Review—Corrosion-Resistant Metastable Al Alloys: An Overview of Corrosion Mechanisms

J. Esquivel, R. K. Gupta

Abstract

Commercial aluminum alloys exhibit localized corrosion when exposed to environments containing aggressive anions. Alloying of Al with specific elements (M: Cr, Mo, V, Nb, etc) using non-equilibrium processing techniques has been reported to result in significantly improved corrosion resistance due to the formation of a supersaturated solid solution and uniform distribution of M in the matrix. Several theories describing the corrosion behavior of Al–M alloys have been postulated. This paper presents an overview of the most common non-equilibrium alloying techniques implemented for the production of the metastable Al–M alloys and posited corrosion mechanisms for the improved corrosion resistance.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Corrosion Behavior and Inhibition · Aluminum Alloy Microstructure Properties · High-Temperature Coating Behaviors

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (100+)

Show source-provided references
1. Gupta · 2017
2. Thermal stability of high-energy ball milled Al alloys
3. Simultaneous improvement in the strength and corrosion resistance of Al via high-energy ball milling and Cr alloying10.1016/j.matdes.2015.06.120 ↗
4. Electrochemical Characteristics of Intermetallic Phases in Aluminum Alloys10.1149/1.1869984 ↗
5. Passivity breakdown, pit initiation and propagation of pits in metallic materials–review10.1016/j.corsci.2014.10.006 ↗
6. Pitting corrosion of metals a review of the critical factors10.1149/1.1838615 ↗
7. Corrosion of aluminum and aluminum alloys
8. Davis · 1999
9. Pourbaix · 1966
10. Polmear · 2005
11. Scamans · 2010
12. Influence of microalloying additions on Al–Mg alloy. Part 1: corrosion and electrochemical response10.1179/1743278213Y.0000000128 ↗
13. Microalloying of Sc, Ni, and Ce in an advanced Al–Zn–Mg—Cu alloy10.1007/s11661-999-0154-1 ↗
14. Influence of microalloying additions on Al–Mg alloy. Part 2: phase analysis and sensitisation behaviour10.1179/1743278213Y.0000000129 ↗
15. Effect of ion implantation on the corrosion behavior of iron, stainless steels, and aluminum—a review10.5006/1.3281675 ↗
16. Structure, composition and pitting behavior of sputtered Al, Al&. zbnd; Cr and Al&. zbnd; Ta films10.1016/0010-938X(93)90081-Q ↗
17. On the Pitting Resistance of Sputter-Deposited Aluminum Alloys10.1149/1.2220794 ↗
18. Davis · 1993
19. Corrosion behavior and hardness of Al–M (M: Mo, Si, Ti, Cr) alloys10.1007/s40195-017-0550-2 ↗
20. Ion beam assisted thin film deposition10.1016/0920-2307(91)90008-B ↗
21. The effect of molybdenum ion implantation on the general and pitting corrosion behaviour of pure aluminium and a high strength aluminium alloy10.1016/0010-938X(80)90116-X ↗
22. Surface analysis studies on the corrosion resistance of Mo implanted Al alloys10.1016/0378-5963(84)90038-2 ↗
23. Localized corrosion behavior of aluminum surface alloys produced by ion implantation and ion beam mixing10.1016/0921-5093(89)90125-1 ↗
24. Surface charge considerations in the pitting of ion-implanted aluminum10.1149/1.2095608 ↗
25. The corrosion behavior of Mo–Al, Cr–Al and Cr–Mo–Al surface alloys produced by ion beam mixing and ion implantation10.1016/0010-938X(91)90086-5 ↗
26. Anodic polarization behaviour of ion implanted aluminum in 3.5 wt% NaCl electrolyte10.1016/S0168-583X(87)80051-4 ↗
27. Novel corrosion resistant alloys by ion implantation10.1021/i360066a018 ↗
28. The effect of ion implantation on the corrosion behaviour of pure iron—I. Argonion implantation10.1016/0010-938X(76)90126-8 ↗
29. The effect of ion implantation on the corrosion behaviour of pure iron—II. Chromium ion implantation
