Plate-Shaped Graphite for Improved Performance of Flow-Electrode Capacitive Deionization

SeungCheol Yang, Hong-ran Park, Jungjoon Yoo, Hanki Kim, Jiyeon Choi, Moon Hee Han, Dong Kook Kim

Publisher page

Abstract

Capacitive deionization (CDI) using a flow-electrode primarily composed of porous materials and an aqueous electrolyte, exhibits continuous deionization and a high desalting efficiency. The development of flow-electrodes with high capacitance and low resistance is essential for achieving an efficient flow-electrode capacitive deionization (FCDI) system with low energy consumption. For this purpose, studies on conductive additives (CAs) that do not clog the flow-channel must be conducted. Here, we evaluated the desalting performance of flow-electrodes with spherical and plate-type conductive additives having sizes between 1 and 10 μm and possessing powder conductivities similar to or higher than nano-sized carbon black, which is often used as the CA in solid fixed electrodes in conventional CDI systems. We confirmed that plate-shaped CAs reduced resistance near the pores and enhanced the desalting performance of the flow-electrodes in FCDI systems. The positive effect of such plate-shaped CAs appears to originate from efficient charge percolation between the ACs via the electrical conductive direction of the graphite and the alignment of the exposed graphite edges to the pumping direction of the flow-electrode. Finally, we verified that the flow-electrode with the newly discovered micro-sized CA could be operated without clogging the flow-channel in FCDI and showed an improved desalting performance of around 1.5 times compared the flow-electrode without the micro-sized CA for extended periods of time.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Membrane-based Ion Separation Techniques · Advanced Battery Materials and Technologies · Advanced battery technologies research

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (50)

Show source-provided references
1. 10.1039/C5EE00519A10.1039/C5EE00519A ↗
2. 10.1016/j.pmatsci.2013.03.00510.1016/j.pmatsci.2013.03.005 ↗
3. 10.1016/j.desal.2007.07.01410.1016/j.desal.2007.07.014 ↗
4. 10.1016/j.desal.2006.04.05110.1016/j.desal.2006.04.051 ↗
5. 10.1021/es201551e10.1021/es201551e ↗
6. 10.1016/j.watres.2008.01.01110.1016/j.watres.2008.01.011 ↗
7. 10.1021/am201683j10.1021/am201683j ↗
8. 10.1039/c1jm13105b10.1039/c1jm13105b ↗
9. 10.1039/C7TA02653F10.1039/C7TA02653F ↗
10. 10.1039/c2jm35340g10.1039/c2jm35340g ↗
11. 10.1016/j.desal.2010.10.02010.1016/j.desal.2010.10.020 ↗
12. 10.1039/c3ee24443a10.1039/c3ee24443a ↗
13. 10.1016/j.elecom.2014.03.00310.1016/j.elecom.2014.03.003 ↗
14. 10.1016/j.desal.2017.05.02310.1016/j.desal.2017.05.023 ↗
15. 10.1007/s10800-017-1046-510.1007/s10800-017-1046-5 ↗
16. 10.1021/acssuschemeng.6b0121210.1021/acssuschemeng.6b01212 ↗
17. 10.1021/acs.est.5b0464010.1021/acs.est.5b04640 ↗
18. 10.1039/C6RA02480G10.1039/C6RA02480G ↗
19. 10.1021/acs.est.6b0342410.1021/acs.est.6b03424 ↗
20. 10.1021/es505598910.1021/es5055989 ↗
21. 10.1039/C5CS00279F10.1039/C5CS00279F ↗
22. 10.1016/j.elecom.2017.01.00810.1016/j.elecom.2017.01.008 ↗
23. 10.1016/j.desal.2017.09.03210.1016/j.desal.2017.09.032 ↗
24. 10.1016/j.elecom.2015.07.01810.1016/j.elecom.2015.07.018 ↗
25. 10.1016/j.elecom.2014.06.00410.1016/j.elecom.2014.06.004 ↗
26. 10.1039/c4ta01783h10.1039/c4ta01783h ↗
27. 10.1039/C5TA10316A10.1039/C5TA10316A ↗
28. 10.1039/c4ta00377b10.1039/c4ta00377b ↗
29. 10.1021/acssuschemeng.6b0068910.1021/acssuschemeng.6b00689 ↗
30. 10.1021/ez500331410.1021/ez5003314 ↗
31. Mise N. Yamada M. Hirasa T. , Carbon black, process for producing the same, and aqueous dispersion and water-base ink both containing the same, US Patent 6123759, wo1998030638
32. 10.1016/j.colsurfa.2004.12.00210.1016/j.colsurfa.2004.12.002 ↗
33. 10.1016/j.colsurfa.2009.03.03910.1016/j.colsurfa.2009.03.039 ↗
34. Shaw D. J. , “Colloid Stability,” Chapter 8 in Introduction to Colloid and Surface Chemistry, 4th edition, edited by Shaw D. J. , Butterworth-Heinemann (1992).10.1016/B978-0-08-050910-5.50012-8 ↗
35. 10.1016/j.colsurfa.2015.08.04110.1016/j.colsurfa.2015.08.041 ↗
36. Http://www.carbon.co.jp/english/products/others/, last accessed oct 13, 2017.
37. Http://sec-carbon.com/eng/fine_powder.html, last accessed oct 13, 2017.
38. 10.1002/app.2584210.1002/app.25842 ↗
39. 10.1016/j.compositesb.2013.04.06910.1016/j.compositesb.2013.04.069 ↗
40. 10.1021/am501650q10.1021/am501650q ↗
41. 10.1039/C6RA13686A10.1039/C6RA13686A ↗
42. 10.1002/cssc.20140349010.1002/cssc.201403490 ↗
43. 10.1016/j.jpowsour.2013.08.10110.1016/j.jpowsour.2013.08.101 ↗
44. 10.1016/j.carbon.2014.05.01710.1016/j.carbon.2014.05.017 ↗
45. 10.1016/j.carbon.2015.04.02010.1016/j.carbon.2015.04.020 ↗
46. 10.1002/ente.20150024310.1002/ente.201500243 ↗
47. Callister W. D. , “Structures and Properties of Ceramics,” Chapter 13 in Material Science and Engineering: an Introduction, 5th edition, edited by Callister W. D. , John Wiley & Sons, Inc. (2000).
48. 10.1149/1.240815110.1149/1.2408151 ↗
49. Pierson H. O. , “Graphite Structure and Properties,” Chapter 3 in Handbook of Carbon, Graphite, Diamonds and Fullerenes: Processing, Properties and Applications, 1st edition, edited by Pierson H. O. , William Andrew (1994).
50. 10.1021/la103537y10.1021/la103537y ↗