Accelerated Degradation of Polymer Electrolyte Membrane Fuel Cell Gas Diffusion Layers
Source abstract
Abstract
In this work, an ex situ accelerated carbon-corrosion-based ageing methodology is presented for stand-alone gas diffusion layers (GDLs). Pristine GDLs were subjected to carbon corrosion (degradation) via submersion in a hydrogen peroxide (H 2 O 2 ) solution. The microporous layer (MPL) experiences up to nine times the loss in carbon mass compared to the carbon fiber substrate. The hydrophobicity of the GDL is also degraded as evidenced by a reduction in the surface contact angle, and this loss of hydrophobicity is associated with surface corrosion and polytetrafluoroethylene (PTFE) degradation. Performance testing reveals increases in mass transport losses for aged GDLs, which is a phenomenon that is attributed to the reduction in GDL hydrophobicity.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Fuel Cells and Related Materials · Electrocatalysts for Energy Conversion · Advanced Battery Technologies Research
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (70)
Show source-provided references
1. 10.1016/j.jpowsour.2005.07.09210.1016/j.jpowsour.2005.07.092 ↗
2. 10.1002/eej.2089910.1002/eej.20899 ↗
3. 10.1149/1.345474010.1149/1.3454740 ↗
4. St-Pierre · Journal of New Materials for Electrochemical Systems · 2000 · 3 · 2
5. 10.1016/j.pecs.2010.06.00310.1016/j.pecs.2010.06.003 ↗
6. 10.1021/cr050182l10.1021/cr050182l ↗
7. 10.1016/j.jpowsour.2015.06.04710.1016/j.jpowsour.2015.06.047 ↗
8. 10.1016/j.ijhydene.2011.01.01410.1016/j.ijhydene.2011.01.014 ↗
9. 10.1016/j.apcatb.2013.03.02110.1016/j.apcatb.2013.03.021 ↗
10. 10.1016/j.ijhydene.2009.06.03610.1016/j.ijhydene.2009.06.036 ↗
11. 10.1016/j.jpowsour.2007.02.02810.1016/j.jpowsour.2007.02.028 ↗
12. 10.1016/j.jpowsour.2005.02.05810.1016/j.jpowsour.2005.02.058 ↗
13. 10.1149/1.218618410.1149/1.2186184 ↗
14. 10.1016/j.electacta.2009.02.02110.1016/j.electacta.2009.02.021 ↗
15. 10.1016/j.jpowsour.2009.04.00510.1016/j.jpowsour.2009.04.005 ↗
16. 10.1016/j.elecom.2008.12.05310.1016/j.elecom.2008.12.053 ↗
17. 10.1149/1.239872810.1149/1.2398728 ↗
18. 10.1016/j.jpowsour.2012.11.00610.1016/j.jpowsour.2012.11.006 ↗
19. 10.1016/j.jpowsour.2013.03.16510.1016/j.jpowsour.2013.03.165 ↗
20. 10.1016/j.ijhydene.2009.09.01710.1016/j.ijhydene.2009.09.017 ↗
21. 10.3390/en2040105710.3390/en20401057 ↗
22. 10.1021/cr020718s10.1021/cr020718s ↗
23. 10.1016/j.jpowsour.2006.03.01610.1016/j.jpowsour.2006.03.016 ↗
24. 10.1039/b703485g10.1039/b703485g ↗
25. 10.1016/0021-9797(83)90396-X10.1016/0021-9797(83)90396-X ↗
26. 10.1021/j150474a01510.1021/j150474a015 ↗
27. 10.1039/tf944400054610.1039/tf9444000546 ↗
28. 10.1016/j.jpowsour.2015.03.13210.1016/j.jpowsour.2015.03.132 ↗
29. 10.1016/j.ijhydene.2011.06.09810.1016/j.ijhydene.2011.06.098 ↗
30. 10.1016/j.apenergy.2011.07.01110.1016/j.apenergy.2011.07.011 ↗
31. 10.1149/05801.0919ecst10.1149/05801.0919ecst ↗
32. 10.1002/fuce.20100017210.1002/fuce.201000172 ↗
33. 10.1016/j.jpowsour.2009.10.02210.1016/j.jpowsour.2009.10.022 ↗
34. 10.1016/j.electacta.2009.04.07310.1016/j.electacta.2009.04.073 ↗
35. 10.1016/j.jpowsour.2010.10.02810.1016/j.jpowsour.2010.10.028 ↗
36. 10.1149/1.348460110.1149/1.3484601 ↗
37. 10.1016/j.jpowsour.2008.01.07010.1016/j.jpowsour.2008.01.070 ↗
38. 10.1016/j.jpowsour.2016.10.03710.1016/j.jpowsour.2016.10.037 ↗
39. 10.1016/j.apenergy.2015.06.06810.1016/j.apenergy.2015.06.068 ↗
40. Pourbaix M. , (1974).
41. 10.1149/1.363560810.1149/1.3635608 ↗
42. 10.1016/j.enconman.2013.07.03410.1016/j.enconman.2013.07.034 ↗
43. 10.1016/j.ijhydene.2011.02.06010.1016/j.ijhydene.2011.02.060 ↗
44. 10.1149/2.004402eel10.1149/2.004402eel ↗
45. 10.1149/2.jes03420510.1149/2.jes034205 ↗
46. 10.1016/j.jpowsour.2015.10.00410.1016/j.jpowsour.2015.10.004 ↗
47. 10.1149/1.307757310.1149/1.3077573 ↗
48. 10.1149/2.0031409jes10.1149/2.0031409jes ↗
49. 10.1149/1.218618410.1149/1.2186184 ↗
50. 10.1149/1.280075210.1149/1.2800752 ↗
51. 10.1149/1.278102510.1149/1.2781025 ↗
52. 10.1016/j.electacta.2009.02.02110.1016/j.electacta.2009.02.021 ↗
53. 10.1149/1.190498810.1149/1.1904988 ↗
54. 10.1016/j.energy.2016.10.06110.1016/j.energy.2016.10.061 ↗
55. Frisk J. Hicks M. Atanasoski R. Boand W. Schmoeckel A. Kurkowski M. , MEA component durability, (2004).
56. 10.1016/j.ijhydene.2016.06.14710.1016/j.ijhydene.2016.06.147 ↗
57. 10.1149/2.0081707jes10.1149/2.0081707jes ↗
58. 10.1149/2.0081707jes10.1149/2.0081707jes ↗
59. 10.1016/j.ijhydene.2015.10.00810.1016/j.ijhydene.2015.10.008 ↗
60. 10.1016/j.electacta.2015.11.11510.1016/j.electacta.2015.11.115 ↗
61. 10.1149/2.0991702jes10.1149/2.0991702jes ↗
62. 10.1107/S160057751502389910.1107/S1600577515023899 ↗
63. 10.1016/j.ijheatmasstransfer.2016.11.04510.1016/j.ijheatmasstransfer.2016.11.045 ↗
64. 10.1149/2.054212jes10.1149/2.054212jes ↗
65. 10.1149/2.0391508jes10.1149/2.0391508jes ↗
66. Barbir F. , PEM fuel cells, Springer (2006).10.1007/1-84628-207-1_2 ↗
67. O'Hayre R. P. Cha S. Colella W. Prinz F. B. , Fuel cell fundamentals, John Wiley & Sons New York (2006).
68. 10.1149/1.204398810.1149/1.2043988 ↗
69. 10.1021/la025769z10.1021/la025769z ↗
70. 10.1149/2.0531608jes10.1149/2.0531608jes ↗