Surface Area Loss of Platinum Supported on Carbon in Phosphoric Acid Electrolyte
Source abstract
Abstract
An experimental study was conducted to determine the surface area loss of platinum supported on carbon in a 191°C phosphoric acid fuel cell environment and to define the mechanism for this process. The surface area was found to decline rapidly initially, but remains above 20 m 2 /g for 20,000 hr, the longest time period investigated. A study of the effect of operating potential, transmission electron microscope studies of electrodes, and Pt deposited on a carbon film, and the results of other previous studies indicate that crystallite migration and coalescence are the major mode by which Pt surface area is lost in this situation.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Fuel Cells and Related Materials · Electrocatalysts for Energy Conversion · Conducting polymers and applications
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
United Technologies Corporation, Power Systems Division, South Windsor, Connecticut 06074