30. The effect of ion implantation on the corrosion behaviour of pure iron-III. Tantalum ion implantation10.1016/S0010-938X(77)80010-3 ↗
31. The pitting corrosion behavior of aluminum ion implanted with tantalum10.1016/0168-583X(91)95716-Q ↗
32. A surface charge model of corrosion pit initiation and of protection by surface alloying10.1149/1.1392021 ↗
33. Magnetron sputtering: a review of recent developments and applications10.1016/S0042-207X(99)00189-X ↗
34. Massalski · Binary Alloy Phase Diagrams. Vol. I and II, Am. Soc. Met. · 1986 · 1986 · 2224
35. Influence of Molybdenum on the pitting corrosion of aluminum films10.1149/1.2108709 ↗
36. Moshier · Corrosion Behavior of Aluminum-Molybdenum Alloys in Chloride Solutions · 1986 · 134 · 2677
37. Pitting of sputtered aluminum alloy thin films10.1149/1.2096864 ↗
38. Evolution of the chemistry of passive films of sputter-deposited, supersaturated Al alloys10.1149/1.2086456 ↗
39. The influence of tungsten alloying additions on the passivity of aluminum10.1149/1.2085404 ↗
40. Mechanisms of passivity of nonequilibrium Al–W alloys10.1149/1.2056234 ↗
41. Corrosion behavior of aluminum‐molybdenum alloys in chloride solutions10.1149/1.2100271 ↗
42. Passive film structure of supersaturated Al–Mo alloys10.1149/1.2085392 ↗
43. Surface chemistry of sputter-deposited Al–Mo and Al–Cr alloys polarized in 0.1 N KCl10.1149/1.2096635 ↗
44. Solute-vacancy interaction model and the effect of minor alloying elements on the initiation of pitting corrosion10.1149/1.2113886 ↗
45. Electrochemical behavior and surface chemistry of non-equilibrium aluminum–tantalum alloys: solute-rich interphase mechanisms10.1002/sia.740230906 ↗
46. An XPS study of the corrosion behavior of sputter-deposited amorphous Al–W alloys in 1 M HCl10.1016/0010-938X(91)90076-2 ↗
47. New frontiers in materials science opened by ionic liquids10.1002/adma.200902184 ↗
48. Electrochemistry of vanadium (II) and the electrodeposition of aluminum-vanadium alloys in the aluminum chloride-1-ethyl-3-methylimidazolium chloride molten salt10.2298/JMMB0302003T ↗
49. Electrodeposition of Al–Mo alloys from the Lewis acidic aluminum chloride-1-ethyl-3-methylimidazolium chloride molten salt10.1149/1.1704611 ↗
50. Electrodeposition of Al–Zr alloys from lewis acidic aluminum chloride-1-ethyl-3-methylimidazolium chloride melt10.1149/1.1753231 ↗
51. Pitting corrosion of electrodeposited aluminum-manganese alloys10.1149/1.2220910 ↗
52. Electrochemistry of titanium and the electrodeposition of Al–Ti alloys in the Lewis acidic aluminum chloride–1-ethyl-3-methylimidazolium chloride melt10.1149/1.1554915 ↗
53. Al–W alloy deposition from lewis acidic room-temperature chloroaluminate ionic liquid10.1149/05011.0239ecst ↗
54. Electroplating of Al–Nb alloys from the lewis acidic chloroaluminate ionic liquid
55. Dispersion strengthened superalloys by mechanical alloying10.1007/BF03037835 ↗
57. Dispersion strengthened aluminum made by mechanical alloying10.1007/BF02643845 ↗
58. Mechanical alloying and milling10.1016/S0079-6425(99)00010-9 ↗
59. Corrosion behaviour and hardness of in situ consolidated nanostructured Al and Al–Cr alloys produced via high-energy ball milling10.1016/j.corsci.2015.06.011 ↗
60. Excellent corrosion resistance and hardness in Al alloys by extended solid solubility and nanocrystalline structure10.1080/21663831.2017.1396262 ↗
61. Effect of chloride ion on the localized breakdown of nickel oxide films10.1149/1.2129194 ↗
62. A comparative review of the aqueous corrosion of glasses, crystalline ceramics, and metals10.1038/s41529-018-0037-2 ↗
63. Chloride ion interactions with oxide-covered aluminum leading to pitting corrosion: a review10.1149/2.1011409jes ↗
64. Chloride uptake by oxide covered aluminum as determined by x-ray photoelectron and x-ray absorption spectroscopy10.1149/1.1391835 ↗
