Nanometer-Scale Corrosion of Copper in De-Aerated Deionized Water
Source abstract
Abstract
Copper is commonly regarded to be immune to corrosion in deaerated deionized electrolytes. The present work shows that, in the absence of hydrogen, copper will corrode on the order of 1 nm/day in deionized water with an O 2 concentration on the order of, or less than, 1 ppb. While a corrosion rate of this magnitude can normally be neglected, it may be catastrophic for nanoscale copper structures utilized in emerging applications to enhance energy transport at the solid-electrolyte interface, such as in cooling advance electronics. This conclusion is supported by a set of experimental and analytical studies that encompass impedance spectroscopy, slow-scan linear sweep voltammetry, thermodynamic calculations for the environment under study, and kinetic simulations. The studies provide a comprehensive insight on details of the corrosion mechanism for copper in deaerated water.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Electrocatalysts for Energy Conversion · Electrochemical Analysis and Applications · Corrosion Behavior and Inhibition
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (50)
Show source-provided references
1. 10.1115/1.400570810.1115/1.4005708 ↗
2. 10.1016/S0065-2717(01)80022-810.1016/S0065-2717(01)80022-8 ↗
3. 10.1109/TDMR.2004.84016010.1109/TDMR.2004.840160 ↗
4. 10.1016/S0035-3159(98)80089-510.1016/S0035-3159(98)80089-5 ↗
5. Zhang C. , Analytical and Experimental Investigation of Capillary Forces Induced by Nanopillars for Thermal Management Applications, Ph.D. dissertation, University of Texas (2010).
6. 10.1021/nl802685710.1021/nl8026857 ↗
7. 10.1016/j.ijheatmasstransfer.2012.12.03010.1016/j.ijheatmasstransfer.2012.12.030 ↗
8. 10.1109/EDL.1981.2536710.1109/EDL.1981.25367 ↗
9. 10.1109/33.18004910.1109/33.180049 ↗
10. 10.1016/0017-9310(94)90103-110.1016/0017-9310(94)90103-1 ↗
11. 10.1016/j.applthermaleng.2005.03.00810.1016/j.applthermaleng.2005.03.008 ↗
12. 10.1016/j.applthermaleng.2006.02.03610.1016/j.applthermaleng.2006.02.036 ↗
13. 10.1016/j.applthermaleng.2009.07.00310.1016/j.applthermaleng.2009.07.003 ↗
14. 10.1016/j.ijheatmasstransfer.2012.12.05810.1016/j.ijheatmasstransfer.2012.12.058 ↗
15. 10.1080/15567265.2011.57591810.1080/15567265.2011.575918 ↗
16. 10.1149/1.212877310.1149/1.2128773 ↗
17. 10.1149/1.222091710.1149/1.2220917 ↗
18. 10.1149/1.240347710.1149/1.2403477 ↗
19. Newman J. S. Thomas-Alyea K. E. , Electrochemical Systems, 3rd edition (Hoboken, NJ: John Wiley & Sons, 2004).
20. 10.1016/0010-938X(89)90125-X10.1016/0010-938X(89)90125-X ↗
21. 10.1016/j.corsci.2010.09.03710.1016/j.corsci.2010.09.037 ↗
22. 10.1007/s10562-009-0113-x10.1007/s10562-009-0113-x ↗
23. 10.1179/1743278210Y.000000000210.1179/1743278210Y.0000000002 ↗
24. 10.1149/1.277208510.1149/1.2772085 ↗
25. Macdonald D. D. Sharifi-Asl S. , Is Copper Immune to Corrosion When in Contact with Water and Aqueous Solutions, Technical Report TR-01-23, Swedish Radiation Safety Authority, Swedish Nuclear Fuel and Waste Management Co Box 5864 SE-102 40 Stockholm Sweden (2011).
26. King F. Ahonen L. Taxen C. Vuorinen U. Werme L. , Copper corrosion under expected conditions in a deep geologic repository, Technical Report TR-01-23, Swedish Nuclear Fueland Waste Management Co, Swedish Nuclear Fuel and Waste Management Co, Box 5864, SE-102 40 Stockholm Sweden (2001).
27. Hultquist G. Szakálos P. S. I. Graham M. J. KingSproule G. I. Wikmark G. , “Detection of Hydrogen in Corrosion of Copper in Pure Water,” in Proceedings of the 2008 International Corrosion Congress, Paper 3884 (2008) 1–9.
28. 10.1016/j.corsci.2010.05.00310.1016/j.corsci.2010.05.003 ↗
29. 10.1557/PROC-807-45910.1557/PROC-807-459 ↗
30. 10.1149/2.143306jes10.1149/2.143306jes ↗
31. Dortwegt R. Maughan E. , “The Chemistry of Copper in Water and Related Studies Planned at the Advanced Photon Source,” in Proceedings of the Particle Accelerator Conference, PAC 2001, volume 2 (IEEE, 2001) 1456–1458.10.1109/PAC.2001.986712 ↗
32. Dortwegt R. Putnam C. Swetin E. , “Mitigation of Copper Corrosion and Agglomeration in APS Process Water Systems,” in 2nd Intl Workshop on Mechanical Engineering Design of Synchrotron Radiation Equipment and Instrumentation (MEDSI2002) (2002) 462–468.
33. 10.1016/j.fusengdes.2013.04.01010.1016/j.fusengdes.2013.04.010 ↗
34. 10.1149/1.242400310.1149/1.2424003 ↗
35. 10.1016/S0098-3004(97)00038-110.1016/S0098-3004(97)00038-1 ↗
36. 10.5006/1.328043210.5006/1.3280432 ↗
37. 10.1149/1.183803610.1149/1.1838036 ↗
38. 10.1021/ac051034y10.1021/ac051034y ↗
39. 10.1016/0013-4686(96)00066-710.1016/0013-4686(96)00066-7 ↗
40. 10.1149/1.242849610.1149/1.2428496 ↗
41. 10.1149/1.206952210.1149/1.2069522 ↗
42. 10.4028/www.scientific.net/MSF.289-292.81310.4028/www.scientific.net/MSF.289-292.813 ↗
43. 10.1016/S0022-0728(84)80324-110.1016/S0022-0728(84)80324-1 ↗
44. 10.1149/1.239888910.1149/1.2398889 ↗
45. 10.1016/j.electacta.2009.10.06510.1016/j.electacta.2009.10.065 ↗
46. 10.1149/1.349956410.1149/1.3499564 ↗
47. 10.1149/1.349956510.1149/1.3499565 ↗
48. 10.1149/2.033306jes10.1149/2.033306jes ↗
49. Haynes W. M. Bruno T. J. Lide D. R. , editors, CRC Handbook of Chemistry and Physics, 94th edition (CRC Press, 2014).10.1201/b17118 ↗
50. 10.1007/s10008-008-0650-z10.1007/s10008-008-0650-z ↗