Cohesive zone modeling of the autoclave pressure effect on the delamination behavior of composite laminates
Source abstract
Abstract
Current manufacturing processes using resin transfer molding or low-pressure prepreg curing may result in different defects and interfacial properties. The effect of autoclave pressure on the delamination behavior of T800/X850 composite laminates is explored. Cohesive zone model was used to model the delamination of unidirectional composite laminates under short-beam bending. Composites with various interlaminar properties were manufactured using autoclave under cure pressure from 0 MPa to 0.6 MPa. Cohesive zone model was validated using the material parameters of the composite cured under 0.6 MPa. The effect of cohesive zone model parameters including cohesive strength, mode I fracture toughness ([Formula: see text]), and mode II fracture toughness ([Formula: see text]) on the delamination behavior and load–displacement response was investigated. Parametric study shows that interlaminar cohesive strength and mode II fracture toughness dominated the initiation of yield and post-yield region, respectively. The correlation between autoclave pressure and mode II fracture toughness was predicted, which is mainly affected by void content.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Mechanical Behavior of Composites · Epoxy Resin Curing Processes · Fatigue and fracture mechanics
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
Light Alloys Research Institute, Central South University, Changsha, China
School of Mechanical and Electrical Engineering, Central South University, Changsha, China
Engineering Department, Cambridge University, Cambridge, UK
Funding
the National Science Foundation of China · the National Program on Key Basic Research Project of China · the project of Innovation-driven Plan in Central South University
References (24)
Show source-provided references
1. 10.1016/j.compositesa.2015.01.02510.1016/j.compositesa.2015.01.025 ↗
2. 10.1007/s12221-014-2404-010.1007/s12221-014-2404-0 ↗
3. 10.1016/j.compstruc.2006.02.00210.1016/j.compstruc.2006.02.002 ↗
4. 10.1002/app.2038210.1002/app.20382 ↗
5. 10.1016/S0266-3538(03)00254-910.1016/S0266-3538(03)00254-9 ↗
6. 10.1007/BF0241024610.1007/BF02410246 ↗
7. 10.1016/j.compscitech.2011.05.00210.1016/j.compscitech.2011.05.002 ↗
8. 10.1007/s12221-017-6606-010.1007/s12221-017-6606-0 ↗
9. 10.1016/j.compstruct.2005.02.00110.1016/j.compstruct.2005.02.001 ↗
10. 10.1016/0022-5096(60)90013-210.1016/0022-5096(60)90013-2 ↗
11. 10.1016/S0065-2156(08)70121-210.1016/S0065-2156(08)70121-2 ↗
12. 10.1016/j.compositesb.2008.10.00610.1016/j.compositesb.2008.10.006 ↗
13. 10.1016/j.compstruct.2010.01.01210.1016/j.compstruct.2010.01.012 ↗
14. 10.1016/j.compstruct.2013.05.04910.1016/j.compstruct.2013.05.049 ↗
15. 10.1016/j.compstruct.2003.11.00510.1016/j.compstruct.2003.11.005 ↗
16. 10.1016/j.compscitech.2009.10.00210.1016/j.compscitech.2009.10.002 ↗
17. 10.1016/0266-3538(96)00005-X10.1016/0266-3538(96)00005-X ↗
18. 10.1016/j.compscitech.2016.02.00810.1016/j.compscitech.2016.02.008 ↗
19. Naya F · Compos Part A Appl Sci Manuf · 2017 · 126 · 60
20. 10.1016/j.compstruct.2015.03.03810.1016/j.compstruct.2015.03.038 ↗
21. 10.1002/pc.2260810.1002/pc.22608 ↗
22. 10.1080/09276440.2016.123711310.1080/09276440.2016.1237113 ↗
23. Greenhald ES. · 2009
24. Shen GL · 2013