65. Chloride ingress into aluminum prior to pitting corrosion an investigation by XANES and XPS10.1149/1.1393630 ↗
66. Localized corrosion (pitting): a model of passivity breakdown including the role of the oxide layer nanostructure10.1016/j.corsci.2008.06.047 ↗
67. The thinning of the passive layer of iron by halides10.1002/maco.19850360104 ↗
68. The point defect model for the passive state10.1149/1.2069096 ↗
69. Nucleation and repassivation of corrosion pits for pitting on iron and nickel10.1002/maco.19760271106 ↗
70. Transport processes and the mechanism of pitting of metals10.1149/1.2132857 ↗
71. Localized corrosion of aluminum alloys—a review10.5006/1.3584905 ↗
72. Pitting corrosion of aluminum10.1016/S0010-938X(99)00012-8 ↗
73. Passive films on stainless steels—chemistry, structure and growth10.1016/S0013-4686(02)00841-1 ↗
74. The effect of pH of zero charge on the pitting potential10.1149/1.2108708 ↗
75. The electrode kinetics of pit initiation on aluminum10.1016/0010-938X(94)00150-5 ↗
76. McCafferty · 2015
77. Determination of the surface isoelectric point of oxide films on metals by contact angle titration10.1006/jcis.1997.5138 ↗
78. Determination of the concentration of surface hydroxyl groups on metal oxide films by a quantitative XPS method10.1002/(SICI)1096-9918(199807)26:8<549::AID-SIA396>3.0.CO;2-Q ↗
79. Kosmulski · 2009
80. Prediction of flatband potentials at semiconductor-electrolyte interfaces from atomic electronegativities10.1149/1.2131419 ↗
81. An application of the microelectrophoresis method to the study of the surface properties of insoluble oxides10.1071/CH9570398 ↗
82. WR whitney award: perspectives on chloride interactions with passive oxides and oxide film breakdown10.5006/2511 ↗
83. In situ X-ray absorption study of chromium valency changes in passive oxides on sputtered AlCr thin films under electrochemical control10.1149/1.2085572 ↗
84. X‐ray absorption study of electrochemically grown oxide films on AlCr sputtered alloys II. In situ studies10.1149/1.2054714 ↗
85. Role of oxide/metal interface in corrosion resistance: Al–W and Al–Mo systems10.5006/1.3277562 ↗
86. The effect of doping on the point of zero of charge of alumina10.1016/0039-6028(72)90016-7 ↗
87. The effects of alloying elements on the passivity of sputter-deposited amorphous Al–Cr–Mo alloys in 1M HCl10.1016/0010-938X(96)00017-0 ↗
88. An angle-resolved xps study of the in-depth structure of passivated amorphous aluminum alloys10.1016/S0010-938X(97)00034-6 ↗
89. Insight into the pitting corrosion behavior of aluminum alloys10.1016/0010-938X(92)90130-U ↗
90. Corrosion inhibition of aluminum and aluminum alloys by soluble chromates, chromate coatings, and chromate-free coatings10.5006/1.3277570 ↗
91. Chromate conversion coating on aluminum alloys III. corrosion protection10.1149/1.1736683 ↗
92. The chemistry underlying chromate toxicity10.1007/BF00136433 ↗
93. The carcinogenicity of metals in humans10.1023/A:1018457305212 ↗
94. Corrosion protection of aluminum alloy 2024-T3 by vanadate conversion coatings10.5006/1.3287733 ↗
95. Mechanisms of corrosion inhibition of AA2024-T3 by vanadates10.1016/j.corsci.2006.10.027 ↗
96. Auger electron spectroscopic and electrochemical analysis of the effect of alloying elements on the passivation behavior of stainless steels10.5006/0010-9312-34.2.52 ↗
97. A molybdate treatment for enhancing the passivity of aluminum in chloride-containing environments10.1149/1.2086428 ↗
98. On-demand release of corrosion-inhibiting ions from amorphous Al–Co–Ce alloys10.1038/nmat1451 ↗
99. Inhibitors for the protection of aerospace aluminium alloy10.1002/maco.19970481104 ↗
100. Electrochemical sacrificial cathodic prevention provided by an Al–Co–Ce metal coating coupled to AA2024-T310.1149/1.1943588 ↗