Effect of High Temperature Circumstance on Lithium-Ion Battery and the Application of Phase Change Material
Source abstract
Abstract
As known, it is common for lithium ion battery (LIB) to be used under extreme circumstances, among the high temperature circumstance is included. Herein, a series of experiments were conducted at elevated temperatures of 50, 60, and 70°C to examine the performance of LIB. Besides, the application of phase change material (PCM) under such condition was also investigated. Based on the experimental results, it is found that ambient temperature has a remarkable impact on the heat generation of battery, which decreases with the increasing ambient temperature. In addition, it is revealed that the inconsistency among batteries will deteriorate under high temperature circumstance by aggravating the differences of temperature and voltage. Moreover, the capacity decay rate of battery is demonstrated to be accelerated greatly by high temperature. After employing PCM into high temperature circumstance, it is presented that battery exhibits better performance including more stable temperature variation, better discharging performance and slower decay rate. And the performance of PCM is related to its thickness.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Advanced Battery Technologies Research · Advancements in Battery Materials · Advanced Battery Materials and Technologies
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (33)
Show source-provided references
1. 10.1016/j.enconman.2016.09.08110.1016/j.enconman.2016.09.081 ↗
2. 10.1016/j.enconman.2017.02.02210.1016/j.enconman.2017.02.022 ↗
3. 10.1016/j.jpowsour.2006.03.04310.1016/j.jpowsour.2006.03.043 ↗
4. 10.1149/2.F03122if10.1149/2.F03122if ↗
5. 10.1007/s10008-007-0449-310.1007/s10008-007-0449-3 ↗
6. Omenya F. Chernova N. A. Zhou H. “Comparative Study Nickel Rich Layered Oxides: NMC 622, NMC 811 and NCA Cathode Materials for Lithium Ion Battery [C]. Meeting Abstracts.” The Electrochemical Society, (3), 531 (2018).10.1149/MA2018-01/3/531 ↗
7. 10.1016/j.electacta.2012.05.03510.1016/j.electacta.2012.05.035 ↗
8. 10.1016/j.jpowsour.2012.10.06010.1016/j.jpowsour.2012.10.060 ↗
9. 10.1016/j.mattod.2014.10.04010.1016/j.mattod.2014.10.040 ↗
10. 10.1002/aenm.20110022310.1002/aenm.201100223 ↗
11. 10.1007/s11581-009-0373-x10.1007/s11581-009-0373-x ↗
12. 10.1016/j.jpowsour.2018.04.03610.1016/j.jpowsour.2018.04.036 ↗
13. 10.1016/j.jpowsour.2016.07.03910.1016/j.jpowsour.2016.07.039 ↗
14. 10.1016/j.jallcom.2012.07.07410.1016/j.jallcom.2012.07.074 ↗
15. 10.1016/j.jpowsour.2014.01.00510.1016/j.jpowsour.2014.01.005 ↗
16. 10.1016/j.ijheatmasstransfer.2016.09.00510.1016/j.ijheatmasstransfer.2016.09.005 ↗
17. 10.1016/j.apenergy.2016.05.12210.1016/j.apenergy.2016.05.122 ↗
18. 10.1016/j.enconman.2014.10.01510.1016/j.enconman.2014.10.015 ↗
19. 10.1016/j.applthermaleng.2017.12.13110.1016/j.applthermaleng.2017.12.131 ↗
20. 10.1016/j.applthermaleng.2015.04.01210.1016/j.applthermaleng.2015.04.012 ↗
21. 10.1039/C7RA03963H10.1039/C7RA03963H ↗
22. 10.1016/j.jpowsour.2017.07.06710.1016/j.jpowsour.2017.07.067 ↗
23. 10.1149/1.139388810.1149/1.1393888 ↗
24. 10.1016/j.enconman.2016.09.05810.1016/j.enconman.2016.09.058 ↗
25. 10.1016/j.applthermaleng.2017.12.12110.1016/j.applthermaleng.2017.12.121 ↗
26. 10.1016/j.applthermaleng.2017.12.05510.1016/j.applthermaleng.2017.12.055 ↗
27. 10.1016/j.energy.2013.09.02810.1016/j.energy.2013.09.028 ↗
28. 10.1016/j.jpowsour.2012.10.06010.1016/j.jpowsour.2012.10.060 ↗
29. 10.1016/j.jpowsour.2008.04.05010.1016/j.jpowsour.2008.04.050 ↗
30. 10.1016/j.ijheatmasstransfer.2018.02.03810.1016/j.ijheatmasstransfer.2018.02.038 ↗
31. 10.1016/j.electacta.2015.08.05610.1016/j.electacta.2015.08.056 ↗
32. 10.1016/j.jpowsour.2014.03.11210.1016/j.jpowsour.2014.03.112 ↗
33. 10.1016/j.enbuild.2006.02.00910.1016/j.enbuild.2006.02.009 ↗