High-temperature oxidation resistance of sol–gel-derived ZrO2/(Al2O3–Y2O3) coating on titanium alloy
Source abstract
Abstract
ZrO2/(Al2O3–Y2O3) composite coating was deposited on Ti-6.5Al-3.5Mo-15Zr-0.3Si (at.%) alloy via sol–gel spin coating with the hope to improve its high-temperature oxidation resistance. The as-prepared coating was dense, uniform and crack-free. Isothermal and cyclic oxidation tests of coated and uncoated specimens at 700 °C for 100 h were performed to evaluate its effect on oxidation behavior of the alloy. The results indicated that oxidation resistance and spallation resistance for coated specimen have been remarkably improved, thickness of oxide scale of coated specimen was thinner than that of uncoated one and the scale was composed of deposited Al2O3 outermost layer, a thin TiO2 middle layer and a mixture of Al2O3 and ZrO2 thick innermost layer. The mechanism of the coating having beneficial effects could be attributed to the inhibition of the inward diffusion of O and outward diffusion of Ti and Al, lower thermal stress and good adhesion between the coating and substrate.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Intermetallics and Advanced Alloy Properties · Metal and Thin Film Mechanics · High-Temperature Coating Behaviors
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (26)
Show source-provided references
1. Clemens H, Kestler H (2000) Adv Eng Mater 2:551–57010.1002/1527-2648(200009)2:9<551::AID-ADEM551>3.0.CO;2-U ↗
2. Cao R, Zhu H, Chen JH et al (2008) J Mater Sci 43:299–31110.1007/s10853-007-2172-y ↗
3. Kothari K, Radhakrishnan R, Wereley NM (2012) Prog Aerosp Sci 55:1–1610.1016/j.paerosci.2012.04.001 ↗
4. Chen L, Paulitsch J, Du Y et al (2012) Surf Coat Technol 206:2954–296010.1016/j.surfcoat.2011.12.028 ↗
5. Varma SK, Chan A, Mahapatra BN (2001) Oxid Met 55:423–43510.1023/A:1010351613733 ↗
6. Teng LD, Nakatomi D, Seetharaman S (2007) Metall Mater Trans B 38:47710.1007/s11663-007-9061-2 ↗
7. Yamaguchi M, Inui H, Ito K (2000) Acta Mater 48:30710.1016/S1359-6454(99)00301-8 ↗
8. Shida Y, Anada H (1996) Oxid Met 45:197–21910.1007/BF01046826 ↗
9. Becker S, Rahmel A, Schorr M et al (1992) Oxid Met 38:425–46410.1007/BF00665663 ↗
10. Wallace TA, Clark RK, Wiedemann KE et al (1992) Oxid Met 37:111–12410.1007/BF00665185 ↗
11. Tang ZL, Wang FH, Wu WT (2000) Mater Sci Eng, A 276:70–7510.1016/S0921-5093(99)00513-4 ↗
12. Li ZW, Gao W, He YD (2001) Scr Mater 45:109910.1016/S1359-6462(01)01146-0 ↗
13. Jung HG, Jung DJ, Kim KY (2002) Surf Coat Technol 154:7510.1016/S0257-8972(01)01716-9 ↗
14. Hovsepian PE, Ehiasarian AP, Braun R et al (2010) Surf Coat Technol 204:270210.1016/j.surfcoat.2010.02.021 ↗
15. Oechsner M, Hillman C, Lange F (1996) J Am Ceram Soc 79:1834–183810.1111/j.1151-2916.1996.tb08003.x ↗
16. Chu MS, Wu SK (2004) Surf Coat Technol 179:257–26410.1016/S0257-8972(03)00819-3 ↗
17. Li H, Liang K, Mei L et al (2001) Mater Lett 51:320–32410.1016/S0167-577X(01)00311-1 ↗
18. Zhang XJ, Zhao SY, Gao CX et al (2009) J Sol Gel Sci Technol 49:221–22710.1007/s10971-008-1863-4 ↗
19. Zhang XJ, Ren BY, Gao CX et al (2011) J Sol Gel Sci Technol 59:561–56810.1007/s10971-011-2527-3 ↗
20. Zhang XJ, Li Q, Zhao SY et al (2008) Appl Surf Sci 255:1860–186410.1016/j.apsusc.2008.06.041 ↗
21. Zhang XJ, Li Q, Zhao SY et al (2008) J Sol Gel Sci Technol 47:107–11410.1007/s10971-008-1744-x ↗
22. Huang JF, Zeng XR, Li HJ et al (2005) Surf Coat Technol 190:25510.1016/j.surfcoat.2004.02.014 ↗
23. Li X, Liu H, Wang JY et al (2004) J Am Ceram Soc 87:228810.1111/j.1151-2916.2004.tb07507.x ↗
24. Wagner C (1952) J Electrochem Soc 99:36910.1149/1.2779605 ↗
25. Pint BA (1996) Oxid Met 45:1–410.1007/BF01046818 ↗
26. Evans HE (1989) Mater Sci Eng, A 120:139–14610.1016/0921-5093(89)90731-4 ↗