Abstract The abrasion resistance of WC–40vol%(FeAl–B), WC–40vol%(Ni 3 Al–B), and WC–40vol%Co, prepared from ultra fine precursor powders and processed by uniaxial hot pressing, has been investigated using a pin-on-drum tester. Intermetallic binders, with different amount of boron including 0, 250, 500, 750, and 1000 ppm B, were prepared in ultrafine form under controlled atmosphere using ring grinding, blended with submicron (0.8 μm) WC powder and then uniaxially hot pressed at 1500 °C under a pressure of 20 MPa for 4 min in 10 −2 MPa argon atmosphere. In an additional investigation, wear results were compared with that of commercial H10F (WC–10wt%Co, WC particle size of 0.7 μm). It was found that the wear resistance of WC–FeAl–B and WC–Ni 3 Al–B increased with the increasing amount of boron. WC–40vol%FeAl–B showed the highest abrasion resistance, close to that for WC–10wt%Co (H10F) composite, followed by WC–40vol%Ni 3 Al–B and WC–40vol%Co.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (19)
Show source-provided references
1. Indentation fracture of WC–Co cermets10.1007/BF00555296 ↗
2. Abrasion resistance of cermets containing Co/Ni binders
3. Friction and wear behavior of several hard materials10.1016/S0263-4368(01)00028-2 ↗
4. Abrasion resistance of nanostructured and conventional cemented carbides
5. Resistance of cemented carbides to sliding abrasion
6. Microstructure and mechanical and tribological properties of high carbon Fe3Al and FeAl intermetallic alloys10.2320/matertrans.43.36 ↗
7. The resistance of nickel and iron aluminides to cavitation erosion and abrasive wear10.1016/0043-1648(90)90090-W ↗
8. Structural applications of intermetallic compounds
9. Iron and nickel aluminide composites10.1080/02533839.1999.9670437 ↗
10. Identification of thermodynamically stable ceramic reinforcement materials for iron aluminides10.1007/BF02782424 ↗
11. Liquid-phase sintered iron aluminide-ceramic composites10.1016/S0966-9795(96)00066-0 ↗
12. Wetting of TiC–WC system carbides with molten Ni3Al10.1007/BF00813961 ↗
13. Tungsten carbide iron aluminide hardmetals: nanocrystalline vs microcrystalline10.4028/www.scientific.net/MSF.360-362.649 ↗
14. Liquid phase sintering of WC–FeAl and WC–Ni3Al composites with and without boron10.4028/www.scientific.net/MSF.426-432.1951 ↗
15. Fracture toughness of monolithic nickel aluminide intermetallics10.1016/0921-5093(92)90375-B ↗
16. Grain boundary chemistry in Ni3Al and Ni3Si
17. Intermetallic bonded WC-based cermets by pressureless melt infiltration10.1016/S0966-9795(97)00010-1 ↗
18. Abrasive wear of intermetallic-based alloys and composites10.1016/S0921-5093(97)00681-3 ↗
19. Environmental embrittlement in boron-free and boron-doped FeAl (40at.%Al) alloys10.1016/0956-716X(90)90343-F ↗