Environmental aging effect on interlaminar properties of graphene nanoplatelets reinforced epoxy/carbon fiber composite laminates
Source abstract
Abstract
Graphene nanoplatelets are two-dimensional carbon structure materials with single or multilayers graphite plane which possesses attractive characteristics. In this study, the environmental aging effect on interlaminar properties of graphene nanoplatelet containing different proportions (0.25, 0.50, 0.75 wt%) reinforced epoxy/carbon fiber (carbon fiber reinforced plastic) composite laminates including interlaminar shear strength and fracture toughness were investigated. The interlaminar properties of graphene nanoplatelets/carbon fiber reinforced plastic composite laminates were improved over that of neat carbon fiber reinforced plastic composite laminates. Experimental results showed that the composite laminates containing graphene nanoplatelets possesses the appreciable improvement. The mechanisms responsible for the interlaminar enhancement were identified by studying the fracture surfaces using field emission scanning electron microscopy.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Fiber-reinforced polymer composites · Mechanical Behavior of Composites · Tribology and Wear Analysis
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
Department of Mold and Die Engineering, National Kaohsiung University of Applied Science, Taiwan
Department of Aviation Mechanical Engineering, China University of Science and Technology, Taiwan
Department of Safety, Health and Environmental Engineering, Hung Kuang University, Taiwan
References (36)
Show source-provided references
1. 10.1081/MB-12002157610.1081/MB-120021576 ↗
2. 10.1016/j.compscitech.2006.11.01010.1016/j.compscitech.2006.11.010 ↗
3. 10.1163/15685540432297140410.1163/156855404322971404 ↗
4. 10.1002/app.210110.1002/app.2101 ↗
5. 10.1016/S0266-3538(02)00201-410.1016/S0266-3538(02)00201-4 ↗
6. 10.1023/A:101470880823010.1023/A:1014708808230 ↗
7. 10.1021/jp071761s10.1021/jp071761s ↗
8. 10.1016/j.carbon.2008.10.01110.1016/j.carbon.2008.10.011 ↗
9. 10.1063/1.222187410.1063/1.2221874 ↗
10. 10.1021/cm801356a10.1021/cm801356a ↗
11. 10.1021/nl080604h10.1021/nl080604h ↗
12. 10.1038/nnano.2007.45110.1038/nnano.2007.451 ↗
13. 10.1021/nn901047210.1021/nn9010472 ↗
14. 10.1016/j.compscitech.2006.08.00910.1016/j.compscitech.2006.08.009 ↗
15. 10.1007/978-1-4899-1822-210.1007/978-1-4899-1822-2 ↗
16. 10.1007/978-94-015-7764-910.1007/978-94-015-7764-9 ↗
17. 10.1016/0010-4361(81)90397-910.1016/0010-4361(81)90397-9 ↗
18. 10.1016/S0032-3861(00)00187-710.1016/S0032-3861(00)00187-7 ↗
19. 10.1016/S0032-3861(03)00372-010.1016/S0032-3861(03)00372-0 ↗
20. 10.1016/j.polymer.2005.05.15110.1016/j.polymer.2005.05.151 ↗
21. 10.1007/s10853-005-5472-010.1007/s10853-005-5472-0 ↗
22. 10.1155/2013/56540110.1155/2013/565401 ↗
23. 10.1016/j.compositesa.2007.11.01310.1016/j.compositesa.2007.11.013 ↗
24. Barikani M · Iran Polym J · 2002 · 11 · 413
25. Reeder JR. A bilinear failure criterion for mixed-mode delamination. Composite materials: Testing and design. In: ASTM STP 1206, ASTM international (ed ET Camponeschi Jr), W. Conshohocken, PA, 1993, pp.303–322.10.1520/STP12636S ↗
26. 10.4236/jmmce.2011.101309910.4236/jmmce.2011.1013099 ↗
27. Morris GE. Determining fracture directions and fracture origins on failed graphite/epoxy surfaces. Nondestructive evaluation and flaw criticality for composite materials. In: ASTM STP 696, ASTM international (ed RB Pipes), Philadelphia, PA, 1979, pp.274–297.10.1520/STP36036S ↗
28. 10.1016/j.msea.2007.04.04310.1016/j.msea.2007.04.043 ↗
29. 10.1163/156855198X0026410.1163/156855198X00264 ↗
30. 10.1007/BF0116074310.1007/BF01160743 ↗
31. 10.1016/0921-5093(90)90167-210.1016/0921-5093(90)90167-2 ↗
32. 10.1016/S0032-3861(03)00084-310.1016/S0032-3861(03)00084-3 ↗
33. 10.1016/j.compscitech.2005.01.01410.1016/j.compscitech.2005.01.014 ↗
34. 10.1016/j.carbon.2013.03.05010.1016/j.carbon.2013.03.050 ↗
35. 10.1016/S0266-3538(97)00222-410.1016/S0266-3538(97)00222-4 ↗
36. 10.1016/j.compositesa.2008.10.00610.1016/j.compositesa.2008.10.006 ↗