journal article·2011-06-01Open access

In Situ Observation and Long-Term Reactivity of Si/C/CMC Composites Electrodes for Li-Ion Batteries

J-S. Bridel, T. Azaïs, M. Morcrette, J-M. Tarascon, D. Larcher

Abstract

Si/C/CMC composite for electrodes (Na-Carboxy-Methyl-Cellulose) appear today as the most promising strategy in view of substituting carbonaceous materials for silicon as negative active material in Li-ion batteries, hence the need to understand their reaction mechanism. By means of solid state Nuclear Magnetic Resonance spectroscopy, we confirmed that CMC chains can bind to Si via covalent or hydrogen bonding depending upon the pH of the mother suspension. Through coupled in situ Scanning Electron Microscopy and Electrochemical Impedance Spectroscopy observations of such electrodes reacting with Li, we demonstrated the ability of their porosity to buffer the Si swelling up to 1.7–2 Li/Si, further lithiation resulting in internal reorganization with either a definitive break of the covalent CMC-Si bond, or preservation of both the texture and electric wiring in the case of weaker Si-CMC hydrogen bonding thanks to a self-healing process. A relationship between the nature of the Si-CMC bonding and the electrode performance was found with a very positive impact of hydrogen interaction as 100 cycles could be achieved with preservation of the initial texture and excellent retention (3000 mAh/g Si after 100 cycles). Besides, we demonstrated that an alteration in the electrode texture/porosity, by a freeze-drying process, also impacts the electrode reversibility.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Advancements in Battery Materials · Supercapacitor Materials and Fabrication · Advanced Battery Materials and Technologies

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (54)

Show source-provided references
1. 2008
2. Tarascon · Nature (London) · 2001 · 404 · 35910.1038/35104644 ↗
3. Nagaura · Prog. Batteries Sol. Cells · 1990 · 9 · 209
4. Ohzuku · Chem. Lett. · 2001 · 1 · 64210.1246/cl.2001.642 ↗
5. Padhi · J. Electrochem. Soc. · 1997 · 144 · 118810.1149/1.1837571 ↗
6. Dey · J. Electrochem. Soc. · 1971 · 118 · 154710.1149/1.2407783 ↗
7. Sharma · J. Electrochem. Soc. · 1976 · 123 · 176310.1149/1.2132692 ↗
8. Lai · J. Electrochem. Soc. · 1976 · 123 · 119610.1149/1.2133033 ↗
9. Boukamp · J. Electrochem. Soc. · 1981 · 128 · 72510.1149/1.2127495 ↗
10. Obrovac · Electrochem. Solid-State Lett. · 2004 · 7, · 9310.1149/1.1652421 ↗
11. Hatchard · J. Electrochem. Soc. · 2004 · 151 · A83810.1149/1.1739217 ↗
12. Ryu · Electrochem. Solid-State Lett. · 2004 · 7 · 30610.1149/1.1792242 ↗
13. Timmons · J. Electrochem. Soc. · 2006 · 153 · A120610.1149/1.2194611 ↗
14. Huggings · J. Power Sources · 1988 · 22 · 34110.1016/0378-7753(88)80028-4 ↗
15. Wilson · J. Appl. Phys. · 1995 · 77 · 236310.1063/1.358759 ↗
16. Coutney · J. Electrochem. Soc. · 1997 · 144 · 204510.1149/1.1837740 ↗
17. Wilson · J. Electrochem. Soc. · 1995 · 142 · 32610.1149/1.2043994 ↗
18. Saint · Adv. Funct. Mater. · 2007 · 17 · 176510.1002/adfm.v17:11 ↗
19. Anani · J. Power Sources · 1992 · 38 · 35110.1016/0378-7753(92)80125-U ↗
20. Yang · Solid State Ionics · 1996 · 90 · 28110.1016/S0167-2738(96)00389-X ↗
21. Li · Solid State Ionics · 2000 · 135 · 18110.1016/S0167-2738(00)00362-3 ↗
22. Hatchard · J. Electrochem. Soc. · 2004 · 151 · A83810.1149/1.1739217 ↗
23. Obrovac · J. Electrochem. Soc. · 2007 · 154 · A10310.1149/1.2402112 ↗
24. Chen · Electrochem. Commun. · 2003 · 5 · 91910.1016/j.elecom.2003.08.017 ↗
25. Liu · Electrochem. Solid-State Lett. · 2005 · 8 · A10010.1149/1.1847685 ↗
26. Li · Electrochem. Solid-State Lett. · 2007 · 10 · A1710.1149/1.2398725 ↗
27. Beattie · J. Electrochem. Soc. · 2008 · 155 · A15810.1149/1.2817828 ↗
28. Bridel · Chem. Mater. · 2010 · 22 · 122910.1021/cm902688w ↗
29. Lestriez · Electrochem. Commun. · 2007 · 9 · 280110.1016/j.elecom.2007.10.001 ↗
30. Guo · Chem. Commun. (Cambridge) · 2010 · 46 · 142810.1039/b918727h ↗
31. Hochgatterer · Electrochem. Solid-State Lett. · 2008 · 11 · A7610.1149/1.2888173 ↗
32. Mazouzi · Electrochem. Solid-State Lett. · 2009 · 12 · A21510.1149/1.3212894 ↗
33. Lee · J. Electrochem. Soc. · 2007 · 154 · A51510.1149/1.2719644 ↗
34. Takami · J. Electrochem. Soc. · 1995 · 142 · 37110.1149/1.2044017 ↗
35. Orazem · 2008
36. Orsini · J. Power Sources · 1999 · 81–82 · 91810.1016/S0378-7753(98)00241-9 ↗
37. Orsini · 1999
38. Tezuka · Carbohydr. Res. · 1996 · 291 · 9910.1016/S0008-6215(96)00163-2 ↗
39. Azaïs · Chem. Mater. · 2006 · 18 · 638210.1021/cm061551c ↗
40. Azaïs · J. Phys. Chem. C · 2010 · 114 · 888410.1021/jp910622m ↗
41. Obrovac · Electrochem. Solid-State Lett. · 2004 · 7 · A9310.1149/1.1652421 ↗
42. Larcher · J. Mater. Chem. · 2007 · 17 · 375910.1039/b705421c ↗
43. Cordier · Nature (London) · 2008 · 451 · 97710.1038/nature06669 ↗
44. Bergman · J. Mater. Chem. · 2008 · 18 · 4110.1039/b713953p ↗
45. Wang · J. Electrochem. Soc. · 2001 · 148 · A76210.1149/1.1377285 ↗
46. Chang · J. Electrochem. Soc. · 2000 · 147 · 5010.1149/1.1393156 ↗
47. Beattie · J. Electrochem. Soc. · 2003 · 150 · A70110.1149/1.1569477 ↗
48. Bridel · J. Power Sources · 2010 · 195 · 203610.1016/j.jpowsour.2009.10.038 ↗
49. Sannier · 2003
50. Sannier · J. Electrochem. Soc. · 2004 · 151 · A87310.1149/1.1710516 ↗
51. Teyssot · 2005
52. Nadler · Anal. Chem. · 1959 · 31 · 210910.1021/ac60156a007 ↗
53. Obrovac · J. Electrochem. Soc. · 2007 · 154 · A84910.1149/1.2752985 ↗
54. Wilkinson · J. Power Sources · 1991 · 36 · 51710.1016/0378-7753(91)80077-B ↗