The Influence of NH 4 F on the Etch Rates of Undoped SiO2 in Buffered Oxide Etch

Harald Proksche, Günter Nagorsen, Detlef Ross

Publisher page

Abstract

The dependence of etch rates of thermal oxide and undoped vapor‐deposited silicon dioxides as a function of the composition of buffered was examined. The composition of the buffered oxide etch (BOE) was varied from 0–30 weight percent (w/o) ammonium fluoride with 2–15 w/o hydrofluoric acid . The etch rates of the silicon dioxides run through a maximum. The position of the maximum increases linearly to higher concentrations with higher content. For the reaction of dissolution, two different paths are discussed. In BOE with concentration lower than 15 w/o silicon dioxides react mainly with . With higher ammonium fluoride concentration the reaction with becomes increasingly dominant. In BOE with 6 w/o , the activation energy for the reaction of dissolution was determined. Diagrams of etch rates as a function of and concentration are presented.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Semiconductor materials and devices · Ga2O3 and related materials · Plasma Diagnostics and Applications

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

Department of Inorganic Chemistry, University of Munich, 8000 Munich, Germany

Siemens AG, Semiconductor Group, Otto Hahn Ring 6, 8000 Munich 83, Germany

References

Reference metadata was not supplied for this record.