Cycling Aging in Different State of Charge Windows in Lithium-Ion Batteries with Silicon-Dominant Anodes
Source abstract
Abstract
Reducing the capacity utilization of silicon-containing anodes and choosing the optimal full-cell voltage window improve the lifetime significantly. In this study, we investigate how different voltage windows affect the aging modes with a common 50% cycling depth. First, the cyclic stability, the anode potentials, and the polarization increase are analyzed for the different voltage windows using 70 wt% microscale silicon anodes and NCA cathodes with a lithium metal reference electrode to investigate the electrode-specific characteristics. Further, the underlying aging modes are quantified in the post-mortem analysis. Finally, the anode thickness increase is quantified using a dilatometer setup for different anode lithiations. In contrast to the literature, the highest voltage window is most beneficial for the lifetime since high anode delithiation potentials and high surface increases are avoided. The anode potential at the end-of-discharge, the charge-averaged full-cell potentials, and the resistance increase are a function of the state of health (SoH). The common underlying main aging mechanism is the loss of lithium inventory, followed by the loss of anode active material. In contrast, the loss of cathode active materials only plays a minor role.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Advancements in Battery Materials · Advanced Battery Technologies Research · Advanced Battery Materials and Technologies
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (41)
Show source-provided references
1. A wide range of testing results on an excellent lithium-ion cell chemistry to be used as benchmarks for new battery technologies10.1149/2.0981913jes ↗
2. Ageing of high energy density automotive li-ion batteries: The effect of temperature and state-of-charge10.1149/1945-7111/aceb8f ↗
3. Influence of state of charge window on the degradation of tesla lithium-ion battery cells10.1016/j.est.2023.110001 ↗
4. Comprehensive analysis of the aging behavior of nickel-rich, silicon-graphite lithium-ion cells subject to varying temperature and charging profiles10.1149/1945-7111/ac03f6 ↗
5. Degradation of commercial lithium-ion cells as a function of chemistry and cycling conditions10.1149/1945-7111/abae37 ↗
6. How the utilised soc window in commercial li-ion pouch cells influence battery ageing10.1016/j.powera.2021.100054 ↗
7. How do depth of discharge, c-rate and calendar age affect capacity retention, impedance growth, the electrodes, and the electrolyte in li-ion cells?10.1149/1945-7111/ac4b82 ↗
8. Lithium-ion battery degradation: Measuring rapid loss of active silicon in silicon-graphite composite electrodes10.1021/acsaem.2c02047 ↗
9. Influence of charging protocols on the charging capability and aging of lithium-ion cells with silicon-containing anodes10.1016/j.est.2022.104044 ↗
10. Silicon-dominant anodes based on microscale silicon particles under partial lithiation with high capacity and cycle stability10.1149/2.1311915jes ↗
11. Revealing the failure mechanism of partially lithiated silicon-dominant anodes based on microscale silicon particles10.1149/1945-7111/ac1491 ↗
12. Effect and progress of the amorphization process for microscale silicon particles under partial lithiation as active material in lithium-ion batteries10.1149/1945-7111/ac4b80 ↗
13. Comparison of silicon and graphite anodes: Temperature-dependence of impedance characteristics and rate performance10.1149/1945-7111/acc09d ↗
14. Modeling and simulation of inhomogeneities in a 18650 nickel-rich, silicon-graphite lithium-ion cell during fast charging10.1016/j.jpowsour.2018.11.043 ↗
15. State of health estimation for lithium-ion batteries
16. Effects of mechanical compression on the aging and the expansion behavior of si/c-composite∣nmc811 in different lithium-ion battery cell formats10.1149/2.1121915jes ↗
17. Morphological changes of silicon nanoparticles and the influence of cutoff potentials in silicon-graphite electrodes10.1149/2.1261807jes ↗
18. Partial lithiation strategies for suppressing degradation of silicon composite electrodes10.1016/j.electacta.2018.11.009 ↗
19. Improving cycle life of silicon-dominant anodes based on microscale silicon particles under partial lithiation10.3390/batteries9010058 ↗
20. A stress-based charging protocol for silicon anode in lithium-ion battery: Theoretical and experimental studies10.1016/j.est.2020.101765 ↗
21. Electrochemically stable in situ dilatometry of nmc, nca and graphite electrodes for lithium-ion cells compared to xrd measurements10.1149/1945-7111/abf262 ↗
22. The role of silicon in silicon-graphite composite electrodes regarding specific capacity, cycle stability, and expansion10.1149/1945-7111/ac4545 ↗
23. Effect of mechanical pressure on lifetime, expansion, and porosity of silicon-dominant anodes in laboratory lithium-ion cells10.1149/1945-7111/ad36e6 ↗
24. Effect of mechanical pressure on rate capability, lifetime, and expansion in multilayer pouch cells with silicon-dominant anodes10.1149/1945-7111/ad71f6 ↗
25. Comparative evaluation of lMR-NCM and NCA cathode active materials in multilayer lithium-ion pouch cells: Part I. Production, electrode characterization, and formation10.1149/1945-7111/abe50c ↗
26. State of health estimation for li-ion battery using characteristic voltage intervals and genetic algorithm optimized back propagation neural network10.1016/j.est.2022.106277 ↗
27. Deconvolution of an SoC- and SoH-dependent contact resistance in a multilayer pouch cell using impedance spectroscopy - manuscript in preparation
28. The implications of particle morphology on the capacity retention, side reactions, and impedance build-up of nickel-rich ncms upon cycling in full-cells: Poly- vs. single-crystalline NCM85100510.1149/1945-7111/acf3a1 ↗
29. Oxygen release and its effect on the cycling stability of LiNixMnyCozO2 (NMC) cathode materials for li-ion batteries10.1149/2.0021707jes ↗
30. Cycling behavior of NCM523/graphite lithium-ion cells in the 3-4.4 V range: Diagnostic studies of full cells and harvested electrodes10.1149/2.0081701jes ↗
31. Degradation diagnostics for lithium ion cells10.1016/j.jpowsour.2016.12.011 ↗
32. Modeling volume change due to intercalation into porous electrodes10.1149/2.030408jes ↗
33. Reaction of li with alloy thin films studied by in situ AFM10.1149/1.1613668 ↗
34. Review–“Knees” in lithium-ion battery aging trajectories10.1149/1945-7111/ac6d13 ↗
35. Electrolyte and sei decomposition reactions of transition metal ions investigated by on-line electrochemical mass spectrometry10.1149/2.0511814jes ↗
36. Electrochemical impedance spectroscopy characterization of silicon-based electrodes for li-ion batteries10.1007/s12678-019-00573-y ↗
37. Understanding anomalous behavior in coulombic efficiency measurements on Li-ion batteries10.1149/2.0191503jes ↗
38. Between scylla and charybdis: Balancing among structural stability and energy density of layered NCM cathode materials for advanced lithium-ion batteries10.1021/acs.jpcc.7b06363 ↗
39. Elucidating the implications of morphology on fundamental characteristics of nickel-rich ncms: Cracking, gassing, rate capability, and thermal stability of poly- and single-crystalline NCM62210.1149/1945-7111/ac5f7f ↗
40. Electrochemical dilatometry of si-bearing electrodes: Dimensional changes and experiment design10.1149/1945-7111/abd465 ↗
41. Mitutoyo