The impact of core-shell nanotube structures on fracture in ceramic nanocomposites
Source abstract
Abstract
Abstract Multi-wall carbon nanotubes (MWCNTs) can be used to create ceramic nanocomposites with improved fracture toughness. In the present work, atomic layer deposition (ALD) was employed to deposit thin oxide layers on MWCNTs. These core-shell structures were then used to create nanocomposites by using a polymer derived ceramic (PDC) to produce the matrix. Variations in both the initial MWCNT structure and the oxide layers led to substantial differences in fiber-pullout behavior. Single tube pullout tests also showed that the oxide coatings led to stronger bonding with the ceramic matrix. With high defect density MWCNTs, this led to shorter pull-out lengths which is consistent with the conventional understanding of fracture in ceramic matrix composites. However, with low defect density MWCNTs longer pullout lengths were observed with the oxide layers. To interpret the different trends that were observed, we believe that the ALD coatings should not be viewed simply as a means of altering the interfacial properties. Instead, the coated MWCNTs should be viewed as more complex core-shell fibers where both interface and internal properties can be controlled with the ALD layers.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advanced ceramic materials synthesis · Tribology and Wear Analysis · Diamond and Carbon-based Materials Research
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (28)
Show source-provided references
1. Silicon-carbide fiber reinforced glass-ceramic matrix composites exhibiting high-strength and toughness10.1007/BF00543747 ↗
2. An indentation method for measuring matrix-fiber frictional stresses in ceramic composites10.1111/j.1151-2916.1984.tb19690.x ↗
3. The mechanics of matrix cracking in brittle-matrix fiber composites10.1016/0001-6160(85)90124-5 ↗
4. Failure mechanisms in ceramic-fiber ceramic-matrix composites10.1111/j.1151-2916.1985.tb15313.x ↗
5. Matrix fracture in fiber-reinforced ceramics10.1016/0022-5096(86)90035-9 ↗
6. Measurement of interfacial mechanical properties in fiber-reinforced ceramic composites10.1111/j.1151-2916.1987.tb05702.x ↗
7. Stress-displacement relation of fiber for fiber-reinforced ceramic composites during (indentation) loading and unloading10.1557/JMR.1989.1529 ↗
8. The relative residual fiber displacement after indentation loading and unloading of fiber-reinforced ceramic composites10.1007/BF00367588 ↗
9. The physics and mechanics of fibre-reinforced brittle matrix composites10.1007/BF00355946 ↗
10. Effect of fiber bridging stress on the fracture resistance of silicon-carbide-fiber/zircon composites10.1111/j.1151-2916.2000.tb01355.x ↗
11. Carbon nanotube reinforced ceramics10.1039/b101294k ↗
12. Direct observation of toughening mechanisms in carbon nanotube ceramic matrix composites10.1016/j.actamat.2003.10.050 ↗
13. Fabrication of carbon-nanotube-reinforced glass-ceramic nanocomposites by ultrasonic in situ sol-gel processing10.1039/b809369e ↗
14. Tough ceramic coatings: carbon nanotube reinforced silica sol-gel10.1016/j.apsusc.2010.04.020 ↗
15. Multi-walled carbon nanotube-reinforced silicon carbide fibers prepared by polymer-derived ceramic route10.1016/j.compositesa.2011.12.007 ↗
16. Ceramic matrix composites containing carbon nanotubes10.1007/s10853-009-3262-9 ↗
17. Carbon nanotubes: do they toughen brittle matrices?10.1007/s10853-011-5387-x ↗
18. Vapor phase fabrication and properties of continuous-filament ceramic composites10.1126/science.253.5024.1104 ↗
19. Fiber coating concepts for brittle-matrix composites10.1111/j.1151-2916.1993.tb03749.x ↗
20. Carbon nanotube pullout, interfacial properties, and toughening in ceramic nanocomposites: mechanistic insights from single fiber pullout analysis
21. Quantification and promotion of interfacial interactions between carbon nanotubes and polymer derived ceramics10.1016/j.carbon.2015.08.104 ↗
22. Interface toughness of carbon nanotube reinforced epoxy composites10.1021/am1011047 ↗
23. Development and application of a novel microfabricated device for the in situ tensile testing of 1-D nanomaterials10.1109/JMEMS.2010.2046014 ↗
24. Theory of mechanical properties of ceramic-matrix composites10.1111/j.1151-2916.1991.tb06852.x ↗
25. Stochastic damage evolution and failure in fiber-reinforced composites
26. Measuring the degree of stacking order in graphite by Raman spectroscopy10.1016/j.carbon.2007.11.015 ↗
27. Defect characterization in graphene and carbon nanotubes using Raman spectroscopy10.1098/rsta.2010.0213 ↗
28. Engineering strong intergraphene shear resistance in multi-walled carbon nanotubes and dramatic tensile improvements10.1002/adma.200902140 ↗