journal article·2025-04-01Open access

Stress Corrosion Cracking of NaSICON Membranes in Aqueous Electrolytes for Redox-Flow Batteries

Mengyao Zhang, Kang-Ting Tseng, David G. Kwabi, Jeff Sakamoto, Neil P. Dasgupta, M. D. Thouless

Abstract

The sodium super-ionic conductor (NaSICON) has versatile applications as a ceramic electrolyte for energy storage, where it can serve as an impermeable separator in solid-state batteries and redox flow systems. In particular, NaSICON systems have been proposed to be relatively stable in contact with water, making them compatible with aqueous battery chemistries. However, owing to their brittle nature and metal oxide constituents, stress-corrosion cracking (SCC) is an important failure mechanism that has not been previously explored. In this study, we assess the fracture toughness of NaSICON membranes in contact with aqueous solutions that are relevant to redox flow systems. Microindentation was performed to generate visible surface cracks and residual stress, which were observed to grow in length after exposure to aqueous solutions. This allows for a quantitative measurement of fracture toughness, which decreases after exposure to water. To contextualize these results, we develop a simplified model of the fracture behavior in aqueous redox-flow batteries that incorporate NaSICON membranes, illustrating the importance of SCC in cell design. This work provides quantitative insights into SCC as a failure mode in NaSICON, enhancing our understanding of the chemo-mechanical behavior of ceramic electrolytes in contact with aqueous solutions.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Advanced battery technologies research · Advanced Battery Materials and Technologies · Thermal Expansion and Ionic Conductivity

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (49)

