The degradation behavior of SiC coated PIP-C/SiC composites in thermal cycling environment
Source abstract
Abstract
Abstract C/SiC composites had been considered as structural material in complex and harsh environments, thermal stability was one of the key issues for C/SiC composites. This study aimed to investigate C/SiC composites in thermal cycling environment. SiC coating on carbon fibers via chemical vapor deposition at time from 0.5 h to 5 h was studied, and then the degradation behavior of coated C/SiC composites had been measured by thermal cycling tests. The results showed that the coating was continuous and uniform, with good surface adhesion. The interface of carbon fibers and SiC coating was partially destroyed during thermal shock tests. The degradation of mechanical properties was closely related to the evolution of the damage in the composites.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advanced ceramic materials synthesis · Fiber-reinforced polymer composites · Tribology and Wear Analysis
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (20)
Show source-provided references
1. Recycling carbon fibre reinforced polymers for structural applications: technology review and market outlook10.1016/j.wasman.2010.09.019 ↗
2. Design, preparation and properties of online-joints of C/SiC-C/SiC with pins10.1016/j.compositesb.2012.09.093 ↗
3. Effects of polycarbosilane infiltration processes on the microstructures and mechanical properties of 3D-Cf/SiC composites10.1016/j.ceramint.2006.02.005 ↗
4. Preparation and mechanical properties of C/SiC nuts and bolts10.1016/j.msea.2012.03.045 ↗
5. Effect of pyrolysis temperature on the pore structure evolution of polysiloxane-derived ceramics10.1016/j.ceramint.2011.11.033 ↗
6. Microstructure of TaC coatings on carbon fibers10.1134/S0020168511070053 ↗
7. Protective ceramic multilayer coatings for carbon fibers
8. Development of carbide coatings for graphite filaments
9. Low temperature preparation of titanium carbide coatings on graphite flakes from molten salts10.1111/j.1551-2916.2007.02184.x ↗
10. Fabrication of protective tantalum carbide coatings on carbon fibers using a molten salt method10.1016/j.apsusc.2008.03.158 ↗
11. Mechanical properties of several advanced Tyranno-SA fiber-reinforced CVI-SiC/SiC composites10.1016/S0921-5093(02)00468-9 ↗
12. Fabrication of advanced SiC fiber/F-CVI SiC matrixcomposites with SiC/C multi-layer interphase10.1016/j.jnucmat.2004.04.120 ↗
13. Mechanical properties of 3D KD-I SiCf/SiC composites with engineered fibre-matrix interfaces10.1016/j.compscitech.2011.01.014 ↗
14. Effects of the single layer CVD SiC interphases on the mechanical properties of the SiCf/SiC composites fabricated by PIP process10.1016/j.ceramint.2010.05.014 ↗
15. ZrB2/SiC as a protective coating for C/SiC Composites: effect of high temperature oxidation on mechanical properties and anti-ablation property10.1016/j.compositesb.2012.07.007 ↗
16. Mechanical behavior of C/SiC composites under simulated space environments10.1016/j.msea.2011.11.087 ↗
17. Processing and characterization of three-dimensional carbon fiber reinforced Si-O-C composites via precursor pyrolysis10.1016/S0921-5093(02)00908-5 ↗
18. Thermal shock behavior of two dimensional woven fiber-reinforced ceramic composites10.1111/j.1151-2916.1996.tb07996.x ↗
19. Thermal shock resistance of SiC fiber-reinforced borosilicate glass and lithium aluminosilicate matrix composites10.1007/BF01151250 ↗
20. Thermal shock properties of a 2D-C/SiC composite prepared by chemical vapor infiltration10.1007/s11665-012-0465-z ↗