Abstract
Nanocrystalline spinel CuAl2O4 powders were prepared by sol-gel method from nitrate Cu(NO3)2·3H2O, Al(NO3)3·9H2O and complex C6H8O7·H2O. Sintering was carried out at 400, 500, 600, 700, 800°C respectively for 2 h in air. The XRD patterns started to appear CuAl2O4 peaks after sintering of 500°C and consist of only CuAl2O4 peaks as spinel crystal after sintering of 700°C. The powders were analyzed by TEM and UV-vis diffuse reflectance spectrum to be round, about 10–30 nm in size and Eg=1.77 eV. Photodegradation property of nanocrystalline CuAl2O4 powders was investigated by using methyl orange as model pollutant and mercury lamp (λ>400 nm) as energy source. The results indicated that CuAl2O4 powders sintered at 700°C had the excellent visible photocatalytic property. Under the irradiation of visible light, methyl orange could be degraded 97% in 120 min.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advanced Photocatalysis Techniques · Copper-based nanomaterials and applications · Catalytic Processes in Materials Science
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (26)
Show source-provided references
1. Hoffmann MR, Martin T, Choi W et al (1995) Chem Rev 95:6910.1021/cr00033a004 ↗
2. Jimm CY, Jun L (1997) J Photochem Photobiol A: Chem 111:19910.1016/S1010-6030(97)00207-4 ↗
3. Ranjit KT, Willner I, Bossmann S et al (1998) J Phys Chem B 102:939710.1021/jp982694s ↗
4. Anpo M, Takeuchi M (2003) J Catal 216:50510.1016/S0021-9517(02)00104-5 ↗
5. Diwald O, Thompson TL, Zubkov T (2004) J Phys Chem B 108:600410.1021/jp031267y ↗
6. Ye JH, Zou ZG, Mitsutake O et al (2002) Chem Phys Lett 356:22110.1016/S0009-2614(02)00254-3 ↗
7. Akyol A, Bayramoğlu M (2005) J hazardous Mater B 124:24110.1016/j.jhazmat.2005.05.006 ↗
8. Hideki K, Akihiko K (2003) Catalysis Today 78:56110.1016/S0920-5861(02)00355-3 ↗
9. Zhang ML, An TC, Hu XH et al (2004) Applied Catalysis 260:21510.1016/j.apcata.2003.10.025 ↗
10. Qiu JX, Wang CY, Gu MY (2004) Mater Sci Eng B 112:110.1016/j.mseb.2004.04.012 ↗
11. Bessekhound Y, Trari M (2001) Int J Hydrog Energy 27:35710.1016/S0360-3199(01)00159-8 ↗
12. Wang DF, Zou ZG (2003) Chem Phys Lett 373:19110.1016/S0009-2614(03)00574-8 ↗
13. Wang DF, Zou ZG, Ye JH (2004) Catalysis Today 93–95:89110.1016/j.cattod.2004.06.090 ↗
14. Ko YG, Lee WY (2002) Catalysis Lett 83:15710.1023/A:1021021627635 ↗
15. Zhang ML, An TC, Hu XH, Wang C, Sheng GY, Fu JM (2004) Appl Catalysis A: General 260:21510.1016/j.apcata.2003.10.025 ↗
16. Bessekhouad Y (2002) Mtrari Int J Hydrog Energy 27:35710.1016/S0360-3199(01)00159-8 ↗
17. Liu GG, Zhang XZ, Xu YJ, Niu XS, Zheng LQ, Ding XJ (2004) Chemosphere 55:128710.1016/j.chemosphere.2004.01.035 ↗
18. Sugimoto T, Zhou XP, Muramatsu A (2003) J Colloid Interface Sci 259:4310.1016/S0021-9797(03)00036-5 ↗
19. Kartini I, Meredith P, Diniz JC, Lu GQ (2004) J Sol-Gel Sci Technol 31:18510.1023/B:JSST.0000047984.60654.a1 ↗
20. Cui HT, Zayat M, Levy D (2005) J Non-Cryst Solids 351:210210.1016/j.jnoncrysol.2005.04.060 ↗
21. Zielińska B, Morawski AW (2005) Appl Catalysis B: Environ 55:22110.1016/j.apcatb.2004.08.015 ↗
22. Qaradawi SA, Salman SR (2002) J Photochem Photobiol A: Chem 148:16110.1016/S1010-6030(02)00086-2 ↗
23. Zhang ML, An TC, Hu XH, Wang C et al (2004) Appl Catalysis A: General 260:21510.1016/j.apcata.2003.10.025 ↗
24. Yao WF, Wang H, Xu XH et al (2003) Mater Lett 57:189910.1016/S0167-577X(02)01097-2 ↗
25. Qiu JX, Wang CY, Gu MY (2004) Mater Sci Eng B 112:110.1016/j.mseb.2004.04.012 ↗
26. Yang QH, Fu XX (2003) J Chin Ceram Soc (in Chinese) 31:254