Show source-provided references
1. Electrochemical and surface chemistry analysis of lithium lanthanum zirconium tantalum oxide (LLZTO)/Liquid electrolyte (LE) interfaces10.1016/j.jpowsour.2020.228598 ↗
2. Liquids-to-power using low-temperature solid oxide fuel cells10.1002/ente.201800408 ↗
3. Correlating stability and performance of NaSICON membranes for aqueous redox flow batteries10.1021/acsami.2c00266 ↗
4. Assessment methods and performance metrics for redox flow batteries10.1038/s41560-020-00772-8 ↗
5. Energy efficient Na-aqueous-catholyte redox flow battery10.1016/j.ensm.2017.10.006 ↗
6. Studying voltage losses during discharge for biphenyl-sodium polysulfide organic redox flow batteries10.1016/j.jpowsour.2023.233538 ↗
7. Toward an inexpensive aqueous polysulfide−polyiodide redox flow battery10.1021/acs.iecr.7b01476 ↗
8. Polysulfide-based redox flow batteries with long life and low levelized cost enabled by charge-reinforced ion-selective membranes10.1038/s41560-021-00804-x ↗
9. Long-life polysulfide−polyhalide batteries with a mediator-ion solid electrolyte10.1021/acsaem.9b00253 ↗
10. Liang · Nat. Commun. · 2023 · 14 · 359110.1038/s41467-023-39385-6 ↗
11. An aqueous redox flow battery based on neutral alkali metal ferri/ferrocyanide and polysulfide electrolytes10.1149/2.0221601jes ↗
12. High energy density MnO4−/MnO42− redox couple for alkaline redox flow batteries10.1039/C6CC08070G ↗
13. Ti-substituted tunnel-type Na 0.44 MnO2 oxide as a negative electrode for aqueous sodium-ion batteries10.1038/ncomms7401 ↗
14. Na + ion-selective desalination system utilizing a NASICON ceramic membrane10.1016/j.watres.2022.118250 ↗
15. Elimination of active species crossover in a room temperature, neutral pH, aqueous flow battery using a ceramic NaSICON membrane10.1016/j.jpowsour.2017.12.041 ↗
16. Survey of the transport properties of sodium superionic conductor materials for use in sodium batteries10.1016/j.jpowsour.2014.09.137 ↗
17. Conductivity versus structure dependence investigation of Na1+xZr2SixP3-xO12 (0 ≤ x ≤ 3) through composition optimization by adjusting Si/P ratio10.1016/j.mtchem.2023.101495 ↗
18. Room temperature demonstration of a sodium superionic conductor with grain conductivity in excess of 0.01 S cm−1 and its primary applications in symmetric battery cells10.1039/c9ta00048h ↗
19. Zirconia-free NaSICON solid electrolyte materials for sodium all-solid-state batteries10.1039/D3TA04665F ↗
20. Improving the ionic conductivity of NASICON through aliovalent cation substitution of Na3Zr2Si2PO1210.1007/s11581-015-1498-8 ↗
21. Multiscale Investigation into Chemically Stable NASICON Solid Electrolyte in Acidic Solutions10.1021/acsami.1c07601 ↗
22. Transport property requirements for flow battery separators10.1149/2.0051601jes ↗
23. Investigation on the structure and properties of Na3.1Zr1.55Si2.3P0.7O11as a solid electrolyte and its application in a seawater battery10.1021/acsami.1c17338 ↗
24. Mechanical properties of NaSICON: a brief review10.1007/s11581-022-04820-z ↗
25. Reaction of NASICON with water10.1016/S0167-2738(01)00683-X ↗
26. Influence of water vapor on crack propagation in soda-lime glass10.1111/j.1151-2916.1967.tb15145.x ↗
27. A molecular interpretation of stress corrosion in silica10.1038/295511a0 ↗
28. The use of hot-pressing to reduce grain boundary resistance in Nasicon of nominal composition Na3Zr2Si2PO1210.1016/j.ssi.2024.116561 ↗
29. An improved technique for determining hardness and elastic modulus using load and displacement sensing indentation experiments10.1557/JMR.1992.1564 ↗
30. Micromechanical assessment of Al/Y-substituted NASICON solid electrolytes10.1016/j.ceramint.2019.07.114 ↗
31. Microstructural and mechanical characterization of Na1+xHf2Si2.3P0.7O10.85+0.5x and Na1+xZr2P3-xSixO12 NASICON-type solid electrolytes10.1007/s10853-022-08023-9 ↗
32. Elastic/plastic indentation damage in ceramics: the median/radial crack system10.1111/j.1151-2916.1980.tb10768.x ↗
33. Microfracture beneath point indentations in brittle solids10.1007/BF00541038 ↗
34. A critical evaluation of indentation techniques for measuring fracture toughness: I, direct crack measurements10.1111/j.1151-2916.1981.tb10320.x ↗
35. Characterization of hot-pressed von Alpen type NASICON ceramic electrolytes10.1016/j.ssi.2021.115712 ↗
36. Composite NASICON (Na3Zr2Si2PO12) solid-state electrolyte with enhanced Na + ionic conductivity: effect of liquid phase sintering10.1021/acsami.9b14986 ↗
37. Analysis of stresses and strains near the end of a crack traversing a plate10.1115/1.4011547 ↗
38. The impact of pH on side reactions for aqueous redox flow batteries based on nitroxyl radical compounds10.1016/j.jpowsour.2016.04.136 ↗
39. Unraveling pH dependent cycling stability of ferricyanide/ferrocyanide in redox flow batteries10.1016/j.nanoen.2017.10.057 ↗
40. Organic redox species in aqueous flow batteries: redox potentials, chemical stability and solubility10.1038/srep39101 ↗
41. Differential pH as a method for increasing cell potential in organic aqueous flow batteries10.1039/C7TA04975G ↗
42. Long-term stability of ferri-/ferrocyanide as an electroactive component for redox flow battery applications: on the origin of apparent capacity fade10.1149/1945-7111/ace936 ↗
43. Corrosion stability of NASICON-based membranes against aqueous solutions: case study for sodium iodine batteries10.1039/d4ta05638h ↗
44. Effect of corrosion processes on subcritical crack growth in glass10.1111/j.1151-2916.1981.tb15870.x ↗
45. Stress-corrosion mechanisms in silicate glasses10.1088/0022-3727/42/21/214006 ↗
46. Stress corrosion cracking of quartz: A note on the influence of chemical environment10.1016/0040-1951(81)90157-8 ↗
47. NaSICON prepared by a solution-assisted reaction shows enhanced stability for high-voltage aqueous redox-flow batteries10.1021/acsaem.4c01739 ↗
48. An aqueous, polymer-based redox-flow battery using non-corrosive, safe, and low-cost materials10.1038/nature15746 ↗
49. Dowling · 2007