journal article·2022-06

Tungsten carbide molds for precision glass molding process: Mechanism of high-temperature degradation

Shengdi Sun, Kangsen Li, Wenyan Chu, Feng Gong

Publisher page

Abstract

Tungsten carbide (WC) is a well-established material used in glass molding field due to its low thermal expansion and high compressive strength at elevated temperatures. During glass molding process, the WC mold has to withstand thousands of thermo-mechanical coupled interactions in the aerobic environment. Understanding the degradation mechanism of WC substrate during precision glass molding is very important for the design and preparation of protective coatings and the optimization of glass molding process. In this study, surface failure analysis of WC substrate was carried out using barrel compression test and ball-to-disk friction test. The microstructures, element compositions, surface morphology of the WC substrates were measured by X-ray diffraction analysis (XRD), scanning electron microscopy (SEM), and white light interferometer (WLI). Damaging phenomena such oxidation, interdiffusion, spallation, glass sticking, and surface roughening on the WC substrate were observed. The experimental results showed that the WC substrate degraded very rapidly at above 600 °Cand air environment. The fundamental degradable reason of WC substrate is the oxidation, which directly leads to the decrease of the material strength, the aggravation of the wear, occurring of the glass sticking, and the increase of surface roughness. Furthermore, the WC mold microhole array without protective coatings can be used to fabricate the glass microlens array in a suitable glass molding environment. This work provides engineering guidance for the fabrication of glass optics during glass molding process.
Source: expertdata · Quality: candidate unverified · Source record ↗

Research context

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (24)

Show source-provided references
1. Temperature effect on the deformation and optical quality of moulded glass lenses in precision glass moulding10.1111/ijag.13617 ↗
2. Direct nanoimprinting of moth-eye structures in chalcogenide glass for broadband antireflection in the mid-infrared10.1364/OPTICA.5.000557 ↗
3. Investigation on shape transferability in ultraprecision glass molding press for microgrooves10.1016/j.precisioneng.2010.09.011 ↗
4. Compression molding of aspherical glass lenses-a combined experimental and numerical analysis10.1111/j.1551-2916.2005.00137.x ↗
5. Deformation behavior of glass nanostructures in hot embossing10.1021/acsami.0c08435 ↗
6. Surface evolution analysis of CrxWyNz coatings on WC mold in glass molding process10.1016/j.surfcoat.2020.125839 ↗
7. Study on the design of precious metal based protective films for glass moulding process10.1016/j.surfcoat.2012.10.066 ↗
8. Chemical inertness of Cr–W–N coatings in glass molding10.1016/j.tsf.2015.09.044 ↗
9. PtIr protective coating system for precision glass molding tools: design, evaluation and mechanism of degradation10.1016/j.surfcoat.2020.125378 ↗
10. Effect of annealing environment on the microstructure and mechanical property of CrWN glass molding coating10.1016/j.surfcoat.2019.125281 ↗
11. High-temperature friction behavior of amorphous carbon coating in glass molding process10.1007/s40544-020-0452-6 ↗
12. Surface failure analysis of AlCrN coating on WC substrate subjected to high-temperature oxidation in glass-molding machine10.1016/j.apsusc.2018.05.031 ↗
13. Oxidation of WC-Co, WC-Ni and WC-Co-Ni hard metals in the temperature range 500–800 °C10.1016/0263-4368(96)00009-1 ↗
14. Strength degradation of a tungsten carbide-cobalt composite at elevated temperatures10.1016/S1044-5803(98)00056-4 ↗
15. Oxidation resistant tungsten carbide hardmetals10.1016/j.ijrmhm.2017.03.009 ↗
16. Oxidation-induced strength degradation of WC–Co hardmetals10.1016/S0263-4368(01)00033-6 ↗
17. Comparison of the oxidation behaviour of WC-Co and WC-Ni-Co-Cr cemented carbides10.1016/j.corsci.2011.05.006 ↗
18. Oxidation behavior of WC-Co10.1016/0921-5093(95)10145-4 ↗
19. New perspectives in hardmetal abrasion simulation10.1016/j.wear.2017.01.038 ↗
20. Understanding the wear failure mechanism of TiAlSiCN nanocomposite coating at evaluated temperatures10.1016/j.triboint.2020.106716 ↗
21. A numerical and experimental study on the interface friction of ball-on-disc test under high temperature10.1016/j.wear.2016.11.035 ↗
22. Tribological behavior and wear mechanism of pure WC at wide range temperature from 25 to 800°C in vacuum and air environment10.1016/j.ijrmhm.2017.11.024 ↗
23. Oxidation of ultrafine-cemented carbide prepared from nanocrystalline WC–10Co composite powder10.1016/j.ceramint.2007.07.029 ↗
24. Damage of different tungsten carbides under impact-sliding motion10.1016/j.wear.2016.12.046 ↗