Titanium alloys (ASTM Grades 1, 2, 7, 12, and 18) are employed as the liner and internal components of autoclaves during the high-pressure acid leaching (HPAL) of nickel laterite ores. This paper summarizes the corrosion behavior of these alloys in sulfuric acid and the effect of the addition of chlorides (NaCl). New thermodynamic –pH diagrams for the , , and systems are presented. Micrographs are also presented and the corrosion morphology is discussed. Long-term immersion tests were carried out to determine corrosion rates. Electrochemical techniques were used to provide insight into the corrosion chemistry. The shortcomings of accelerated corrosion testing of Ti alloys are addressed. Pd enrichment on the surface of Ti-18 was confirmed by a combination of open-circuit potential measurements and chronoamperometric measurements.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Corrosion Behavior and Inhibition · Hydrogen embrittlement and corrosion behaviors in metals · Metal Extraction and Bioleaching

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References

Reference metadata was not supplied for this record.