Laser Sintering of Printed Anodes for Al-Air Batteries
Source abstract
Abstract
We report on a 3D printed Al anode for Al-air battery combined with laser sintering method. We verified that laser sintering contributed to effective removal of the organic solvent in the slurry and increased the conductivity of the printed anode. By application of infrared laser sintering, we significantly improved electrical contacts of Al nanoparticles and electrochemical performance of Al-air cells. A Pt/C coated hydrophobic carbon paper was used for air cathode to provide a good electrical contact, an oxygen flow ability, and the water sealing. Gel-style KOH was introduced as the electrolyte and waterways also utilized in the chemical reaction. The laser sintered Al-air battery could provide 239 mAh/g discharge capacity and a 0.95 V operation voltage. Also, a 3D structured anode was fabricated by 3D printing the active material on current collectors to achieve a high mass-loading with active material thickness of 360 μm, 560 μm and 680 μm for 1, 2 and 3 layers 3D printed electrodes. The battery cells provide areal discharge capacities of 1.5 mAh/cm 2 , 2.8mAh/cm 2 , and 3.23 mAh/cm 2 , respectively for 1, 2 and 3 layers-electrodes.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Advanced Battery Materials and Technologies · Supercapacitor Materials and Fabrication · Advancements in Battery Materials
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (49)
Show source-provided references
1. 10.1016/j.rser.2007.01.02310.1016/j.rser.2007.01.023 ↗
2. 10.1002/aenm.20120002610.1002/aenm.201200026 ↗
3. 10.1016/j.pnsc.2008.07.01410.1016/j.pnsc.2008.07.014 ↗
4. 10.1039/c0ee00777c10.1039/c0ee00777c ↗
5. 10.1002/cplu.20140223810.1002/cplu.201402238 ↗
6. 10.1039/C4CP02533D10.1039/C4CP02533D ↗
7. Linden D. , Handbook of batteries and fuel cells, New York, McGraw-Hill Book Co., 1984, 1075 p. No individual items are abstracted in this volume., 1984.
8. 10.1016/S0378-7753(02)00370-110.1016/S0378-7753(02)00370-1 ↗
9. 10.1016/j.jpowsour.2007.11.10810.1016/j.jpowsour.2007.11.108 ↗
10. Mori R. , Suppression of by-product accumulation in rechargeable aluminum–air batteries using non-oxide ceramic materials as air cathode materials., Sustainable Energy & Fuels, 2017.10.1039/C7SE00087A ↗
11. 10.1016/j.jpowsour.2013.01.14110.1016/j.jpowsour.2013.01.141 ↗
12. 10.1016/S0378-7753(01)01014-X10.1016/S0378-7753(01)01014-X ↗
13. 10.1016/j.jpowsour.2005.11.09710.1016/j.jpowsour.2005.11.097 ↗
14. 10.1016/j.matchemphys.2010.02.00610.1016/j.matchemphys.2010.02.006 ↗
15. 10.1016/j.jiec.2015.08.00410.1016/j.jiec.2015.08.004 ↗
16. 10.1016/0022-0728(90)85094-L10.1016/0022-0728(90)85094-L ↗
17. 10.1016/0013-4686(90)87074-C10.1016/0013-4686(90)87074-C ↗
18. 10.1016/S0008-6223(97)00173-510.1016/S0008-6223(97)00173-5 ↗
19. 10.1016/j.jpowsour.2007.07.04910.1016/j.jpowsour.2007.07.049 ↗
20. 10.1149/2.062310jes10.1149/2.062310jes ↗
21. 10.1016/j.solmat.2008.10.00410.1016/j.solmat.2008.10.004 ↗
22. 10.1063/1.282439210.1063/1.2824392 ↗
23. 10.1088/0022-3727/47/2/02550110.1088/0022-3727/47/2/025501 ↗
24. 10.1016/j.actamat.2007.07.04010.1016/j.actamat.2007.07.040 ↗
25. 10.1063/1.350260410.1063/1.3502604 ↗
26. 10.1149/2.0161504jss10.1149/2.0161504jss ↗
27. 10.1039/C5NR00312A10.1039/C5NR00312A ↗
28. 10.1039/b823329b10.1039/b823329b ↗
29. 10.1088/0957-4484/19/17/17520110.1088/0957-4484/19/17/175201 ↗
30. 10.1016/j.tsf.2014.02.00110.1016/j.tsf.2014.02.001 ↗
31. 10.1016/j.tsf.2006.11.14110.1016/j.tsf.2006.11.141 ↗
32. 10.1007/s11664-008-0591-410.1007/s11664-008-0591-4 ↗
33. 10.1016/j.matlet.2009.09.04710.1016/j.matlet.2009.09.047 ↗
34. 10.1016/j.jpowsour.2009.02.08210.1016/j.jpowsour.2009.02.082 ↗
35. Giancoli D. C. , Physics: principles with applications, 4th Edition. 1995: Pearson/Prentice Hall.
36. 10.1016/j.jcrysgro.2005.02.01910.1016/j.jcrysgro.2005.02.019 ↗
37. 10.1016/S0927-7757(97)00004-610.1016/S0927-7757(97)00004-6 ↗
38. The Influence of Metal-Ion Inclusion on the Morphology of Gibbsite
39. 10.1016/S0892-6875(96)00133-110.1016/S0892-6875(96)00133-1 ↗
40. 10.1016/0013-4686(89)87025-210.1016/0013-4686(89)87025-2 ↗
41. 10.1016/0368-2048(90)80004-T10.1016/0368-2048(90)80004-T ↗
42. 10.1149/1.208656610.1149/1.2086566 ↗
43. Particle Size Effects of Pt Nanocatalyst in the Catalyst Layer of Proton Exchange Membrane Fuel Cell
44. 10.1038/451652a10.1038/451652a ↗
45. 10.1016/S0378-7753(98)00242-010.1016/S0378-7753(98)00242-0 ↗
46. 10.1149/1.296942410.1149/1.2969424 ↗
47. 10.1002/ese3.4710.1002/ese3.47 ↗
48. Elango R. , Thick Binder‐Free Electrodes for Li–Ion Battery Fabricated Using Templating Approach and Spark Plasma Sintering Reveals High Areal Capacity., Advanced Energy Materials, 2018.10.1002/aenm.201703031 ↗
49. 10.1002/aenm.20110026110.1002/aenm.201100261 ↗