid[J]10.1111/j.1551-2916.2007.01911.x ↗
27. Effect of titanium content on microstructure and mechanical properties of PcBN synthesized in cBN-Si3N4-Ti system[J]10.1002/mawe.201900089 ↗
28. Effects of Al2O3 addition on sintering behaviour, microstructure, and physical properties of Al2O3/vitrified bond CBN composite[J]10.1016/j.ceramint.2022.11.080 ↗
29. Composition, microstructure and mechanical properties of cBN-based composites sintered with AlN- Al- Ni binder[J]10.1016/j.ceramint.2018.06.130 ↗
30. Sintering behaviors of fine-grained cBN-10 wt.% Al3.21Si0.47 system under high pressure[J]10.1016/j.diamond.2012.08.001 ↗
31. Microstructure and mechanical properties of cBN-WC-Co composites used for cutting tools[J]10.1007/s00170-014-6410-6 ↗
32. Preparation and characterization of cBN-based composites from cBN-Ti3AlC2 mixtures[J]10.1016/j.diamond.2016.05.003 ↗
33. Preparation and cutting performance study of YSZ-toughened PcBN superhard tools[J]10.1039/D3RA02079G ↗
34. Microstructure and mechanical properties of TiB2–SiC ceramic composites by Reactive Hot Pressing[J]10.1016/j.ijrmhm.2013.10.007 ↗
35. High thermal stability of diamond-cBN-B4C-Si composites[J]10.1088/1674-1056/26/1/018102 ↗
36. Microstructural and mechanical properties of cBN-Si composites prepared from the high pressure infiltration method[J]10.1016/j.ijrmhm.2016.07.020 ↗
37. Preparation of polycrystalline cBN containing nanodiamond[J]10.1016/j.jmatprotec.2007.06.080 ↗