Abstract
The degradation of proton exchange membrane water electrolysis cells is usually measured in a temporal increase of the cell voltage. Although this is sufficient to evaluate the stability of a system, it is less suitable for targeted material development. Thus, an overpotential-specific and temporally resolved electrochemical characterization protocol is proposed. In this the ohmic overpotential is determined with high frequency resistance measurements. These are also used in combination with polarization curves to distinguish between the kinetic and mass transport overpotentials and to determine kinetic key parameters, according to the Butler-Volmer and transition state theory. Complementary electrochemical impedance spectroscopy measurements further unravel the individual resistances. On this basis, the following statements can already be issued. The major share of the measured cell voltage increase, i.e. degradation, is of apparent nature as it is recovered once lower potentials are applied. It is suggested that this is due to changes in the oxidation states of the iridium-based catalyst. Real degradation occurs in the ohmic and mass transport overpotential mainly at higher current densities and longer operating times. The increasing kinetic overpotential with increasing operating time is primarily potential-driven. Interestingly, both the Tafel slope and the apparent exchange current density slightly increase over time.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Fuel Cells and Related Materials · Advanced battery technologies research · Advanced Battery Technologies Research
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (30)
Show source-provided references
1. 10.1149/1.368479810.1149/1.3684798 ↗
2. 10.1016/j.cattod.2015.10.01910.1016/j.cattod.2015.10.019 ↗
3. Bertuccioli L. Chan A. Hart D. Lehner F. Madden B. Standen E. , Study on development of water electrolysis in the EU, (2014).
4. 10.1149/1.348449610.1149/1.3484496 ↗
5. 10.1149/2.1441704jes10.1149/2.1441704jes ↗
6. 10.1016/j.jpowsour.2017.09.00610.1016/j.jpowsour.2017.09.006 ↗
7. 10.1002/anie.20160860110.1002/anie.201608601 ↗
8. U.S. Department of Energy (DOE), U.S. DRIVE Fuel Cell Tech Team, Cell Component Accelerated Stress Test and Polarization Curve Protocols for PEM Fuel Cells, (2013).
9. Ayers K. E. Anderson E. Capuano C. Hanlon G. Styche E. , 215th ECS Meeting(Abstract #380) (2009).10.1149/MA2009-01/7/380 ↗
10. Lickert T. Schwarz C. Gese P. Fallisch A. Schlüter M. Höfling N. Smolinka T. , Towards selective test protocols for accelerated Towards selective test protocols for accelerated in situ degradation of PEM electrolysis cell components, (2017).
11. van Berkel F. de Groot A. ten Hoopen S. , Impact of Dynamic Load from Renewable Energy Sources on PEM Electrolyzer Lifetime, (2017).
12. 10.1016/j.renene.2018.02.02410.1016/j.renene.2018.02.024 ↗
13. 10.1016/j.electacta.2018.04.15410.1016/j.electacta.2018.04.154 ↗
14. 10.1016/j.ijhydene.2016.07.12510.1016/j.ijhydene.2016.07.125 ↗
15. 10.1016/j.jpowsour.2007.09.03410.1016/j.jpowsour.2007.09.034 ↗
16. 10.1016/j.electacta.2016.06.12010.1016/j.electacta.2016.06.120 ↗
17. Rheinländer P. J. Bernt M. Incedag Y. Gasteiger H. A. , PRiME 2016/230th ECS Meeting, Abstract #2427 (2016).10.1149/MA2016-02/38/2427 ↗
18. 10.1038/s41929-018-0085-610.1038/s41929-018-0085-6 ↗
19. 10.1039/C6SC04622C10.1039/C6SC04622C ↗
20. 10.1149/2.0421908jes10.1149/2.0421908jes ↗
21. 10.1149/1.226629410.1149/1.2266294 ↗
22. O.'M. Bockris J. Reddy A. K. N. , Modern electrochemistry, New York, Kluwer Academic Publishers (2002).
23. 10.1039/C4EE00440J10.1039/C4EE00440J ↗
24. 10.1016/j.electacta.2018.05.15010.1016/j.electacta.2018.05.150 ↗
25. Barin I. , Thermochemical data of pure substances, Weinheim, VCH (1995).10.1002/9783527619825 ↗
26. 10.1021/ja01316a02210.1021/ja01316a022 ↗
27. 10.1016/S0304-386X(98)00007-310.1016/S0304-386X(98)00007-3 ↗
28. 10.1149/2.0341904jes10.1149/2.0341904jes ↗
29. 10.1149/2.0231611jes10.1149/2.0231611jes ↗
30. 10.1149/2.0171908jes10.1149/2.0171908jes ↗