Research on the fracture toughness of pipeline steel X80 in a hydrogen environment
Bibliographic record
Abstract
No abstract is available for this record. The assistant can identify its topic from the title, but cannot infer the study’s results.
Source: Not provided · Quality: missing
Research context
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (35)
Show source-provided references
1. Effect of ultrasonic impact treatment on hydrogen embrittlement susceptibility of X80 pipeline steel10.1016/j.ijhydene.2025.02.321 ↗
2. The energy transition towards hydrogen utilization for green life and sustainable human development in Patagonia10.1016/j.ijhydene.2020.01.246 ↗
3. Hydrogen effects on X80 pipeline steel in high-pressure natural gas/hydrogen mixtures10.1016/j.ijhydene.2016.05.145 ↗
4. Enhanced hydrogen degradation of two pipeline steels by increasing inert gas pressure in hydrogen-containing mixtures: experimental and theoretical insights10.1016/j.corsci.2024.112466 ↗
5. Influence of hydrogen in natural gas mixed hydrogen environment on mechanical properties of X80 pipeline steel10.1016/j.ijhydene.2023.09.138 ↗
6. Investigation on dynamic deformation and damage of steel ribbon wound vessel for hydrogen storage under fragment impact loading
7. Anderson · 2017
8. Fatigue and fracture of pipeline steels in high-pressure hydrogen gas
9. San Marchi · 2012
10. Fracture Property Testing of Carbon Steel in High Pressure Hydrogen
11. Effect of high pressure hydrogen gas on fatigue and fracture properties of API X65 linepipe steels
12. Different effects of pure hydrogen vs. hydrogen/natural gas mixture on fracture toughness degradation of two carbon steels10.1016/j.matlet.2021.129924 ↗
13. The synergistic action and interplay of hydrogen embrittlement mechanisms in steels and iron: localized plasticity and decohesion10.1016/j.engfracmech.2019.106528 ↗
14. Hydrogen-enhanced localized plasticity—a mechanism for hydrogen-related fracture10.1016/0921-5093(94)90975-X ↗
15. Quantitative estimation method of the effect of segregated solute on hydrogen-enhanced decohesion at a grain boundary10.1016/j.scriptamat.2024.116366 ↗
16. Hydrogen damage of steels: a case study and hydrogen embrittlement model10.1016/j.engfailanal.2015.05.017 ↗
17. A quantitative description on fracture toughness of steels in hydrogen gas10.1016/j.ijhydene.2013.07.033 ↗
18. The fracture toughness and its prediction model for Ti–5Al–5Mo–5V–1Cr–1Fe titanium alloy with basket-weave microstructure10.1016/j.jallcom.2015.01.217 ↗
19. Predictive environmental hydrogen embrittlement on fracture toughness of commercial ferritic steels with hydrogen-modified fracture strain model10.1016/j.ijhydene.2021.12.128 ↗
20. On the effect of hydrogen on the fracture toughness of steel10.1007/s10704-005-1974-7 ↗
21. Metallic materials–Unified method of test for the determination of quasistatic fracture toughness, ISO 12135-20212021.
22. H.W. Liu, Stress-corrosion cracking and the interaction between crack-tip stress field and solute atoms, 1970.10.1115/1.3425090 ↗
23. G.R. Irwin, Analysis of stresses and strains near the end of a crack traversing a plate, 1957.10.1115/1.4011547 ↗
24. On the relationship between critical tensile stress and fracture toughness in mild steel10.1016/0022-5096(73)90008-2 ↗
25. ASME BPVC VIII-3 KD-4.
26. Microstructure and mechanical property performance of commercial grade API pipeline steels in high pressure gaseous hydrogen
27. API579-1/ASME FFS-1-2016. Fitness-For-Service, 2016.
28. Fracture resistance and fatigue crack growth of X80 pipeline steel in gaseous hydrogen
29. GB/T 19624-2019. Safety Assessment of In-Service Pressure Equipment Containing Defects, 2019.
30. Mitigating hydrogen embrittlement in CoCrNi alloy using a self-refilling nanoscale amorphous oxide layer10.1016/j.corsci.2025.112941 ↗
31. Hydrogen embrittlement of additively manufactured metallic materials10.1016/j.ijhydene.2025.03.222 ↗
32. Effects of Al2O3 diffusion barrier layer (including Y-containing small oxide precipitates) and nanostructured YSZ top coat on the oxidation behavior of HVOF NiCoCrAlTaY/APS YSZ coatings at 1100 °C10.1016/j.corsci.2018.07.013 ↗
33. Modification of surface hardness, wear resistance and corrosion resistance of cold spray Al coated AZ31B Mg alloy using cold spray double layered Ta/Ti coating in 3.5 wt % NaCl solution10.1016/j.corsci.2020.109029 ↗
34. Oxygen impurity effects on hydrogen assisted fatigue and fracture of X100 pipeline steel
35. Inhibiting effect of carbon monoxide on gaseous hydrogen embrittlement of pipelines transporting hydrogen10.1016/j.corsci.2023.111789 ↗